Abstract
Abstract The invention is directed toward a formable bone composition for application to a bone defect site to promote new bone growth at the site which comprises a new bone growth inducing compound of demineralized lyophilized allograft bone particles. The particle size ranges from about 0.1 mm to about 1.0 cm and is mixed in a hydrogel carrier containing a sodium phosphate saline buffer, the hydrogel component of the carrier ranging from about 1.0 to 5.0% of the composition and a pH between 6.8–7.4 with one or more additives of a cellular material, growth factor, demineralized bone chips or mineralized bone chips.
Inventors
- 👤 Arthur A. Gertzman
- 👤 Moon Hae Sunwoo
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-22 22:54
CPC Classifications
A; A61; A61L; A61L24/00; A61L24/0005; A61K; A61K35/00; A61K35/12; A61K35/32; A61K38/00; A61K38/16; A61K38/17; A61K38/18; A61K38/1875; A61L24/001; A61L24/0031; A61L24/0047; A61L24/0073; A61L24/0094; A61L27/00; A61L27/36; A61L27/3604; A61L27/3608; A61L27/3641; A61L27/3645; A61L27/365; A61L27/3683; A61L27/38; A61L27/3804; A61L27/3821; A61L27/3834; A61L27/3839; A61L27/3843; A61L27/3847; A61L27/40; A61L27/44; A61L27/48; A61L27/50; A61L27/52; C; C08; C08L; C08L5/00; C08L5/08; A61F; A61F2/00; A61F2/02; A61F2/28; A61F2/30; A61F2002/30001; A61F2002/30003; A61F2002/30004; A61F2002/30059; A61F2310/00; A61F2310/00005; A61F2310/00359; A61L2430/00; A61L2430/02
Claims Analysis
Total Claims: 28
Claim 1
Independent Claim
194 words
A sterile formable bone composition for application to a bone defect site to promote new bone growth at the site comprising demineralized osteoinductive and osteoconductive bone particles in an aqueous carrier solution, said bone particles are alloaraft bone ranging from about 100 microns to about 850 microns in size at a concentration ranging from 20% to 35% by weight of the composition, the carrier comprising a hydrogel component of sodium hyaluronate or its derivatives in a phosphate buffered aqueous solution, said hydrogel ranging from about 1.0% to about 5.0% by weight of the aqueous carrier solution and cellular material taken from a group consisting of living cells, cell elements such as red blood cells, white blood cells, platelets, blood plasma, pluripotential cells, osteoblasts, osteoclasts, and fibroblasts, epithelial cells, and endothelial cells present at a concentration of 10 5 to 10 8 per cc of the carrier, said hydrogel component having a high molecular weight ranging from about six hundred sixty thousand to three million Daltons with a stable viscosity at a temperature ranging from about 22° C. to about 37° C. and said composition having a pH ranging from about 6.8 to about 7.4
Claim 2
Dependent Claim
194 words
A sterile formable bone composition for application to a bone defect site to promote new bone growth at the site comprising demineralized osteoinductive and osteoconductive bone particles in an aqueous carrier solution, said bone particles are alloaraft bone ranging from about 100 microns to about 850 microns in size at a concentration ranging from 20% to 35% by weight of the composition, the carrier comprising a hydrogel component of sodium hyaluronate or its derivatives in a phosphate buffered aqueous solution, said hydrogel ranging from about 1.0% to about 5.0% by weight of the aqueous carrier solution and cellular material taken from a group consisting of living cells, cell elements such as red blood cells, white blood cells, platelets, blood plasma, pluripotential cells, osteoblasts, osteoclasts, and fibroblasts, epithelial cells, and endothelial cells present at a concentration of 10 5 to 10 8 per cc of the carrier, said hydrogel component having a high molecular weight ranging from about six hundred sixty thousand to three million Daltons with a stable viscosity at a temperature ranging from about 22° C. to about 37° C. and said composition having a pH ranging from about 6.8 to about 7.4
Claim 3
Dependent Claim
65 words
A sterile formable bone composition as claimed in claim 1 including growth factor additive added to said composition, said growth factor comprising one or more of a group consisting of transforming growth factor (TGF-beta), insulin growth factor (IGF-1); platlet derived growth factor (PDGF), vascular endothelial growth factor (VEGF), fibroblast growth factor (FGF) (numbers 1–23), osteopontin, growth hormones such as somatotropin celiular attractants and attachment agents.
Claim 4
Dependent Claim
45 words
A sterile formable bone composition as claimed in claim 1 including growth factor additive added to said composition comprising one or more of a group consisting of fibroblast growth factor (FGF) (numbers 1–23) in the amount of 2–4 milligrams in 10 cc of carrier solution.
Claim 5
Dependent Claim
21 words
A sterile formable bone composition as claimed in claim 1 wherein said composition includes an additive collagen and insoluble collagen derivatives.
Claim 6
Dependent Claim
27 words
A sterile formable bone composition as claimed in claim 1 wherein said composition includes the addition of calcium hydroxyapatite at a concentration of 20–35% measured as calcium.
Claim 7
Dependent Claim
56 words
A sterile formable bone composition as claimed in claim 1 wherein said composition includes bone chips taken from a group consisting of partially demineralized chips and non demineralized chips having a particle size ranging from 0.1 mm to 1.0 cm which are added to said viscous carrier at a concentration of about 5% to about 25%.
Claim 8
Dependent Claim
203 words
A sterile formable bone composition for application to a bone defect site to promote new bone growth at the site comprising a demineralized or vartiallv demineralized osteoinductive and osteoconductive bone particles in an aqueous carrier solution, said bone particles ranging from about 100 microns to about 850 microns in size at a concentration ranging from about 20% to about 35% by weight of the composition the carrier comprising a hydrogel component of sodium hyaluronate or its derivatives in a phosphate buffered aqueous solution, said hydrogel ranging from about 1.0% to about 5.0% by weight of the aqueous carrier solution and said hydrogel component having a high molecular weight ranging from about six hundred sixty thousand to three million Daltons with a stable viscosity at a temperature ranging from about 22° C. to about 37° C., said composition having a pH ranging from about 6.8 to about 7.4 and a growth factor additive added to said composition, said growth factor comprising one or more of a group consisting of transforming growth factor (TGF-beta), insulin growth factor (IGF-1); platlet derived growth factor (PDGF), vascular endothelial growth factor (VEOF), fibroblast growth factor (FGF) (numbers 1–23), osteopontin, growth hormones such as somatotropin cellular attractants and attachment agents.
Claim 9
Dependent Claim
203 words
A sterile formable bone composition for application to a bone defect site to promote new bone growth at the site comprising a demineralized or vartiallv demineralized osteoinductive and osteoconductive bone particles in an aqueous carrier solution, said bone particles ranging from about 100 microns to about 850 microns in size at a concentration ranging from about 20% to about 35% by weight of the composition the carrier comprising a hydrogel component of sodium hyaluronate or its derivatives in a phosphate buffered aqueous solution, said hydrogel ranging from about 1.0% to about 5.0% by weight of the aqueous carrier solution and said hydrogel component having a high molecular weight ranging from about six hundred sixty thousand to three million Daltons with a stable viscosity at a temperature ranging from about 22° C. to about 37° C., said composition having a pH ranging from about 6.8 to about 7.4 and a growth factor additive added to said composition, said growth factor comprising one or more of a group consisting of transforming growth factor (TGF-beta), insulin growth factor (IGF-1); platlet derived growth factor (PDGF), vascular endothelial growth factor (VEOF), fibroblast growth factor (FGF) (numbers 1–23), osteopontin, growth hormones such as somatotropin cellular attractants and attachment agents.
Claim 10
Dependent Claim
80 words
A sterile formable bone composition as claimed in claim 7 including a cellular material taken from a group consisting of living cells and cell elements such as chondrocytes, red blood cells, white blood cells, platelets, blood plasma, bone marrow cells, mesenchymal stem cells, pluripotential cells, osteoblasts, osteoclasts, and fibroblasts, epithelial cells, and endothelial cells. These cells or cell elements or combinations of the same are present at a concentration of 10 5 to 10 8 per cc of the carrier.
Claim 11
Dependent Claim
21 words
A sterile formable bone composition as claimed in claim 7 wherein said composition includes an additive collagen and insoluble collagen derivatives.
Claim 12
Dependent Claim
30 words
A sterile formable bone composition as claimed in claim 7 wherein said composition includes the addition of calcium hydroxyapatite at a concentration of 20–35% measured by weight of the compostion.
Claim 13
Dependent Claim
35 words
A sterile formable bone composition as claimed in claim 7 wherein said bone particles are taken from a group consisting of allograft bone, cortical allograft bone, corticalcancellous bone, cancellous bone, autologous bone and xenograft bone.
Claim 14
Dependent Claim
56 words
A sterile formable bone composition as claimed in claim 7 wherein said composition includes bone chips taken from a group consisting of partially demineralized chips and fully mineralized chips having a particle size ranging from 0.1 mm to 1.0 cm which are added to said viscous carrier at a concentration of about 5% to about 25%.
Claim 15
Dependent Claim
193 words
A sterile formable bone composition for application to a bone defect site to promote new bone growth at the site comprising a demineralized osteoinductive and osteoconductive bone particles in an aqueous carrier solution, the bone particles being added to a viscous carrier at a concentration ranging from about 20% to about 50% (w/w), the carrier comprising a hydrogel taken from a group consisting of Dextran, carboxymethylcellulose (CMC) and hydroxypropylmethylcellulose (HPMC) in a phosphate buffered aqueous solution, said hydrogel ranging from about 15% to about 30% by weight of the aqueous carrier solution and said hydrogel component having a molecular weight ranging from twenty thousand to forty thousand Daltons with a stable viscosity at a temperature ranging from about 22° C. to about 37° C. and said composition having a pH ranging from about 6.8 to about 7.4 and a growth factor additive added to said composition, said growth factor comprising one or more of a group consisting of transforming growth factor (TGF-beta), insulin growth factor (IGF-1); platlet derived growth factor (PDGF), vascular endothelial growth factor (VEGF), fibroblast growth factor (FGF) (numbers 1–23), osteopontin, growth hormones such as somatotropin cellular attractants and attachment agents.
Claim 16
Dependent Claim
193 words
A sterile formable bone composition for application to a bone defect site to promote new bone growth at the site comprising a demineralized osteoinductive and osteoconductive bone particles in an aqueous carrier solution, the bone particles being added to a viscous carrier at a concentration ranging from about 20% to about 50% (w/w), the carrier comprising a hydrogel taken from a group consisting of Dextran, carboxymethylcellulose (CMC) and hydroxypropylmethylcellulose (HPMC) in a phosphate buffered aqueous solution, said hydrogel ranging from about 15% to about 30% by weight of the aqueous carrier solution and said hydrogel component having a molecular weight ranging from twenty thousand to forty thousand Daltons with a stable viscosity at a temperature ranging from about 22° C. to about 37° C. and said composition having a pH ranging from about 6.8 to about 7.4 and a growth factor additive added to said composition, said growth factor comprising one or more of a group consisting of transforming growth factor (TGF-beta), insulin growth factor (IGF-1); platlet derived growth factor (PDGF), vascular endothelial growth factor (VEGF), fibroblast growth factor (FGF) (numbers 1–23), osteopontin, growth hormones such as somatotropin cellular attractants and attachment agents.
Claim 17
Dependent Claim
81 words
A sterile formable bone composition as claimed in claim 13 including a cellular material additive taken from a group consisting of living cells and cell elements such as chondrocytes, red blood cells, white blood cells, platelets, blood plasma, bone marrow cells, mesenchymal stem cells, pluripotential cells, osteoblasts, osteoclasts, and fibroblasts, epithelial cells, and endothelial cells, said cells or cell elements or combinations of the same being present at a concentration of 10 5 to 10 8 per cc of the carrier.
Claim 18
Dependent Claim
171 words
A sterile formable bone composition for application to a bone defect site to promote new bone growth at the site comprising demineralized osteoinductive and osteoconductive bone particles an aqueous carrier solution, the bone particles being added to a viscous carrier at a concentration ranging from about 20% to about 50% (w/w), the carrier comprising a hydrogel taken from a group consisting of Dextran, carboxymethylcellulose (CMC) and hydroxypropyhnethylcellulose (HPMC) in a phosphate buffered aqueous solution, said hydrogel ranging from about 15% to about 30% by weight of the aqueous carrier solution and cellular material taken from a group consisting of living cells, cell elements such as red blood cells, white blood cells, platelets, blood plasma, pluripotential cells, osteoblasts, osteoclasts, and fibroblasts, epithelial cells, and endothelial cells present at a concentration of 10 5 to 10 8 per cc of the carrier, said hydrogel component having a molecular weight ranging twenty thousand to forty thousand Daltons with a stable viscosity and said composition having a pH ranging from about 6.8 to about 7.4
Claim 19
Dependent Claim
171 words
A sterile formable bone composition for application to a bone defect site to promote new bone growth at the site comprising demineralized osteoinductive and osteoconductive bone particles an aqueous carrier solution, the bone particles being added to a viscous carrier at a concentration ranging from about 20% to about 50% (w/w), the carrier comprising a hydrogel taken from a group consisting of Dextran, carboxymethylcellulose (CMC) and hydroxypropyhnethylcellulose (HPMC) in a phosphate buffered aqueous solution, said hydrogel ranging from about 15% to about 30% by weight of the aqueous carrier solution and cellular material taken from a group consisting of living cells, cell elements such as red blood cells, white blood cells, platelets, blood plasma, pluripotential cells, osteoblasts, osteoclasts, and fibroblasts, epithelial cells, and endothelial cells present at a concentration of 10 5 to 10 8 per cc of the carrier, said hydrogel component having a molecular weight ranging twenty thousand to forty thousand Daltons with a stable viscosity and said composition having a pH ranging from about 6.8 to about 7.4
Claim 20
Dependent Claim
65 words
A sterile formable bone composition as claimed in claim 15 including growth factor additive added to said composition, said growth factor comprising one or more of a group consisting of transforming growth factor (TGF-beta), insulin growth factor (IGF-1); platlet derived growth factor (PDGF), vascular endothelial growth factor (VEGF), fibroblast growth factor (FGF) (numbers 1–23), osteopontin, growth hormones such as somatotropin cellular attractants and attachment agents.
Claim 21
Dependent Claim
45 words
A sterile formable bone composition as claimed in claim 15 including growth factor additive added to said composition comprising one or more of a group consisting of fibroblast growth factor (FGF) (numbers 1–23) in the amount of 2–4 milligrams in 10 cc of carrier solution.
Claim 22
Dependent Claim
189 words
A sterile formable bone composition for application to a bone defect site to promote new bone growth at the site comprising a demineralized osteo inductive and osteoconductive bone particles in an aqueous carrier solution, the bone particles being added to a viscous carrier at a concentration ranging from 5–50% (w/w), the carrier comprising a hydrogel taken from a group consisting of chitosan and sodium alginate in a phosphate buffered aqueous solution, said hydrogel ranging from about 5.0% to about 20.0% by weight of the aqueous carrier solution and said hydrogel component having a molecular weight ranging from ten thousand to three hundred thousand Daltons with a stable viscosity at a temperature ranging from about 22° C. to about 37° C. and said composition having a pH ranging from about 6.8 to about 7.4 and a growth factor additive added to said composition, said growth factor comprising one or more of a group consisting of transforming growth factor (TGF-beta), insulin growth factor (IGF-1); platlet derived growth factor (PDGF), vascular endothelial growth factor (VEGF), fibroblast growth factor (FGF) (numbers 1–23), osteopontin, growth hormones such as somatotropin cellular attractants and attachment agents.
Claim 23
Dependent Claim
189 words
A sterile formable bone composition for application to a bone defect site to promote new bone growth at the site comprising a demineralized osteo inductive and osteoconductive bone particles in an aqueous carrier solution, the bone particles being added to a viscous carrier at a concentration ranging from 5–50% (w/w), the carrier comprising a hydrogel taken from a group consisting of chitosan and sodium alginate in a phosphate buffered aqueous solution, said hydrogel ranging from about 5.0% to about 20.0% by weight of the aqueous carrier solution and said hydrogel component having a molecular weight ranging from ten thousand to three hundred thousand Daltons with a stable viscosity at a temperature ranging from about 22° C. to about 37° C. and said composition having a pH ranging from about 6.8 to about 7.4 and a growth factor additive added to said composition, said growth factor comprising one or more of a group consisting of transforming growth factor (TGF-beta), insulin growth factor (IGF-1); platlet derived growth factor (PDGF), vascular endothelial growth factor (VEGF), fibroblast growth factor (FGF) (numbers 1–23), osteopontin, growth hormones such as somatotropin cellular attractants and attachment agents.
Claim 24
Dependent Claim
81 words
A sterile formable bone composition as claimed in claim 18 including a cellular material additive taken from a group consisting of living cells and cell elements such as chondrocytes, red blood cells, white blood cells, platelets, blood plasma, bone marrow cells, mesenchymal stem cells, pluripotential cells, osteoblasts, osteoclasts, and fibroblasts, epithelial cells, and endothelial cells. These cells or cell elements or combinations of the same are present at a concentration of 10 5 to 10 8 per cc of the carrier.
Claim 25
Dependent Claim
168 words
A sterile formable bone composition for application to a bone defect site to promote new bone growth at the site comprising demineralized osteoinductive and osteoconductive bone particles in an aqueous carrier solution, the bone particles being added to a viscous carrier at a concentration ranging from 5–50% (w/w), the carrier comprising a hydrogel taken from a group consisting of chitosan and sodium alginate in a phosphate buffered aqueous solution, said hydrogel ranging from about 5.0% to about 20.0% by weight of the aqueous carrier solution and cellular material taken from a group consisting of living cells, cell elements such as red blood cells, white blood cells, platelets, blood plasma, pluripotential cells, osteoblasts, osteoclasts, and fibroblasts, epithelial cells, and endothelial cells present at a concentration of 10 5 to 10 8 per cc of the carrier, said hydrogel component having a molecular weight ranging from ten thousand to three hundred thousand Daltons with a stable viscosity and said composition having a pH ranging from about 6.8 to about 7.4
Claim 26
Dependent Claim
168 words
A sterile formable bone composition for application to a bone defect site to promote new bone growth at the site comprising demineralized osteoinductive and osteoconductive bone particles in an aqueous carrier solution, the bone particles being added to a viscous carrier at a concentration ranging from 5–50% (w/w), the carrier comprising a hydrogel taken from a group consisting of chitosan and sodium alginate in a phosphate buffered aqueous solution, said hydrogel ranging from about 5.0% to about 20.0% by weight of the aqueous carrier solution and cellular material taken from a group consisting of living cells, cell elements such as red blood cells, white blood cells, platelets, blood plasma, pluripotential cells, osteoblasts, osteoclasts, and fibroblasts, epithelial cells, and endothelial cells present at a concentration of 10 5 to 10 8 per cc of the carrier, said hydrogel component having a molecular weight ranging from ten thousand to three hundred thousand Daltons with a stable viscosity and said composition having a pH ranging from about 6.8 to about 7.4
Claim 27
Dependent Claim
65 words
A sterile formable bone composition as claimed in claim 20 including growth factor additive added to said composition, said growth injector comprising one or more of a group consisting of transforming growth factor (TGF-beta), insulin growth factor (IGF-1); platlet derived growth factor (PDGF), vascular endothelial growth factor (VEGF), fibroblast growth factor (FGF) (numbers 1–23), osteopontin, growth hormones such as somatotropin cellular attractants and attachment agents.
Claim 28
Dependent Claim
45 words
A sterile formable bone composition as claimed in claim 20 including growth factor additive added to said composition comprising one or more of a group consisting of fibroblast growth factor (FGF) (numbers 1–23) in the amount of 2–4 milligrams in 10 cc of carrier solution.
References Cited (Backward Citations)
US4172128A
Cited
US4191747A
Cited
US5510418A
Cited
US5073373A
Cited
US5290558A
Cited
US5356629A
Cited
US5314476A
Cited
US5507813A
Cited
US5707962A
Cited
US5830493A
Cited
US6294187B1
Cited
US6689747B2
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 2009-03-27 | 2009-09-26 | 2010-03-28 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 2013-03-27 | 2013-09-26 | 2014-03-28 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 2017-03-27 | 2017-09-26 | 2018-03-28 | $7700.00 | Window Closed / Lapsed |