Patent US5284468A successfully refreshed from Google Patents.
US5284468A
Expired / Lapsed
US
⏱️ 0.0 years remaining
Orthopedic splinting article
Assignee: M Pact Worldwide Management Corp
•
Filing: 1991-08-19
•
Granted: 1994-02-08
•
Expires: 2011-08-19
Abstract
Abstract A polyvinyl acetal sponge formed from a high molecular weight polyvinyl alcohol is used for forming a splint for a portion of body, such as during healing of a bone fracture or other injury. The sponge is maintained in a softened condition in the presence of vapors of a softening agent such as ethyl alcohol within a sealed pouch. Upon removal from the pouch, the sponge is applied to the body portion and it hardens to form the splint as the softening agent vapors dissipate.
Inventors
- 👤 Thomas W. Nelson
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-22 23:20
CPC Classifications
A; A61; A61F; A61F5/00; A61F5/01; A61F5/04; A61F5/05; A61F5/058; A61F5/05825
Claims Analysis
Total Claims: 20
Claim 1
Independent Claim
132 words
A packaged splint for use in forming a hard structure about a body portion, said packaged splint comprising: a layer of polyvinyl acetal sponge made from a polyvinyl alcohol having a molecular weight within the range of approximately 85,000 to approximately 186,000; softening agent vapors associated with said sponge for softening the sponge to permit placement thereof about said body portion; and a package sealingly enclosing said sponge to maintain the softening agent in association with the sponge, said package being constructed to permit removal of the softened sponge from the package for placement about said body portion, whereupon said sponge sets to a hardened state having a modulus of elasticity within the range of 132,000 to 172,000 psi to form said structure as the softening agent vapors disassociate from the sponge.
Claim 2
Dependent Claim
132 words
A packaged splint for use in forming a hard structure about a body portion, said packaged splint comprising: a layer of polyvinyl acetal sponge made from a polyvinyl alcohol having a molecular weight within the range of approximately 85,000 to approximately 186,000; softening agent vapors associated with said sponge for softening the sponge to permit placement thereof about said body portion; and a package sealingly enclosing said sponge to maintain the softening agent in association with the sponge, said package being constructed to permit removal of the softened sponge from the package for placement about said body portion, whereupon said sponge sets to a hardened state having a modulus of elasticity within the range of 132,000 to 172,000 psi to form said structure as the softening agent vapors disassociate from the sponge.
Claim 3
Dependent Claim
28 words
The packaged splint of claim 1, wherein said sponge is made from a polyvinyl alcohol having a molecular weight within the range of approximately 124,000 to approximately 186,000.
Claim 4
Dependent Claim
28 words
The packaged splint of claim 1, wherein said sponge is made from a polyvinyl alcohol having a molecular weight within the range of approximately 160,000 to approximately 186,000.
Claim 5
Dependent Claim
32 words
The packaged splint of claim 3, wherein said softening agent vapors are selected from vapors from the group consisting of a C 1 to C 3 alcohol and water and mixtures thereof.
Claim 6
Dependent Claim
25 words
The packaged splint of claim 3, wherein said softening agent vapors are selected from vapors of one or more C 1 to C 3 alcohols.
Claim 7
Dependent Claim
21 words
The packaged splint of claim 3, wherein said softening agent vapors comprise methyl or ethyl alcohol vapors or a mixture thereof.
Claim 8
Dependent Claim
15 words
The packaged splint of claim 6, wherein said softening agent vapors comprise ethyl alcohol vapors.
Claim 9
Dependent Claim
28 words
The packaged splint of claim 7, wherein said sponge sets to said hardened condition within approximately 15 minutes following removal from said package and exposure to ambient air.
Claim 10
Dependent Claim
21 words
The packaged splint of claim 7, wherein said sponge has a density within the range of approximately 0.49 to 0.87 gm/ml.
Claim 11
Dependent Claim
121 words
A packaged splint for use in forming a hard structure about a body portion, said packaged splint comprising: a layer of polyvinyl acetal sponge made from a polyvinyl alcohol having a molecular weight within the range of approximately 85,000 to approximately 186,000; softening agent vapors associated with said sponge and causing softening of the sponge to permit placement thereof about said body portion; and a package sealingly enclosing said sponge to maintain the softening agent in association with the sponge, said package being constructed to permit removal of the softened sponge from the package for placement about said body portion, whereupon said sponge sets to a hardened state to form said structure as the softening agent vapors disassociate from the sponge.
Claim 12
Dependent Claim
121 words
A packaged splint for use in forming a hard structure about a body portion, said packaged splint comprising: a layer of polyvinyl acetal sponge made from a polyvinyl alcohol having a molecular weight within the range of approximately 85,000 to approximately 186,000; softening agent vapors associated with said sponge and causing softening of the sponge to permit placement thereof about said body portion; and a package sealingly enclosing said sponge to maintain the softening agent in association with the sponge, said package being constructed to permit removal of the softened sponge from the package for placement about said body portion, whereupon said sponge sets to a hardened state to form said structure as the softening agent vapors disassociate from the sponge.
Claim 13
Dependent Claim
28 words
The packaged splint of claim 10, wherein said sponge is made from a polyvinyl alcohol having a molecular weight within the range of approximately 124,000 to approximately 186,000.
Claim 14
Dependent Claim
28 words
The packaged splint of claim 10, wherein said sponge is made from a polyvinyl alcohol having a molecular weight within the range of approximately 160,000 to approximately 186,000.
Claim 15
Dependent Claim
31 words
The packaged splint of claim 10, wherein said softening agent vapors are selected from vapors from the group consisting of C 1 to C 3 alcohol and water and mixtures thereof.
Claim 16
Dependent Claim
26 words
The packaged splint of claim 10, wherein said softening agent vapors are selected from vapors of one or more of C 1 to C 3 alcohols.
Claim 17
Dependent Claim
21 words
The packaged splint of claim 10, wherein said softening agent vapors comprise methyl or ethyl alcohol vapors or a mixture thereof.
Claim 18
Dependent Claim
15 words
The packaged splint of claim 10, wherein said softening agent vapors comprise ethyl alcohol vapors.
Claim 19
Dependent Claim
28 words
The packaged splint of claim 10, wherein said sponge sets to said hardened condition within approximately 15 minutes following removal from said package and exposure to ambient air.
Claim 20
Dependent Claim
21 words
The packaged splint of claim 10, wherein said sponge has a density within the range of approximately 0.49 to 0.87 gm/ml.
References Cited (Backward Citations)
US2194579A
Cited
US2277259A
Cited
US2282274A
Cited
US2609347A
Cited
US2616418A
Cited
US2664367A
Cited
US2653917A
Cited
US2668153A
Cited
US2846407A
Cited
US2847992A
Cited
US3663470A
Cited
US3737398A
Cited
US3849238A
Cited
US4052282A
Cited
US4098728A
Cited
US4066488A
Cited
US4539369A
Cited
US4664662A
Cited
US4852556A
Cited
US4801636A
Cited
US5053455A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1997-02-07 | 1997-08-09 | 1998-02-08 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 2001-02-07 | 2001-08-09 | 2002-02-08 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 2005-02-07 | 2005-08-09 | 2006-02-08 | $7700.00 | Window Closed / Lapsed |