Abstract A composite comprising an unfired ceramic body comprising an admixture of finely divided particles of ceramic solids and sinterable inorganic binder dispersed in a volatilizable solid polymeric binder having affixed and closely conformed to a surface of said body a flexible constraining release layer comprising finely divided particles of non-metallic inorganic solids dispersed in a volatilizable solid polymeric binder, the sinterable inorganic binder of the ceramic body being such that Penetration of said binder into said constraining release layer during subsequent firing is no more than 50 mu m and said constraining release layer being affixed and closely conforming such that upon firing X-Y shrinkage of the ceramic body is reduced. Also, a method for making the composite. The flexible, constraining, release layer substantially reduces and controls green ceramic body shrinkage in the x- and y-directions during firing.
A composite comprising an unfired ceramic body comprising an admixture of finely divided particles of ceramic solids and sinterable inorganic binder dispersed in a volatilizable solid polymeric binder having affixed and closely conformed to a surface of said ceramic body a flexible constraining release layer comprising finely divided particles of non-metallic inorganic solids dispersed in a volatilizable solid polymeric binder, the sinterable inorganic binder of the ceramic body being such that Penetration of said binder into said inorganic constraining release layer during subsequent firing is no more than 50 μm and said constraining release layer being affixed and closely conforming such that upon firing X-Y shrinkage of the ceramic body is reduced.
Claim 2
Dependent Claim
112 words
A composite comprising an unfired ceramic body comprising an admixture of finely divided particles of ceramic solids and sinterable inorganic binder dispersed in a volatilizable solid polymeric binder having affixed and closely conformed to a surface of said ceramic body a flexible constraining release layer comprising finely divided particles of non-metallic inorganic solids dispersed in a volatilizable solid polymeric binder, the sinterable inorganic binder of the ceramic body being such that Penetration of said binder into said inorganic constraining release layer during subsequent firing is no more than 50 μm and said constraining release layer being affixed and closely conforming such that upon firing X-Y shrinkage of the ceramic body is reduced.
Claim 3
Dependent Claim
28 words
The composite of claim 1 in which at least one surface of the unfired ceramic body has printed thereon an unfired pattern of thick film electrically functional paste.
Claim 4
Dependent Claim
22 words
The composite of claim 2 in which the thick film pattern is printed on the constraining layer side of the ceramic body.
Claim 5
Dependent Claim
13 words
The composite of claim 3 in which the thick film pattern is conductive.
Claim 6
Dependent Claim
14 words
The composite of claim 3 in which the thick film pattern is a resistor.
Claim 7
Dependent Claim
20 words
The composite of claim 2 or claim 3 having both resistor and conductor patterns printed on the unfired ceramic body.
Claim 8
Dependent Claim
145 words
A method for making the composite of claim 1 comprising the sequential steps of a. applying to at least one surface of an unfired ceramic body a flexible constraining release layer such that the constraining layer conforms closely to the surface of the ceramic body and reduces X-Y shrinkage of the ceramic body upon firing, the unfired ceramic body comprising an admixture of finely divided particles of ceramic solids and sinterable inorganic binder dispersed in a volatilizable organic medium comprising solid polymeric binder dissolved in volatile organic solvent, the flexible constraining release layer comprising finely divided particles of non-metallic inorganic solids dispersed in volatilizable solid polymeric binder, and sinterable inorganic binder of the ceramic body being such that Penetration of said inorganic binder into said constraining release layer during subsequent firing is no more than 50 μm; and b. removing the organic solvent by evaporation.
Claim 9
Dependent Claim
19 words