Method for controlling corrosion using molybdate compositions

Assignee: ECC SPECIALTY CHEMICALS Inc
•
Filing: 1988-04-21
•
Granted: 1989-01-17
•
Expires: 2008-04-21
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A method for inhibiting corrosion in aqueous systems comprising adding to the system being treated an effective amount of a composition comprising a molybdate ion source and a water-soluble component selected from polymaleic acid anhydride, amine adducts of polymaleic anhydride, maleic anhydride copolymers, carboxylic acid/sulfonic acid polymers, salts of the above-described polymers, phosphonates, phosphino carboxylic acids, polyphosphoric acid and esters of polyphosphoric acid.

Inventors

  • 👤 Bennett P. Boffardi
  • 👤 Susan P. Rey

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-23 20:10
CPC Classifications
C; C23; C23F; C23F11/00; C23F11/08; C23F11/18; C23F11/187; C23F11/188

Claims Analysis

Total Claims: 4
Claim 1
Independent Claim 136 words
A method for inhibiting corrosion in an aqueous system comprising adding to said system an effective amount of a corrosion inhibiting composition comprising: (a) a molybdate ion source; and (b) a water-soluble component selected from the group consisting of polymaleic anhydride; amine adducts of polymaleic anhydride; polymers prepared by polymerizing maleic anhydride with dimethyl diallyl ammonium chloride or homologs thereof; polymers prepared from 50-70%, by weight, acrylic acid or methacrylic acid, 10-40%, by weight, 2-acrylamido-2-methylpropyl sulfonic acid or 2-methyacrylamido-2-methylpropyl sulfonic acid and 10-30%, by weight, of a polyalkyleneoxide compound; salts of the above described polymers; phosphonates selected from the group consisting of 2-phosnphonobutane-1,2,4 tricarboxylic acid and hydroxyphosphono acetic acid; phosphino carboxylic acids; polyphosphoric acid and polyhydroxy esters of polyphosphoric acid; wherein the weight of (a):(b), on an active basis, ranges from about 10:1 to about 1:10.
Claim 2
Independent Claim 136 words
A method for inhibiting corrosion in an aqueous system comprising adding to said system an effective amount of a corrosion inhibiting composition comprising: (a) a molybdate ion source; and (b) a water-soluble component selected from the group consisting of polymaleic anhydride; amine adducts of polymaleic anhydride; polymers prepared by polymerizing maleic anhydride with dimethyl diallyl ammonium chloride or homologs thereof; polymers prepared from 50-70%, by weight, acrylic acid or methacrylic acid, 10-40%, by weight, 2-acrylamido-2-methylpropyl sulfonic acid or 2-methyacrylamido-2-methylpropyl sulfonic acid and 10-30%, by weight, of a polyalkyleneoxide compound; salts of the above described polymers; phosphonates selected from the group consisting of 2-phosnphonobutane-1,2,4 tricarboxylic acid and hydroxyphosphono acetic acid; phosphino carboxylic acids; polyphosphoric acid and polyhydroxy esters of polyphosphoric acid; wherein the weight of (a):(b), on an active basis, ranges from about 10:1 to about 1:10.
Claim 3
Dependent Claim 116 words
A composition comprising: (a) a molybdate ion source; and (b) a water-soluble component selected from the group consisting of polymaleic anhydride; amine adducts of polymaleic anydride; polymers prepared by polymerizing maleic anhydride with dimethyl diallyl ammonium chloride or homologs thereof; polymers prepared from 50-70%, by weight, acrylic acid or methacrylic acid, 10-40%, by weight, 2-acrylamido-2-methylpropyl sulfonic acid or 2-methyacrylamido-2-methylpropyl sulfonic acid and 10-30%, by weight, of a polyalkyleneoxide compound; salts of the above described polymers; phosphonates selected from the group consisting of 2-phosphonobutane-1,2,4 tricarboxylic acid and hydroxyphosphono acetic acid; phosphino carboxylic acids; polyphosphoric acid and polyhydroxy esters of polyphosphoric acid; wherein the weight of (a):(b), on an active basis, ranges from about 10:1 to about 1:10.
Claim 4
Dependent Claim 116 words
A composition comprising: (a) a molybdate ion source; and (b) a water-soluble component selected from the group consisting of polymaleic anhydride; amine adducts of polymaleic anydride; polymers prepared by polymerizing maleic anhydride with dimethyl diallyl ammonium chloride or homologs thereof; polymers prepared from 50-70%, by weight, acrylic acid or methacrylic acid, 10-40%, by weight, 2-acrylamido-2-methylpropyl sulfonic acid or 2-methyacrylamido-2-methylpropyl sulfonic acid and 10-30%, by weight, of a polyalkyleneoxide compound; salts of the above described polymers; phosphonates selected from the group consisting of 2-phosphonobutane-1,2,4 tricarboxylic acid and hydroxyphosphono acetic acid; phosphino carboxylic acids; polyphosphoric acid and polyhydroxy esters of polyphosphoric acid; wherein the weight of (a):(b), on an active basis, ranges from about 10:1 to about 1:10.

References Cited (Backward Citations)

US4176059A Cited
US4409121A Cited
US4440721A Cited
US4548787A Cited
US4640793A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1992-01-17 1992-07-18 1993-01-17 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1996-01-17 1996-07-18 1997-01-17 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2000-01-17 2000-07-18 2001-01-17 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag