Abstract

Abstract A transcutaneous blood carbon dioxide sensor together with a method for making such a sensor and for making electrodes used in the sensor. The sensor comprises a palladium/palladium oxide junction type electrode and a silver/silver halide junction type electrode applied to an electrically nonconductive substrate, partially coated with an insulative dielectric and partially coated with a polymeric membrane material including a bound electrolyte, the polymeric membrane material being permeable to carbon dioxide. The Pd/PD0 electrode was made cathodic prior to terminating the electro-oxidizing conditions.

Inventors

  • 👤 Nicholas Papadakis
  • 👤 Daniel G. Kalynchuk

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-23 14:37
CPC Classifications
A; A61; A61B; A61B5/00; A61B5/145; A61B5/14542; A61B5/14539; A61B5/1468; A61B5/1477; G; G01; G01N; G01N27/00; G01N27/26; G01N27/403; G01N27/404; G01N27/4045; G01N33/00; G01N33/48; G01N33/483; G01N33/487; G01N33/49; G01N33/4925

Claims Analysis

Total Claims: 19
Claim 1
Independent Claim 166 words
A CO 2 gas sensor comprising: an electrically nonconductive substrate; a metal/metal oxide junction type active electrode including an active electrode metal, the active electrode metal being applied to the substrate by one of thick film and thin film techniques, and the active metal being then subjected to electro-oxidizing conditions for a period of time sufficient to oxidize a portion of the applied active electrode metal, the applied active electrode metal being made cathodic prior to discontinuance of the electro-oxidizing conditions; a silver/silver halide junction type reference electrode, adheringly applied to the substrate; an insulating, dielectric coating applied over at least portions of the substrate and electrodes; and a polymeric membrane comprising a laminate of a hydrophobic polymeric material atop a hydrophilic membrane material applied over at least those portions of the electrodes not having the insulating dielectric coating applied thereto, the polymeric membrane being capable of relatively rapidly transmitting CO 2 thereacross, and the polymeric material including a liquid electrolyte bound by the polymeric membrane.
Claim 2
Dependent Claim 166 words
A CO 2 gas sensor comprising: an electrically nonconductive substrate; a metal/metal oxide junction type active electrode including an active electrode metal, the active electrode metal being applied to the substrate by one of thick film and thin film techniques, and the active metal being then subjected to electro-oxidizing conditions for a period of time sufficient to oxidize a portion of the applied active electrode metal, the applied active electrode metal being made cathodic prior to discontinuance of the electro-oxidizing conditions; a silver/silver halide junction type reference electrode, adheringly applied to the substrate; an insulating, dielectric coating applied over at least portions of the substrate and electrodes; and a polymeric membrane comprising a laminate of a hydrophobic polymeric material atop a hydrophilic membrane material applied over at least those portions of the electrodes not having the insulating dielectric coating applied thereto, the polymeric membrane being capable of relatively rapidly transmitting CO 2 thereacross, and the polymeric material including a liquid electrolyte bound by the polymeric membrane.
Claim 3
Independent Claim 141 words
A method for making a solid state pH sensor comprising the steps of: selecting an electrically nonconducting substrate formed from a material selected from a group consisting essentially of ceramics, refractories, thermoplastics, and thermosetting resins; applying an active electrode metal to the substrate by one of thick and thin film techniques to form an electrode of desired physical configuration adhered to the substrate; adheringly applying to the substrate a silver/silver halide junction type reference electrode; oxidizing a portion of the active electrode metal by subjecting the active electrode metal to electro-oxidizing conditions for a period of time necessary to form a desired quantity of an oxide of the metal, the active electrode metal being made cathodic at least immediately prior to terminating the electro-oxidizing conditions; and applying to at least portions of the electrodes and the substrate an insulating dielectric coating.
Claim 4
Independent Claim 141 words
A method for making a solid state pH sensor comprising the steps of: selecting an electrically nonconducting substrate formed from a material selected from a group consisting essentially of ceramics, refractories, thermoplastics, and thermosetting resins; applying an active electrode metal to the substrate by one of thick and thin film techniques to form an electrode of desired physical configuration adhered to the substrate; adheringly applying to the substrate a silver/silver halide junction type reference electrode; oxidizing a portion of the active electrode metal by subjecting the active electrode metal to electro-oxidizing conditions for a period of time necessary to form a desired quantity of an oxide of the metal, the active electrode metal being made cathodic at least immediately prior to terminating the electro-oxidizing conditions; and applying to at least portions of the electrodes and the substrate an insulating dielectric coating.
Claim 5
Dependent Claim 41 words
The method of claim 2, the active electrode metal being applied by thick film screen printing of a precursor compound including the metal onto the substrate and then sintering the applied precursor to provide an active electrode metal upon the substrate.
Claim 6
Dependent Claim 108 words
The method of claim 3, the substrate being alumina, wherein electro-oxidation is accomplished by making the active electrode metal anodic within a fused salt electrolyte consisting of NaNO 3 and LiCl salts under an impressed current of between about 0.1 milliamperes and 20.0 milliamperes per square centimeter of active electrode metal surface, followed by making the active electrode metal cathodic prior to removing the now active electrode from the fused salt electrolyte and including the step of: applying to at least those portions of the electrode not having an applied coating of an insulating dielectric a polymeric membrane capable of binding a liquid electrolyte within the polymeric membrane.
Claim 7
Dependent Claim 108 words
The method of claim 2, the substrate being alumina, wherein electro-oxidation is accomplished by making the active electrode metal anodic within a fused salt electrolyte consisting of NaNO 3 and LiCl salts under an impressed current of between about 0.1 milliamperes and 20.0 milliamperes per square centimeter of active electrode metal surface, followed by making the active electrode metal cathodic prior to removing the now active electrode from the fused salt electrolyte and including the step of: applying to at least those portions of the electrode not having an applied coating of an insulating dielectric a polymeric membrane capable of binding a liquid electrolyte within the polymeric membrane.
Claim 8
Dependent Claim 12 words
A pH sensor produced by the method set forth in claim 3.
Claim 9
Independent Claim 245 words
A method for making a CO 2 gas sensor comprising the steps: selecting an electrically nonconducting substrate formed from a material selected from a group consisting essentially of ceramics, refractories, thermoplastics, and thermosetting resins; applying an active electrode metal to the substrate by one of thick and thin film techniques to form an electrode of desired physical configuration adhered to the substrate; adheringly applying to the substrate a silver/silver halide junction type reference electrode; applying to at least portions of the electrodes and the substrate an insulating dielectric coating; oxidizing a portion of the active electrode metal by subjecting the active electrode metal to electro-oxidizing conditions for a period of time necessary to form a desired quantity of an oxide of the active electrode metal, the active electrode metal being made cathodic prior to terminating the electro-oxidizing conditions; and applying to at least those portions of the resulting sensor not having an applied coating of an insulating dielectric a polymeric membrane comprising a laminate of a hydrophobic polymeric material atop a hydrophilic membrane material capable of binding a liquid electrolyte within the polymeric membrane, electro-oxidation being accomplished by making the active electrode metal anodic within a fused salt electrolyte consisting of NaNO 3 and LiCl salts under an impressed current of between about 0.1 milliamperes and 20.0 milliamperes per square centimeter of active electrode metal surface, followed by making the now active electrode cathodic prior to removing the active electrode from the fused salt electrolyte.
Claim 10
Independent Claim 245 words
A method for making a CO 2 gas sensor comprising the steps: selecting an electrically nonconducting substrate formed from a material selected from a group consisting essentially of ceramics, refractories, thermoplastics, and thermosetting resins; applying an active electrode metal to the substrate by one of thick and thin film techniques to form an electrode of desired physical configuration adhered to the substrate; adheringly applying to the substrate a silver/silver halide junction type reference electrode; applying to at least portions of the electrodes and the substrate an insulating dielectric coating; oxidizing a portion of the active electrode metal by subjecting the active electrode metal to electro-oxidizing conditions for a period of time necessary to form a desired quantity of an oxide of the active electrode metal, the active electrode metal being made cathodic prior to terminating the electro-oxidizing conditions; and applying to at least those portions of the resulting sensor not having an applied coating of an insulating dielectric a polymeric membrane comprising a laminate of a hydrophobic polymeric material atop a hydrophilic membrane material capable of binding a liquid electrolyte within the polymeric membrane, electro-oxidation being accomplished by making the active electrode metal anodic within a fused salt electrolyte consisting of NaNO 3 and LiCl salts under an impressed current of between about 0.1 milliamperes and 20.0 milliamperes per square centimeter of active electrode metal surface, followed by making the now active electrode cathodic prior to removing the active electrode from the fused salt electrolyte.
Claim 11
Independent Claim 234 words
A method for making a transcutaneous blood CO 2 gas sensor comprising the steps: selecting an electrically nonconducting substrate formed from alumina; applying an active electrode metal to the substrate by one of thick and thin film techniques to form an electrode of desired physical configuration adhered to the substrate; adheringly applying to the substrate a silver/silver halide junction type reference electrode; applying to at least portions of the electrodes and the substrate an insulating dielectric coating; oxidizing a portion of the active electrode metal by subjecting the active electrode metal to electro-oxidizing conditions for a period of time necessary to form a desired quantity of an oxide of the active electrode metal, the active electrode metal being made cathodic prior to terminating the electro-oxidizing conditions; and applying to at least those portions of the resulting sensor not having an applied coating of an insulating dielectric a polymeric membrane comprising a laminate of a hydrophobic polymer material atop a hydrophilic membrane material capable of binding a liquid electrolyte within the polymeric membrane, and wherein electro-oxidation is accomplished by making the active electrode anodic within a fused salt electrolyte consisting of NaNO 3 and LiCl salts under an impressed current of between about 0.1 milliamperes and 20.0 milliamperes per square centimeter of active electrode metal surface, followed by making the now active electrode cathodic prior to removing the active electrode from the fused salt electrolyte.
Claim 12
Independent Claim 234 words
A method for making a transcutaneous blood CO 2 gas sensor comprising the steps: selecting an electrically nonconducting substrate formed from alumina; applying an active electrode metal to the substrate by one of thick and thin film techniques to form an electrode of desired physical configuration adhered to the substrate; adheringly applying to the substrate a silver/silver halide junction type reference electrode; applying to at least portions of the electrodes and the substrate an insulating dielectric coating; oxidizing a portion of the active electrode metal by subjecting the active electrode metal to electro-oxidizing conditions for a period of time necessary to form a desired quantity of an oxide of the active electrode metal, the active electrode metal being made cathodic prior to terminating the electro-oxidizing conditions; and applying to at least those portions of the resulting sensor not having an applied coating of an insulating dielectric a polymeric membrane comprising a laminate of a hydrophobic polymer material atop a hydrophilic membrane material capable of binding a liquid electrolyte within the polymeric membrane, and wherein electro-oxidation is accomplished by making the active electrode anodic within a fused salt electrolyte consisting of NaNO 3 and LiCl salts under an impressed current of between about 0.1 milliamperes and 20.0 milliamperes per square centimeter of active electrode metal surface, followed by making the now active electrode cathodic prior to removing the active electrode from the fused salt electrolyte.
Claim 13
Dependent Claim 41 words
The method of claim 8, the active electrode metal being applied by thick film screen printing of a precursor compound including the metal onto the substrate and then sintering the applied precursor to provide an active electrode metal upon the substrate.
Claim 14
Independent Claim 110 words
A method for making a precious metal/precious metal oxide junction type electrode comprising the steps of: selecting a precious metal electrode precursor the metal being selected from a group consisting of palladium, iridium, rhodium, ruthenium and osmium; immersing at least a portion of the electrical precursor in a molten salt electrolyte; making the electrode precursor anodic at an electrical current not exceeding about 20 milliamperes per square centimeter of immersed electrode precursor to form a desired quantity of the precious metal oxide; and at least once making the electrode precursor cathodic prior to removal from the molten salt electrolyte at an electrical current not exceeding the current density while anodic.
Claim 15
Independent Claim 110 words
A method for making a precious metal/precious metal oxide junction type electrode comprising the steps of: selecting a precious metal electrode precursor the metal being selected from a group consisting of palladium, iridium, rhodium, ruthenium and osmium; immersing at least a portion of the electrical precursor in a molten salt electrolyte; making the electrode precursor anodic at an electrical current not exceeding about 20 milliamperes per square centimeter of immersed electrode precursor to form a desired quantity of the precious metal oxide; and at least once making the electrode precursor cathodic prior to removal from the molten salt electrolyte at an electrical current not exceeding the current density while anodic.
Claim 16
Dependent Claim 107 words
A solid state pH sensor comprising: an electrically nonconductive substrate; a metal/metal oxide junction type active electrode including an active electrode metal, the active electrode metal being applied to the substrate by one of thick film and thin film techniques, and the active metal being then subjected to electro-oxidizing conditions for a period of time sufficient to oxidize a portion of the applied active electrode, the applied active electrode metal being made cathodic prior to discontinuance of the electro-oxidizing conditions; a metal/metal halide junction type reference electrode, adheringly applied to the substrate; and an insulating, dielectric coating applied over at least portions of the substrate and electrodes.
Claim 17
Dependent Claim 107 words
A solid state pH sensor comprising: an electrically nonconductive substrate; a metal/metal oxide junction type active electrode including an active electrode metal, the active electrode metal being applied to the substrate by one of thick film and thin film techniques, and the active metal being then subjected to electro-oxidizing conditions for a period of time sufficient to oxidize a portion of the applied active electrode, the applied active electrode metal being made cathodic prior to discontinuance of the electro-oxidizing conditions; a metal/metal halide junction type reference electrode, adheringly applied to the substrate; and an insulating, dielectric coating applied over at least portions of the substrate and electrodes.
Claim 18
Dependent Claim 33 words
The sensor of claim 11 including a polymeric membrane capable of supporting hydrogen ion transport thereacross applied over at least those portions of the electrodes not having the insulating dielectric coating applied thereto.
Claim 19
Dependent Claim 21 words
The sensor of claim 11 wherein the metal/metal oxide electrode is palladium/palladium oxide and the metal/metal halide electrode is silver/silver halide.

References Cited (Backward Citations)

DE2148260A1 Cited
US3709810A Cited
US3705088A Cited
US3671414A Cited
US3856649A Cited
US3905889A Cited
US4133735A Cited
US4324256A Cited
FR2426904A1 Cited
US4409980A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1988-08-19 1989-02-18 1989-08-20 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1992-08-19 1993-02-18 1993-08-20 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1996-08-19 1997-02-18 1997-08-20 $7700.00 Window Closed / Lapsed