Abstract Storable polypropylene ether polyurethane compositions composed of (a) a prepolymer of a polypropylene ether glycol and sufficient organic polyisocyanate to give preferably an excess of about 3 to 15 percent NCO in said prepolymer with the proviso that the free NCO is obtained from methylenedi-p-phenyl diisocyanate and (b) a complex of an alkali metal salt with 4,4'-methylenedianiline (MDA), said composition being relatively inactive at temperatures below 100° C., but being heat activatible at much higher temperatures to effect a cure. The improved composition wherein a catalyst is present in said composition which effectively lowers the cure temperature, said catalyst being a pseudocrown ether containing radicals having the formula --y--CH 2 --CH 2 ) n with y being nitrogen, sulfur or oxygen and n has values sufficient to form the crown structure, viz., at least 3 or more.
The storable polypropylene ether polyurethane composition comprising a mixture of (a) an equivalent of a prepolymer formed by reacting a polypropylene ether polyol of 2 to 6 OH with sufficient organic polyisocyanate to give an excess of about 3 to 15 percent by weight of free NCO in said prepolymer with the proviso that the free NCO is obtained from methane di(phenyl isocyanate); (b) 0.7 to 1.05 equivalents of a complex of an alkali metal salt with 4,4'-methylenedianiline, said alkali metal being selected from the class consisting of sodium, potassium and lithium; and (c) a catalyst for said complex consisting of a crown or pseudocrown ether, said ether being composed of radicals having the structural formula --y--CH 2 --CH 2 ) n where y can be nitrogen, sulfur or oxygen and n is a number 3 to 100.
Claim 2
Dependent Claim
138 words
The storable polypropylene ether polyurethane composition comprising a mixture of (a) an equivalent of a prepolymer formed by reacting a polypropylene ether polyol of 2 to 6 OH with sufficient organic polyisocyanate to give an excess of about 3 to 15 percent by weight of free NCO in said prepolymer with the proviso that the free NCO is obtained from methane di(phenyl isocyanate); (b) 0.7 to 1.05 equivalents of a complex of an alkali metal salt with 4,4'-methylenedianiline, said alkali metal being selected from the class consisting of sodium, potassium and lithium; and (c) a catalyst for said complex consisting of a crown or pseudocrown ether, said ether being composed of radicals having the structural formula --y--CH 2 --CH 2 ) n where y can be nitrogen, sulfur or oxygen and n is a number 3 to 100.
Claim 3
Dependent Claim
15 words
The composition of claim 1 wherein the catalyst is the dimethyl ether of tetraethylene glycol.
Claim 4
Dependent Claim
20 words
The polyurethane composition of claim 1 wherein the polypropylene ether glycol has a molecular weight of about 900 to 4500.
Claim 5
Dependent Claim
24 words
The polyurethane composition of claim 1 containing a small amount to about 50 parts of silicate filler per 100 parts of the polyurethane composition.
Claim 6
Dependent Claim
12 words
The polyurethane composition of claim 3 wherein the silicate filler is talc.
Claim 7
Dependent Claim
16 words
The polyurethane composition of claim 1 wherein the free NCO is about 5 to 10 percent.
Claim 8
Dependent Claim
14 words
The polyurethane composition of claim 1 wherein y in the repeating radical is oxygen.
Claim 9
Dependent Claim
22 words
The polyurethane composition of claim 1 wherein the catalyst is present in from 0.1 to 20 parts per hundred of said prepolymer.