Method of fabricating a socket type electrical contact
Assignee: Amphenol Corp
•
Filing: 1981-01-26
•
Granted: 1983-08-09
•
Expires: 2001-01-26
Abstract
Abstract A method of making a gold plated socket contact characterized by heat treating in a vacuum furnace the previously formed and partially gold plated inner sleeve (10) of a three piece contact assembly.
Inventors
- 👤 John G. Bickos
- 👤 Gilbert G. Warren
- 👤 R. Amelia Piscitelli
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-23 17:11
CPC Classifications
H; H01; H01R; H01R43/00; H01R43/16; H01R13/00; H01R13/02; H01R13/03; H01R13/10; H01R13/11; H01R13/111; Y; Y10; Y10T; Y10T29/00; Y10T29/49; Y10T29/49002; Y10T29/49117; Y10T29/49204; Y10T29/49208; Y10T29/49224
Claims Analysis
Total Claims: 5
Claim 1
Independent Claim
130 words
A method of fabricating a socket type electrical contact for use in an electrical connector comprising the steps of: plating a strip of beryllium copper with nickel; plating only one end portion of one side of said strip with a first layer of gold to a thickness of at least 0.625 micrometers; stamping, from said sheet a rectangularly shaped piece having a plurality of fingers extending longitudinally from one end of said piece; forming said rectangular piece into a tubular form; heating said tubular form in a vacuum furnace at a pressure below 50 microns for at least 2 hours and 15 mintues at a temperature of about 489 degrees centigrade; and plating the entire tubular form with a second layer of gold to a thickness less than 0.250 micrometers.
Claim 2
Independent Claim
130 words
A method of fabricating a socket type electrical contact for use in an electrical connector comprising the steps of: plating a strip of beryllium copper with nickel; plating only one end portion of one side of said strip with a first layer of gold to a thickness of at least 0.625 micrometers; stamping, from said sheet a rectangularly shaped piece having a plurality of fingers extending longitudinally from one end of said piece; forming said rectangular piece into a tubular form; heating said tubular form in a vacuum furnace at a pressure below 50 microns for at least 2 hours and 15 mintues at a temperature of about 489 degrees centigrade; and plating the entire tubular form with a second layer of gold to a thickness less than 0.250 micrometers.
Claim 3
Dependent Claim
37 words
The method as recited in claim 1 including the steps of: placing an intermediate sleeve over said tubular form; and placing an outer sleeve over a portion of the intermediate sleeve that surrounds the plurality of fingers.
Claim 4
Independent Claim
25 words
The method as recited in claims 1 or 2 wherein the first layer of gold comprises a band along each end portion of said strip.
Claim 5
Dependent Claim
37 words
The method as recited in claim 1 including the steps of: placing a sleeve over the portion of the tubular form having the fingers; and placing another sleeve over the opposite end portion of said tubular form.
References Cited (Backward Citations)
DE515579C
Cited
US2816066A
Cited
US3364064A
Cited
US3953246A
Cited
US4072394A
Cited
US4120556A
Cited
US4136923A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1986-08-08 | 1987-02-07 | 1987-08-09 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1990-08-08 | 1991-02-07 | 1991-08-09 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1994-08-08 | 1995-02-07 | 1995-08-09 | $7700.00 | Window Closed / Lapsed |