Patent US4337090A successfully refreshed from Google Patents.
← Back to Patent Explorer
US4337090A Expired / Lapsed US ⏱️ 0.0 years remaining

Heat recoverable nickel/titanium alloy with improved stability and machinability

Assignee: Memry Corp
•
Filing: 1980-09-05
•
Granted: 1982-06-29
•
Expires: 2000-09-05
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Nickel/titanium alloys containing less than a stoichiometric quantity of titanium, which are capable of having the property of heat recoverability imparted thereto at a temperature above the boiling point of liquid nitrogen, may be stabilized by the addition of from 1.5 to 9 atomic percent copper. These stabilized alloys also possess improved workability and machinability.

Inventors

  • 👤 John D. Harrison

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-23 11:49
CPC Classifications
C; C22; C22C; C22C19/00; C22C19/03; C22F; C22F1/00; C22F1/006

Claims Analysis

Total Claims: 4
Claim 1
Independent Claim 99 words
A shape memory alloy consisting essentially of nickel, titanium and copper within an area defined on a nickel, titanium, and copper ternary phase diagram by a triangle with its first vertex at 49.7 atomic percent nickel, 48.8 atomic percent titanium, and 1.5 atomic percent copper; its second vertex at 47.5 atomic percent nickel, 47.5 atomic percent titanium, and 5.0 atomic percent copper; and its third vertex at 47.5 atomic percent nickel, 43.5 atomic percent titanium, and 9.0 atomic percent copper, said alloy possessing improved temper stability and machinability and having an A 50 between -50° C. and -196° C.
Claim 2
Dependent Claim 99 words
A shape memory alloy consisting essentially of nickel, titanium and copper within an area defined on a nickel, titanium, and copper ternary phase diagram by a triangle with its first vertex at 49.7 atomic percent nickel, 48.8 atomic percent titanium, and 1.5 atomic percent copper; its second vertex at 47.5 atomic percent nickel, 47.5 atomic percent titanium, and 5.0 atomic percent copper; and its third vertex at 47.5 atomic percent nickel, 43.5 atomic percent titanium, and 9.0 atomic percent copper, said alloy possessing improved temper stability and machinability and having an A 50 between -50° C. and -196° C.
Claim 3
Dependent Claim 116 words
A shape memory alloy consisting essentially of nickel, titanium and copper within an area defined on a nickel, titanium, and copper ternary phase diagram by a quadrilateral with its first vertex at 49.7 atomic percent nickel, 48.8 atomic percent titanium, and 1.5 atomic percent copper; its second vertex at 47.5 atomic percent nickel, 47.5 atomic percent titanium, and 5.0 atomic percent copper; its third vertex at 47.5 atomic percent nickel, 46.0 atomic percent titanium, and 6.5 atomic percent copper; and its fourth vertex at 48.9 atomic percent nickel, 46.8 atomic percent titanium, and 4.3 atomic percent copper, said alloy possessing improved temper stability and machinability and having an A 50 between -50° C. and -196° C.
Claim 4
Dependent Claim 116 words
A shape memory alloy consisting essentially of nickel, titanium and copper within an area defined on a nickel, titanium, and copper ternary phase diagram by a quadrilateral with its first vertex at 49.7 atomic percent nickel, 48.8 atomic percent titanium, and 1.5 atomic percent copper; its second vertex at 47.5 atomic percent nickel, 47.5 atomic percent titanium, and 5.0 atomic percent copper; its third vertex at 47.5 atomic percent nickel, 46.0 atomic percent titanium, and 6.5 atomic percent copper; and its fourth vertex at 48.9 atomic percent nickel, 46.8 atomic percent titanium, and 4.3 atomic percent copper, said alloy possessing improved temper stability and machinability and having an A 50 between -50° C. and -196° C.

References Cited (Backward Citations)

US3174851A Cited
US3351463A Cited
US3558369A Cited
US3832243A Cited
US3753700A Cited
US3740839A Cited
US4198081A Cited
US4035077A Cited
CH606456A5 Cited
US4144057A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1985-06-28 1985-12-28 1986-06-29 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1989-06-28 1989-12-28 1990-06-29 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1993-06-28 1993-12-28 1994-06-29 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag