Abstract An improved diamond abrasive tool and method of manufacture characterized by a direct brazing technique of diamond crystals to a substrate surface which requires no pre-conditioning of the surface of the diamond in order to obtain the necessary wetting thereof. The method employed utilizes readily available, very hard and durable brazing alloys which have been discovered to readily wet the diamond surface to obtain a final product wherein the minimum depth of the alloy bond tends to occur intermediate adjacent diamond crystals with outstanding retention of the crystals and greatly extended tool life.

Inventors

  • 👤 James T. Lowder
  • 👤 Edwin M. Tausch

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-23 10:58
CPC Classifications
B; B23; B23K; B23K35/00; B23K35/22; B23K35/24; B23K35/30; B23K35/3033; B23K35/304; B23K1/00; B23K1/19; B24; B24D; B24D18/00; B24D3/00; B24D3/02; B24D3/04; B24D3/06; B24D3/08

Claims Analysis

Total Claims: 6
Claim 1
Independent Claim 109 words
A diamond abrasive tool comprising, in combination, a metal substrate and a monolayer of diamond crystals bonded on said substrate by a braze alloy comprising approximately 60 to 92 percent by weight of one of the metals selected from the group consisting of nickel and cobalt or mixtures thereof and no more than approximately 12 percent of one or more of the elements selected from the group consisting of boron, silicon and phosphorous and a chromium content between at least approximately 2 to approximately 30 percent by weight, said tool characterized by a configuration wherein the braze alloy bond has its minimum depth at a point intermediate adjacent crystals.
Claim 2
Dependent Claim 109 words
A diamond abrasive tool comprising, in combination, a metal substrate and a monolayer of diamond crystals bonded on said substrate by a braze alloy comprising approximately 60 to 92 percent by weight of one of the metals selected from the group consisting of nickel and cobalt or mixtures thereof and no more than approximately 12 percent of one or more of the elements selected from the group consisting of boron, silicon and phosphorous and a chromium content between at least approximately 2 to approximately 30 percent by weight, said tool characterized by a configuration wherein the braze alloy bond has its minimum depth at a point intermediate adjacent crystals.
Claim 3
Dependent Claim 48 words
The diamond tool of claim 1 wherein said braze alloy includes more than approximately 5% and less than approximately 26 percent chromium and one or more metals taken from the group comprising boron, silicon, and phosphorus which individually or together comprise no more than 10% of the alloy.
Claim 4
Dependent Claim 80 words
A diamond tool comprising in combination, a metal substrate and a monolayer of diamond crystals bonded on said substrate by an alloy comprising approximately 60 to 92 percent nickel, between approximately 5 and 15 percent chromium and less than approximately 10 percent of one or more elements selected from the group consisting of boron, silicon and phosphorus said tool being characterized by a configuration wherein the braze alloy bond exhibits a minimum depth at a point intermediate adjacently bonded crystals.
Claim 5
Dependent Claim 80 words
A diamond tool comprising in combination, a metal substrate and a monolayer of diamond crystals bonded on said substrate by an alloy comprising approximately 60 to 92 percent nickel, between approximately 5 and 15 percent chromium and less than approximately 10 percent of one or more elements selected from the group consisting of boron, silicon and phosphorus said tool being characterized by a configuration wherein the braze alloy bond exhibits a minimum depth at a point intermediate adjacently bonded crystals.
Claim 6
Dependent Claim 49 words
A diamond tool as defined in claim 3 wherein said braze alloy includes less than a total of approximately 12 percent by weight of one or more elements taken from a group consisting of boron, silicon and phosphorus and possesses a melting point of less than approximately 1200° C.

References Cited (Backward Citations)

US2138882A Cited
US2201196A Cited
US2233175A Cited
US3598554A Cited
US3630699A Cited
US3751283A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1980-04-18 1980-10-18 1981-04-19 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1984-04-18 1984-10-18 1985-04-19 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1988-04-18 1988-10-18 1989-04-19 $7700.00 Window Closed / Lapsed