US3995089A Expired / Lapsed US ⏱️ 0.0 years remaining

Magnetic recording media

Assignee: BASF SE
•
Filing: 1975-04-02
•
Granted: 1976-11-30
•
Expires: 1995-04-02
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A magnetic recording medium in the form of a card having a non-magnetic support with a magnetic coating on one side of the support and a backcoating on the opposite side of the support, which backcoating exhibits improved scratch resistance and adherence to the support and improved frictional characteristics and consists essentially of 20 to 50% by weight of a binder mixture containing 10 to 60% by weight of an elastomeric polyurethane and, incorporated in the binder mixture, a non-magnetic pulverulent mixture of 10 to 40% by weight of conductive carbon powder and 60 to 90% by weight of platelet-shaped and spherical particles.

Inventors

  • 👤 Job Werner Hartmann
  • 👤 Hans-Joerg Hartmann
  • 👤 Dieter Mayer
  • 👤 Peter Felleisen
  • 👤 Ursula Klein
  • 👤 Herbert Motz

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-23 14:17
CPC Classifications
G; G11; G11B; G11B5/00; G11B5/62; G11B5/68; G11B5/70; G11B5/708; Y; Y10; Y10S; Y10S428/00; Y10S428/90; Y10T; Y10T428/00; Y10T428/24; Y10T428/24355; Y10T428/24372; Y10T428/24413; Y10T428/26; Y10T428/263; Y10T428/264; Y10T428/265; Y10T428/31504; Y10T428/31551; Y10T428/31609

Claims Analysis

Total Claims: 6
Claim 1
Independent Claim 165 words
A magnetic recording medium in card form comprising a flat non-magnetic support, a magnetic coating on one side of the support and a backcoating comprising polymeric binder, conductive particles and non-magnetic pigments on the opposite side of the support, wherein the said backcoating consists essentially of i. 20 to 50% by weight of a binder containing 10 to 60% by weight of an elastomeric flexible polyurethane substantially free of isocyanate groups, and ii. a non-magnetic pulverulent mixture of 10 to 40 parts by weight of conductive carbon powder (a), 40 to 90 parts by weight of an intimate mixture (b) of 20 to 45% by weight of kaolinite powder having platelet-shaped particles and 55 to 80% by weight of quartz powder having spherical particles, and optionally 5 to 40 parts by weight of corundum powder (c) having spherical particles the coefficient of friction (C m ) between the back surface of a card and the magnetized surface of an adjacent card being less than 0.50.
Claim 2
Dependent Claim 165 words
A magnetic recording medium in card form comprising a flat non-magnetic support, a magnetic coating on one side of the support and a backcoating comprising polymeric binder, conductive particles and non-magnetic pigments on the opposite side of the support, wherein the said backcoating consists essentially of i. 20 to 50% by weight of a binder containing 10 to 60% by weight of an elastomeric flexible polyurethane substantially free of isocyanate groups, and ii. a non-magnetic pulverulent mixture of 10 to 40 parts by weight of conductive carbon powder (a), 40 to 90 parts by weight of an intimate mixture (b) of 20 to 45% by weight of kaolinite powder having platelet-shaped particles and 55 to 80% by weight of quartz powder having spherical particles, and optionally 5 to 40 parts by weight of corundum powder (c) having spherical particles the coefficient of friction (C m ) between the back surface of a card and the magnetized surface of an adjacent card being less than 0.50.
Claim 3
Dependent Claim 38 words
A magnetic recording medium as set forth in claim 1 wherein the non-magnetic pulverulent mixture consists of 10 to 25 parts by weight of carbon black powder (a) and 75 to 90 parts by weight of mixture (b).
Claim 4
Dependent Claim 49 words
A magnetic recording medium as set forth in claim 1 wherein the non-magnetic pulverulent mixture consists of 10 to 40 parts by weight of conductive carbon powder (a), 40 to 85 parts by weight of mixture (b) and 5 to 40 parts by weight of corundum powder (c) .
Claim 5
Dependent Claim 23 words
A magnetic recording media as set forth in claim 1 in which said backcoating has a thickness of from 7 to 13 μ.
Claim 6
Dependent Claim 23 words
A magnetic recording media as set forth in claim 1 in which said backcoating has a thickness of from 9 to 11 μ.

References Cited (Backward Citations)

US2804401A Cited
US3293066A Cited
US3687725A Cited
US3617378A Cited
US3734772A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1979-11-30 1980-05-31 1980-11-30 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1983-11-30 1984-05-31 1984-11-30 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1987-11-30 1988-05-31 1988-11-30 $7700.00 Window Closed / Lapsed