Process for making decorative sheet-like articles
Assignee: Chavannes Industrial Synthetics Inc
•
Filing: 1946-10-31
•
Granted: 1952-03-04
•
Expires: 1966-10-31
Abstract
No abstract record available.
Inventors
- 👤 Marc A Chavannes
- 👤 Leon E Magoon
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-23 04:23
CPC Classifications
B; B44; B44C; B44C1/00; B44C1/22; B29; B29C; B29C41/00; B29C41/24; B29C41/28; B29D; B29D7/00; B32; B32B; B32B27/00; B44C1/16; B44C3/00; B44C3/08; B29C71/00; Y; Y10; Y10T; Y10T428/00; Y10T428/24; Y10T428/24479; Y10T428/24521; Y10T428/2457; Y10T428/24612; Y10T428/2462; Y10T428/24802
Claims Analysis
Total Claims: 2
Claim 1
Independent Claim
181 words
A METHOD OF PRODUCING A FLEXIBLE VINYL FILM HAVING A TWO-TONED IRREGULAR SURFACE, COMPRISING THE STEPS OF APPLYING A FLUID SUBSTANCE INCLUDING A VINYL RESIN TO ONLY THE HIGH REGIONS OF AN EMBOSSED SURFACE OF AN ADVANCING FLEXIBLE CARRIER, SO AS TO LEAVE EXPOSED THE LOW REGIONS OF SAID SURFACE, DRYING SAID SUBSTANCE ON SAID HIGH REGIONS, SAID SURFACE BEING ONLY LIGHTLY ADHESIVE TO VINYL RESIN WHEN THE LATTER IS DRIED THEREON, FORMING OVER SAID EXPOSED LOW REGIONS OF SAID SURFACE AND OVER SAID DRIED, FIRST-APPLIED SUBSTANCE ON SAID HIGH REGIONS A CONTINUOUS LAYER OF A FILM-FORMING DISPERSION COMPRISING A VINYL RESIN, A PLASTICIZER, AND A DILUENT, SAID DISPERSION BEING SUFFICIENTLY INERT IN RELATION TO SAID DRIED FIRST-APPLIED SUBSTANCE NOT TO DISSOLVED SAME AND DESTROY THE PATTERN THEREOF, AND BEING COLORED DIFFERENTLY FROM SAID FIRST-APPLIED SUBSTANCE, DRYING SAID LAYER, BONDING SAID DRIED LAYER PERMANENTLY TO SAID DRIED FIRST-APPLIED SUBSTANCE BY HEATING THEM TO A FUSING TEMPERATURE, AND STRIPPING SAID LAYER TOGETHER WITH SAID FIRST-APPLIED SUBSTANCE FROM SAID CARRIER BY APPLYING TENSION TO SAID LAYER IN A DIRECTION AWAY FROM SAID CARRIER.
Claim 2
Independent Claim
181 words
A METHOD OF PRODUCING A FLEXIBLE VINYL FILM HAVING A TWO-TONED IRREGULAR SURFACE, COMPRISING THE STEPS OF APPLYING A FLUID SUBSTANCE INCLUDING A VINYL RESIN TO ONLY THE HIGH REGIONS OF AN EMBOSSED SURFACE OF AN ADVANCING FLEXIBLE CARRIER, SO AS TO LEAVE EXPOSED THE LOW REGIONS OF SAID SURFACE, DRYING SAID SUBSTANCE ON SAID HIGH REGIONS, SAID SURFACE BEING ONLY LIGHTLY ADHESIVE TO VINYL RESIN WHEN THE LATTER IS DRIED THEREON, FORMING OVER SAID EXPOSED LOW REGIONS OF SAID SURFACE AND OVER SAID DRIED, FIRST-APPLIED SUBSTANCE ON SAID HIGH REGIONS A CONTINUOUS LAYER OF A FILM-FORMING DISPERSION COMPRISING A VINYL RESIN, A PLASTICIZER, AND A DILUENT, SAID DISPERSION BEING SUFFICIENTLY INERT IN RELATION TO SAID DRIED FIRST-APPLIED SUBSTANCE NOT TO DISSOLVED SAME AND DESTROY THE PATTERN THEREOF, AND BEING COLORED DIFFERENTLY FROM SAID FIRST-APPLIED SUBSTANCE, DRYING SAID LAYER, BONDING SAID DRIED LAYER PERMANENTLY TO SAID DRIED FIRST-APPLIED SUBSTANCE BY HEATING THEM TO A FUSING TEMPERATURE, AND STRIPPING SAID LAYER TOGETHER WITH SAID FIRST-APPLIED SUBSTANCE FROM SAID CARRIER BY APPLYING TENSION TO SAID LAYER IN A DIRECTION AWAY FROM SAID CARRIER.
References Cited (Backward Citations)
US1876432A
Cited
US986162A
Cited
US1733469A
Cited
US1920118A
Cited
US1961025A
Cited
US2144388A
Cited
GB500298A
Cited
US2273700A
Cited
US2326001A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1955-03-04 | 1955-09-03 | 1956-03-04 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1959-03-04 | 1959-09-03 | 1960-03-04 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1963-03-04 | 1963-09-03 | 1964-03-04 | $7700.00 | Window Closed / Lapsed |