Claims Analysis
Total Claims: 34
Claim 1
Independent Claim
63 words
An elongated member configured for advancement within a body lumen which is formed at least in part of a cold worked biocompatible alloy consisting essentially of 28 to 65% by wt. cobalt, 2 to 40% by wt. nickel, 5 to 35% by wt. chromium, up to 12% by wt. molybdenum, up to 20% by wt. tungsten and up to 20% by wt. iron.
Claim 2
Dependent Claim
63 words
An elongated member configured for advancement within a body lumen which is formed at least in part of a cold worked biocompatible alloy consisting essentially of 28 to 65% by wt. cobalt, 2 to 40% by wt. nickel, 5 to 35% by wt. chromium, up to 12% by wt. molybdenum, up to 20% by wt. tungsten and up to 20% by wt. iron.
Claim 3
Dependent Claim
37 words
The elongated member of claim 1 wherein the cold worked biocompatible alloy includes 30 to 45% by wt. cobalt, 25 to 37% by wt. nickel, and 25% by wt. chromium and 5 to 15% by wt. molybdenum.
Claim 4
Dependent Claim
16 words
The elongated member of claim 2 wherein the cold worked biocompatible alloy has been age hardened.
Claim 5
Dependent Claim
12 words
The elongated member of claim 1 in the form of a guidewire.
Claim 6
Dependent Claim
18 words
The elongated member of claim 1 wherein a distal portion thereof is formed of a pseudoelastic NiTi alloy.
Claim 7
Dependent Claim
47 words
A composite product comprising: a) a first portion formed of a high strength alloy containing 28 to 65% by wt. cobalt, 2 to 40% by wt. nickel and 5 to 35% by wt. chromium; and b) a second portion formed of an alloy of nickel and titanium.
Claim 8
Dependent Claim
47 words
A composite product comprising: a) a first portion formed of a high strength alloy containing 28 to 65% by wt. cobalt, 2 to 40% by wt. nickel and 5 to 35% by wt. chromium; and b) a second portion formed of an alloy of nickel and titanium.
Claim 9
Dependent Claim
29 words
The composite product of claim 6 wherein the second portion exhibits a stress induced transformation from an austenite phase which is stable at body temperature to a martensite phase.
Claim 10
Dependent Claim
32 words
The composite product of claim 6 having an elongated shape with the second portion being an elongated inner member and the first portion being an outer sheath disposed about the inner member.
Claim 11
Dependent Claim
38 words
The composite product of claim 8 wherein the composite product has proximal and distal sections and has at least a portion of the outer sheath removed from the inner member in at least part of the distal section.
Claim 12
Dependent Claim
24 words
The composite product of claim 9 wherein the inner member in the distal section tapers in the distal direction to a smaller transverse dimension.
Claim 13
Dependent Claim
88 words
A co-worked high strength elongated composite intracorporeal device comprising: a) a first member formed of a pseudoelastic NiTi alloy which has; desirable mechanical properties due to having been subjected to certain thermomechanical processing; and b) a second member secured to the first member formed of a high strength alloy which contains 28 to 65% by wt. cobalt, 2 to 40% by wt. nickel and 5 to 35% by wt. chromium and which has been subjected to the same thermomechanical processing to which the first member has been subjected.
Claim 14
Dependent Claim
88 words
A co-worked high strength elongated composite intracorporeal device comprising: a) a first member formed of a pseudoelastic NiTi alloy which has; desirable mechanical properties due to having been subjected to certain thermomechanical processing; and b) a second member secured to the first member formed of a high strength alloy which contains 28 to 65% by wt. cobalt, 2 to 40% by wt. nickel and 5 to 35% by wt. chromium and which has been subjected to the same thermomechanical processing to which the first member has been subjected.
Claim 15
Dependent Claim
33 words
The intracorporeal device of claim 11 wherein the thermomechanical processing includes a plurality of cold working stages with intermediate anneals and a final cold working stage followed by an age hardening heat treatment.
Claim 16
Dependent Claim
66 words
An elongated guidewire for intracorporeal use comprising: a) a core member having an inner portion formed of a pseudoelastic NiTi alloy; and an outer portion formed of a high strength alloy which contains 28 to 65% by wt. cobalt, 2 to 40% by wt. nickel and 5 to 35% by wt. chromium; and b) a helical coil disposed about a distal portion of the core member.
Claim 17
Dependent Claim
66 words
An elongated guidewire for intracorporeal use comprising: a) a core member having an inner portion formed of a pseudoelastic NiTi alloy; and an outer portion formed of a high strength alloy which contains 28 to 65% by wt. cobalt, 2 to 40% by wt. nickel and 5 to 35% by wt. chromium; and b) a helical coil disposed about a distal portion of the core member.
Claim 18
Dependent Claim
32 words
The elongated guidewire of claim 13 having proximal and distal sections with a length of the outer portion removed to expose the underlying inner portion in the distal section of the guidewire.
Claim 19
Dependent Claim
20 words
The elongated guidewire of claim 14 wherein the helical coil is disposed about the exposed portion of the core member.
Claim 20
Dependent Claim
24 words
The elongated guidewire of claim 15 wherein the helical coil is secured by its proximal portion to the outer portion of the core member.
Claim 21
Dependent Claim
37 words
The elongated guidewire of claim 16 wherein a shapeable ribbon having proximal and distal ends is secured by its distal end to the distal end of the coil and by its proximal end to the core member.
Claim 22
Dependent Claim
20 words
The elongated guidewire of claim 16 wherein the helical coil is secured by its distal end to the core member.
Claim 23
Dependent Claim
62 words
The elongated guidewire of claim 13 wherein the Co--Ni--Cr alloy consists essentially of 28 to 65% by wt. cobalt, 2 to 40% by wt. nickel, and 5% to 35% by wt. chromium and up to 12% by wt. molybdenum, up to 20% by wt. tungsten, up to 20% by wt. iron and the balance inconsequential amounts of other alloying constituents and impurities.
Claim 24
Dependent Claim
38 words
The elongated guidewire of claim 19 wherein the Co--Ni--Cr alloy includes 30 to 45% by wt. cobalt, 25 to 37% by wt. nickel, 15 to 25% by wt. chromium and about 5 to about 15% by wt. molybdenum.
Claim 25
Dependent Claim
37 words
The elongated guidewire of claim 13 wherein the Ni--Ti alloy consists essentially of 25 to 47% by wt. titanium and the balance nickel and up to about 10% by wt. of one or more additional alloying elements.
Claim 26
Dependent Claim
40 words
The elongated guidewire of claim 21 wherein the additional alloying elements are selected from the group consisting of up to 3% by wt. of iron, cobalt, chromium, platinum and palladium and up to about 10% by wt. copper and vanadium.
Claim 27
Independent Claim
73 words
A method of making an elongated composite product comprising: a) providing an elongated outer sheath formed of a Co--Ni--Cr alloy with an inner lumen extending therein; b) advancing an elongated core member formed of NiTi alloy into the inner lumen of the outer sheath to form an assembly therewith; and c) cold working the assembly in a plurality of cold working stages and intermediate annealing the cold worked assembly between cold working stages.
Claim 28
Independent Claim
73 words
A method of making an elongated composite product comprising: a) providing an elongated outer sheath formed of a Co--Ni--Cr alloy with an inner lumen extending therein; b) advancing an elongated core member formed of NiTi alloy into the inner lumen of the outer sheath to form an assembly therewith; and c) cold working the assembly in a plurality of cold working stages and intermediate annealing the cold worked assembly between cold working stages.
Claim 29
Dependent Claim
19 words
The method of claim 23 wherein the outer sheath is formed of an alloy containing up to 10% molybdenum.
Claim 30
Dependent Claim
26 words
The method of claim 23 wherein the assembly is cold worked by drawing with a reduction of at least about 20% in each cold working stage.
Claim 31
Dependent Claim
22 words
The method of claim 23 wherein the cold worked assembly is intermediate annealed at a temperature of about 600° and 900° C.
Claim 32
Dependent Claim
18 words
The method of claim 25 wherein the final cold working stage includes a reduction of at least 50%.
Claim 33
Dependent Claim
47 words
The method of claim 24 wherein the cold worked assembly is heat treated after the final cold working stage at a temperature between about 400° and about 700° C. to age harden the outer sheath formed of Co--Ni--Cr--Mo alloy and provide pseudoelastic characteristics to the inner member.
Claim 34
Dependent Claim
41 words
The method of claim 24 wherein the cold worked assembly is heat treated at a temperature between about 550° and about 675° C. to age harden the outer sheath formed of Co--Ni--Cr--Mo alloy and provide pseudoelastic characteristics to the inner member.