Abstract

Abstract There is disclosed a collagen preparation of improved adhesive properties and formed of microparticulate collagen of a particle size of from 0.5 to 2 μm, preferably 0.5 to 1.0 μm preferably submicrosized in a delivery system, such as an aerosol, and thus in sprayable form as a wound dressing alone, or with releasing drugs or other active agents. The microparticulate collagen is formed by ball milling collagen for a time sufficient to form the microparticulate collagen having a particle size of from 0.5 to 2 μm, preferably 0.5 to 1 μm.

Inventors

  • 👤 Vinay K. Sharma

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-23 11:09
CPC Classifications
A; A61; A61K; A61K47/00; A61K47/30; A61K47/42; A61K9/00; A61K9/70; A61K9/7015; A61L; A61L24/00; A61L24/04; A61L24/10; A61L24/102; A61L26/00; A61L26/0009; A61L26/0028; A61L26/0033; A61L26/0052; A61L26/0061; A61L26/0066; A61L26/0076; A61P; A61P17/00; A61P43/00; A61L2300/00; A61L2300/40; A61L2300/404; A61L2300/41; A61L2300/412; A61L2300/414; A61L2300/60; A61L2300/62; A61L2300/622

Claims Analysis

Total Claims: 8
Claim 1
Independent Claim 46 words
A process for particulating collagen, which comprises: a) introducing collagen with an inert media into a ball mixing zone; b) ball milling for a time sufficient to form microparticulate collagen having a particle size of from 0.1 to 5.0 μm; and c) recovering said microparticulate collagen.
Claim 2
Dependent Claim 46 words
A process for particulating collagen, which comprises: a) introducing collagen with an inert media into a ball mixing zone; b) ball milling for a time sufficient to form microparticulate collagen having a particle size of from 0.1 to 5.0 μm; and c) recovering said microparticulate collagen.
Claim 3
Dependent Claim 30 words
The process as defined in claim 1 wherein ball milling is effected for a time sufficient to produce submicroparticulate collagen of a particle size of from 0.5 to 2.0 μm.
Claim 4
Dependent Claim 17 words
The process as defined in claim 1 wherein said inert media is a low molecular weight alcohol.
Claim 5
Dependent Claim 21 words
The process as defined in claim 2 wherein collagen to inert liquid is in a ratio of from 1:5 to 1:50.
Claim 6
Dependent Claim 15 words
The process as defined in claim 3 wherein said ratio is preferably 1:10 to 1:15.
Claim 7
Dependent Claim 18 words
The process as defined in claim 1 wherein ball milling is effected for from 60 to 90 hours.
Claim 8
Dependent Claim 16 words
The process as defined in claim 6 wherein ball milling is effected for about 72 hours.

References Cited (Backward Citations)

US4741872A Cited
US5059425A Cited
US4950699A Cited
US5128136A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1997-10-17 1998-04-18 1998-10-18 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2001-10-17 2002-04-18 2002-10-18 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2005-10-17 2006-04-18 2006-10-18 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag