Abstract

Abstract Setting times of calcium phosphate cement compositions are enhanced by the addition of phosphate or carbonate lubricant compositions. Methods for preparing the cement compositions are provided.

Inventors

  • 👤 Brent R. Constanz
  • 👤 Mark T. Fulmer
  • 👤 Bryan M. Barr

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-23 09:07
CPC Classifications
A; A61; A61L; A61L24/00; A61L24/02; A61K; A61K6/00; A61K6/30; A61K6/50; A61K6/54; A61K6/70; A61K6/71; A61K6/74; A61K6/75; A61K6/80; A61K6/831; A61K6/838; A61K6/849; A61K6/864; A61K6/873; A61K6/876; A61L27/00; A61L27/02; A61L27/12; A61L27/40; A61L27/44; A61L27/46; A61L27/50; A61L27/58; C; C01; C01B; C01B25/00; C01B25/16; C01B25/26; C01B25/32; C01B25/322; C01B25/327; C01B25/455; A61F; A61F2/00; A61F2/02; A61F2/28; A61F2002/2817; A61F2/30; A61F2002/30001; A61F2002/30003; A61F2002/3006; A61F2002/30062; A61F2210/00; A61F2210/0004; A61F2310/00; A61F2310/00005; A61F2310/00179; A61F2310/00293; Y; Y10; Y10S; Y10S623/00; Y10S623/901

Claims Analysis

Total Claims: 16
Claim 1
Independent Claim 100 words
A method for preparing a rapid setting calcium phosphate composition capable of rapidly setting up in a viable mammalian host, said method comprising: combining with mixing dry precursors for producing a calcium phosphate mineral composition, said precursors comprising a calcium source and a phosphoric acid source free of uncombined water; combining said combined precursors with a lubricant at a pH in the range of 6-11, wherein said lubricant comprises a member selected from the group consisting of phosphate and carbonate and is from about 15 to 70 weight percent of the total composition; to form a rapidly setting flowable composition.
Claim 2
Independent Claim 100 words
A method for preparing a rapid setting calcium phosphate composition capable of rapidly setting up in a viable mammalian host, said method comprising: combining with mixing dry precursors for producing a calcium phosphate mineral composition, said precursors comprising a calcium source and a phosphoric acid source free of uncombined water; combining said combined precursors with a lubricant at a pH in the range of 6-11, wherein said lubricant comprises a member selected from the group consisting of phosphate and carbonate and is from about 15 to 70 weight percent of the total composition; to form a rapidly setting flowable composition.
Claim 3
Dependent Claim 46 words
A method according to claim 1, wherein said member selected from the group consisting of phosphate and carbonate is present in said lubricant in a concentration ranging from 0.05 to 0.5M and said pH of said lubricant is in the range of about 7 to 9.
Claim 4
Dependent Claim 13 words
A method according to claim 1, wherein said precursors are milled after combining.
Claim 5
Dependent Claim 28 words
A method according to claim 3, wherein said calcium source comprises at least one of a member selected from the group consisting of tetracalcium phosphate and calcium carbonate.
Claim 6
Dependent Claim 44 words
A method according to claim 1, wherein at least one of said combined precursors and lubricant comprise a protein in an amount equal to from about 0.1 to 5 parts per part by weight as compared with the total weight of calcium phosphate mineral.
Claim 7
Dependent Claim 25 words
A method according to claim 1, wherein said total composition further comprises from about 50 to 90 weight percent of physiologically acceptable particles or aggregate.
Claim 8
Dependent Claim 16 words
A bone tissue comprising ex vivo a composition prepared according to the method of claim 1.
Claim 9
Dependent Claim 26 words
A method for making bone repair, said method comprising: introducing at a bone site for repair, a composition prepared according to the method of claim 1.
Claim 10
Independent Claim 125 words
A method for preparing a rapid setting calcium phosphate composition capable of rapidly setting up in a viable mammalian host, said method comprising: combining with mixing dry precursors for producing a calcium phosphate mineral composition, said precursors comprising a calcium source comprising tetracalcium phosphate and calcium carbonate and a phosphate source comprising at least one of monocalcium phosphate and orthophosphoric acid free of uncombined water; combining said combined precursors with a lubricant comprising a member selected from the group consisting of sodium phosphate and carbonate in a concentration ranging from 0.05 to 0.5M, said lubricant at a pH in the range of 6-11, wherein said lubricant is from about 15 to 70 weight percent of the total composition; a form a rapidly setting flowable composition.
Claim 11
Independent Claim 125 words
A method for preparing a rapid setting calcium phosphate composition capable of rapidly setting up in a viable mammalian host, said method comprising: combining with mixing dry precursors for producing a calcium phosphate mineral composition, said precursors comprising a calcium source comprising tetracalcium phosphate and calcium carbonate and a phosphate source comprising at least one of monocalcium phosphate and orthophosphoric acid free of uncombined water; combining said combined precursors with a lubricant comprising a member selected from the group consisting of sodium phosphate and carbonate in a concentration ranging from 0.05 to 0.5M, said lubricant at a pH in the range of 6-11, wherein said lubricant is from about 15 to 70 weight percent of the total composition; a form a rapidly setting flowable composition.
Claim 12
Dependent Claim 23 words
A method according to claim 9, wherein said lubricant comprises sodium phosphate at a pH in the range of about 7 to 9.
Claim 13
Dependent Claim 13 words
A method according to claim 9, wherein said precursors are milled after combining.
Claim 14
Dependent Claim 16 words
A method according to claim 11, wherein said calcium source comprises tetracalcium phosphate and calcium carbonate.
Claim 15
Dependent Claim 44 words
A method according to claim 9, wherein at least one of said combined precursors and lubricant comprise a protein in an amount equal to from about 0.1 to 5 parts per part by weight as compared with the total weight of calcium phosphate mineral.
Claim 16
Dependent Claim 25 words
A method according to claim 9, wherein said total composition further comprises from about 50 to 90 weight percent of physiologically acceptable particles or aggregate.

References Cited (Backward Citations)

US4497075A Cited
USRE33161E Cited
US4959104A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1997-08-08 1998-02-07 1998-08-09 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2001-08-08 2002-02-07 2002-08-09 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2005-08-08 2006-02-07 2006-08-09 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag