US5295288A Expired / Lapsed US ⏱️ 0.0 years remaining

Method of making coating surrounding a piezoelectric solid state motor stack

Assignee: Caterpillar Inc
•
Filing: 1992-12-14
•
Granted: 1994-03-22
•
Expires: 2012-12-14
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A solid state motor includes a plurality of piezoelectric elements assembled in a stack. Each element has two opposing planar surfaces. A plurality of electrodes each has a planar section contacting the planar surfaces of two adjacent elements in the stack. A silicone adhesive is adapted to adhere to the piezoelectric elements. A plurality of alumina particles are disposed in the silicone adhesive. A protective housing cylindrically encases the combination of the stack, electrodes, and silicone adhesive.

Inventors

  • 👤 Chuong Q. Dam
  • 👤 Kurtis C. Kelley

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-23 10:06
CPC Classifications
H; H10; H10N; H10N30/00; H10N30/80; H10N30/88; H10N30/883; H10N30/50; H10N30/503; H10N30/01; H10N30/02; H10N30/05; H10N30/057; H10N30/87; H10N30/875; Y; Y10; Y10T; Y10T29/00; Y10T29/42

Claims Analysis

Total Claims: 8
Claim 1
Independent Claim 123 words
A method for encapsulating a piezoelectric solid state motor having a plurality of elements assembled in a stack interleaved with electrodes, comprising the steps of: adding a plurality of ceramic particles to a low viscosity silicone adhesive having high thermal conductivity characteristics, wherein the grain size of said ceramic particles is substantially equal to the grain size of the piezoelectric material of said piezoelectric elements; encapsulating said stack with said low viscosity silicone adhesive; curing the silicone adhesive at a first temperature for a first predetermined amount of time for setting said silicone adhesive; and thereafter curing the silicone adhesive at a second temperature for a second predetermined amount of time for further establishing adhesion between said piezoelectric elements and said silicone adhesive.
Claim 2
Independent Claim 123 words
A method for encapsulating a piezoelectric solid state motor having a plurality of elements assembled in a stack interleaved with electrodes, comprising the steps of: adding a plurality of ceramic particles to a low viscosity silicone adhesive having high thermal conductivity characteristics, wherein the grain size of said ceramic particles is substantially equal to the grain size of the piezoelectric material of said piezoelectric elements; encapsulating said stack with said low viscosity silicone adhesive; curing the silicone adhesive at a first temperature for a first predetermined amount of time for setting said silicone adhesive; and thereafter curing the silicone adhesive at a second temperature for a second predetermined amount of time for further establishing adhesion between said piezoelectric elements and said silicone adhesive.
Claim 3
Dependent Claim 43 words
A method, as set forth in claim 8, wherein the step of encapsulating further includes the steps of: grit blasting the stack to remove debris; cleaning the stack to remove unwanted contaminants; and applying the silicone adhesive to said stack under a vacuum.
Claim 4
Dependent Claim 28 words
A method, as set forth in claim 2, wherein the steps of encapsulating and curing are performed while the stack is loaded at a predetermined amount of force.
Claim 5
Dependent Claim 19 words
A method, as set forth in claim 3, including the step of aligning said stack within a protective housing.
Claim 6
Dependent Claim 25 words
A method, as set forth in claim 4, wherein said step of encapsulating fills an area between said stack and said housing with silicone adhesive.
Claim 7
Dependent Claim 30 words
A method, as set forth in claim 1, wherein the silicon adhesive is cured at the first temperature of 1180° C. for the first predetermined time period of 2 hours.
Claim 8
Dependent Claim 31 words
A method, as set forth in claim 6, wherein the silicon adhesive is cured at the second temperature of about 145°-150° C. for the second predetermined time period of 4 hours.

References Cited (Backward Citations)

US4011474A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1997-03-21 1997-09-20 1998-03-22 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2001-03-21 2001-09-20 2002-03-22 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2005-03-21 2005-09-20 2006-03-22 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag