Claims Analysis
Total Claims: 21
Claim 1
Independent Claim
106 words
A method for the application of gelatin-resorcinol aldehyde glue to a biological tissue surface, comprising: (i) applying a solution of gelatin-resorcinol to the surface to obtain a gelatin-resorcinol coated surface using a kit including a first container of a solution of gelatin-resorcinol and a second container of a solution of an aldehyde, the second container including means for aerosolizing the solution of aldehyde; (ii) aerosolizing a solution of an aldehyde onto the gelatin-resorcinol coated surfaced wherein the aldehyde is an aqueous solution of approximately 25% glutaraldehyde and (iii) allowing the mixture of gelatin resorcinol and the aldehyde on the surface, obtained in step (ii), to polymerize.
Claim 2
Independent Claim
106 words
A method for the application of gelatin-resorcinol aldehyde glue to a biological tissue surface, comprising: (i) applying a solution of gelatin-resorcinol to the surface to obtain a gelatin-resorcinol coated surface using a kit including a first container of a solution of gelatin-resorcinol and a second container of a solution of an aldehyde, the second container including means for aerosolizing the solution of aldehyde; (ii) aerosolizing a solution of an aldehyde onto the gelatin-resorcinol coated surfaced wherein the aldehyde is an aqueous solution of approximately 25% glutaraldehyde and (iii) allowing the mixture of gelatin resorcinol and the aldehyde on the surface, obtained in step (ii), to polymerize.
Claim 3
Dependent Claim
44 words
A method according to claim 1, wherein step (iii) includes the steps of (a) allowing the mixture to polymerize for not more than approximately 30 seconds; and (b) rinsing the surface, immediately after step (a), with an aqueous solution to remove the excess aldehyde.
Claim 4
Independent Claim
73 words
A method for the application of gelatin-resorcinol aldehyde glue to a graft, comprising: (i) obtaining a graft; (ii) applying a solution of gelatin-resorcinol to the graft, obtained in step (i), to obtain a gelatin-resorcinol coated graft; (iii) aerosolizing a solution of an aldehyde onto the coated graft, obtained in step (ii), to obtain a gelatin-resorcinol aldehyde mixture on the graft; (iv) allowing the mixture on the graft, obtained in step (iii), to polymerize.
Claim 5
Independent Claim
73 words
A method for the application of gelatin-resorcinol aldehyde glue to a graft, comprising: (i) obtaining a graft; (ii) applying a solution of gelatin-resorcinol to the graft, obtained in step (i), to obtain a gelatin-resorcinol coated graft; (iii) aerosolizing a solution of an aldehyde onto the coated graft, obtained in step (ii), to obtain a gelatin-resorcinol aldehyde mixture on the graft; (iv) allowing the mixture on the graft, obtained in step (iii), to polymerize.
Claim 6
Dependent Claim
62 words
A method according to claim 3, further comprising, before step (ii), the step of obtaining a kit including a first container of a solution of gelatin-resorcinol and a second container of a solution of an aldehyde, the second container including means for aerosolizing the solution of aldehyde, and wherein steps (ii) and (iii) are conducted using the first and second containers respectively.
Claim 7
Dependent Claim
53 words
A method according to claim 3, wherein the graft, obtained in step (i), is a high porosity vascular prosthesis; and wherein the method further comprises, after step (iv), the step of: (v) implanting the prosthesis in a vascular tissue; and wherein, in step (v), a prosthesis with improved hemostasis after implantation is obtained.
Claim 8
Dependent Claim
62 words
A method according to claim 5, further comprising, before step (ii), the step of obtaining a kit including a first container of a solution of gelatin-resorcinol and a second container of a solution of an aldehyde, the second container including means for aerosolizing the solution of aldehyde, and wherein steps (ii) and (iii) are conducted using the first and second containers respectively.
Claim 9
Dependent Claim
24 words
A method according to claim 5, wherein the aldehyde solution includes one or more aldehydes selected from the group consisting of glutaraldehyde and formaldehyde.
Claim 10
Dependent Claim
18 words
A method according to claim 7, wherein the aldehyde solution is an aqueous solution of approximately 25% glutaraldehyde.
Claim 11
Dependent Claim
44 words
A method according to claim 8, wherein step (iv) includes the steps of: (a) allowing the mixture to polymerize for not more than approximately 30 seconds; and (b) rinsing the graft, immediately after step (a), with an aqueous solution to remove the excess aldehyde.
Claim 12
Dependent Claim
55 words
A method according to claim 7, wherein step (i) further comprises the steps of: (a) obtaining a high porosity vascular prosthesis; and (b) implanting the prosthesis, obtained in step (a), in a vascular tissue, to obtain a graft that includes an anastomosis; and wherein, in step (iv), an implanted prosthesis with improved hemostasis is obtained.
Claim 13
Dependent Claim
62 words
A method according to claim 10, further comprising, before step (ii), the step of obtaining a kit including a first container of a solution of gelatin-resorcinol and a second container of a solution of an aldehyde, the second container including means for aerosolizing the solution of aldehyde, and wherein steps (ii) and (iii) are conducted using the first and second containers respectively.
Claim 14
Dependent Claim
24 words
A method according to claim 10, wherein the aldehyde solution includes one or more aldehydes selected from the group consisting of glutaraldehyde and formaldehyde.
Claim 15
Dependent Claim
18 words
A method according to claim 12, wherein the aldehyde solution is an aqueous solution of approximately 25% glutaraldehyde.
Claim 16
Dependent Claim
44 words
A method according to claim 13, wherein step (iv) includes the steps of: (a) allowing the mixture to polymerize for not more than approximately 30 seconds; and (b) rinsing the graft, immediately after step (a), with an aqueous solution to remove the excess aldehyde.
Claim 17
Dependent Claim
24 words
A method according to claim 3, wherein the aldehyde solution includes one or more aldehydes selected from the group consisting of glutaraldehyde and formaldehyde.
Claim 18
Dependent Claim
18 words
A method according to claim 15, wherein the aldehyde solution is an aqueous solution of approximately 25% glutaraldehyde.
Claim 19
Dependent Claim
44 words
A method according to claim 16, wherein step (iv) includes the steps of: (a) allowing the mixture to polymerize for not more than approximately 30 seconds; and (b) rinsing the graft, immediately after step (a), with an aqueous solution to remove the excess aldehyde.
Claim 20
Dependent Claim
66 words
A kit, for the application of gelatin-resorcinol aldehyde glue to a surface, comprising: (i) a first container including a solution of gelatin resorcinol; and (ii) a second container including a solution of an aldehyde and means for aerosolizing the solution of aldehyde wherein the aldehyde solution includes at least one aldehydes selected from the group consisting of formaldehyde and approximately 25% glutaraldehyde in an aqueous solution.
Claim 21
Dependent Claim
66 words
A kit, for the application of gelatin-resorcinol aldehyde glue to a surface, comprising: (i) a first container including a solution of gelatin resorcinol; and (ii) a second container including a solution of an aldehyde and means for aerosolizing the solution of aldehyde wherein the aldehyde solution includes at least one aldehydes selected from the group consisting of formaldehyde and approximately 25% glutaraldehyde in an aqueous solution.