US4914068A
Expired / Lapsed
US
⏱️ 0.0 years remaining
Process for the dispersion of Group VIII metals in large pore zeolite catalysts
Assignee: ExxonMobil Chemical Patents Inc
•
Filing: 1988-03-21
•
Granted: 1990-04-03
•
Expires: 2008-03-21
Abstract
Abstract This invention relates to methods for dispersing Group-VIII and other metals containing zeolites, particularly large pore zeolites.
Inventors
- 👤 Virginia R. Cross
- 👤 Jar L. Kao
- 👤 Thomas H. Vanderspurt
- 👤 Murray Nadler
- 👤 Theodorus M. Wortel
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-23 20:01
CPC Classifications
B; B01; B01J; B01J29/00; B01J29/04; B01J29/06; B01J29/08; B01J29/10; B01J29/064; B01J29/072; B01J29/16; B01J29/60; B01J29/61; B01J29/62; B01J29/90; B01J38/00; B01J38/04; B01J38/42; B01J38/44
Claims Analysis
Total Claims: 39
Claim 1
Independent Claim
128 words
A method for dispersing at least one Group-VIII metal in a catalyst containing a large pore zeolite and at least one Group-VIII metal comprising the steps of: (a) dispersing the at least one Group-VIII metal on the zeolite by exposing the catalyst to a gaseous stream containing at least one halogen source elected from a halogen, a halogen and oxygen, a hydrogen halide and oxygen, oxygen and an organic compound containing halogen, and mixture of these at a temperature sufficient to form oxyhalides or halides of said metal; (b) cooling the catalyst to a temperature less than the dispersing temperature of step (a) and then (c) reducing said Group-VIII metal by contacting the catalyst with a reducing as at least initially within the temperature range of step (b).
Claim 2
Independent Claim
128 words
A method for dispersing at least one Group-VIII metal in a catalyst containing a large pore zeolite and at least one Group-VIII metal comprising the steps of: (a) dispersing the at least one Group-VIII metal on the zeolite by exposing the catalyst to a gaseous stream containing at least one halogen source elected from a halogen, a halogen and oxygen, a hydrogen halide and oxygen, oxygen and an organic compound containing halogen, and mixture of these at a temperature sufficient to form oxyhalides or halides of said metal; (b) cooling the catalyst to a temperature less than the dispersing temperature of step (a) and then (c) reducing said Group-VIII metal by contacting the catalyst with a reducing as at least initially within the temperature range of step (b).
Claim 3
Dependent Claim
21 words
The method of claim 1 wherein water vapor is present in at least one of the dispersing, cooling and reducing steps.
Claim 4
Dependent Claim
14 words
The method of claim 2 wherein water vapor is present during the cooling step.
Claim 5
Dependent Claim
13 words
The method of claim 2 wherein oxygen is present in the cooling step.
Claim 6
Dependent Claim
25 words
The method of claim 1 wherein the gaseous stream present during the cooling step contains the same components as that present in the dispersing step.
Claim 7
Dependent Claim
43 words
The method of claim 1 wherein the dispersing step is at a temperature above about 475° C., the cooling step terminates at a temperature less than about 430° C., and the reducing step is conducted at a temperature less than about 430° C.
Claim 8
Dependent Claim
33 words
The method of claim 1 wherein the dispersing step is terminated between one and ten hours after a halide or hydrogen halide is detected at the outlet of a bed containing said catalyst.
Claim 9
Dependent Claim
39 words
The method of claim 1 wherein the cooling step is conducted in the presence of a gas stream also comprising at least one halogen source selected from a halogen, a hydrogen halide, and an organic compound containing a halogen.
Claim 10
Dependent Claim
13 words
The method of claim 8 wherein oxygen is present in the cooling step.
Claim 11
Dependent Claim
30 words
The method of claim 6 wherein said gas in the dispersing step includes water vapor and gas present in the cooling step comprises oxygen, water vapor and a halogen source.
Claim 12
Dependent Claim
11 words
The method of claim 10 wherein the halogen sources comprise chlorine.
Claim 13
Dependent Claim
14 words
The method of claim 1 wherein the large pore zeolite is a zeolite L.
Claim 14
Dependent Claim
16 words
The method of claim 12 wherein the zeolite L is of a generally cylindrical crystal shape.
Claim 15
Dependent Claim
21 words
The method of claim 11 wherein the zeolite L contains cation from potassium, barium, cesium, rubidium, calcium, magnesium and mixtures thereof.
Claim 16
Dependent Claim
10 words
The method of claim 14 wherein the catalyst is formed.
Claim 17
Dependent Claim
10 words
The method of claim 12 wherein the cation is potassium.
Claim 18
Dependent Claim
18 words
The method of claim 6 wherein the reduction step terminates at a temperature less than about 350° C.
Claim 19
Dependent Claim
18 words
The method of claim 6 wherein the cooling step terminates at a temperature less than about 350° C.
Claim 20
Dependent Claim
42 words
The method of claim 1 wherein the catalyst contains coke, further comprising the step of burning said coke by exposing the catalyst in said bed to an oxygen-containing gas at a temperature and oxygen concentration sufficient to cause combustion of the coke.
Claim 21
Dependent Claim
28 words
The method of claim 19 wherein the oxygen containing gas in said burning step contains water vapor sufficient to provide a concentration of at least about 3000 vppm.
Claim 22
Dependent Claim
32 words
The method of claim 1 wherein the concentration of hydrogen in said reducing gas is controlled to limit the concentration of hydrogen halides leaving the catalyst in less than about 1200 ppmv.
Claim 23
Dependent Claim
31 words
The method of claim 1 additionally comprising the step of contacting the catalyst with a soaking gas containing oxygen and water after the cooling step and prior to the reducing step.
Claim 24
Dependent Claim
24 words
The method of claim 1 wherein said catalyst is cooled, in said cooling step, at an average rate of at least about 27° C./hr.
Claim 25
Dependent Claim
34 words
The method of claim 6 also comprising the additional reducing step of contacting the catalyst with gas containing hydrogen and water vapor at a temperature in the range of 475° C. and 545° C.
Claim 26
Dependent Claim
19 words
The method of claim 24 wherein the additional reducing step is carried out between 475° C. and 520° C.
Claim 27
Dependent Claim
19 words
The method of claim 25 wherein the additional reducing step is carried out between 475° C. and 500° C.
Claim 28
Dependent Claim
25 words
The method of claim 1 wherein said Group-VIII metal is selected from the group, consisting of nickel, ruthenium, rhodium, iridium, palladium, platinum and combinations thereof.
Claim 29
Dependent Claim
27 words
The method of claim 27 wherein the catalyst also contains a metal selected from copper, silver, gold, molybdenum, tungsten, rhenium, tin, nickel, ruthenium, palladium, or mixtures thereof.
Claim 30
Dependent Claim
66 words
The method of claim 2 wherein said zeolite L is a zeolite having an x-ray deflection pattern obtained from CuKαradiation with significant d values set out in Table A and comprising highly crystalline crystallites having at least 50% of its crystallites in the form of distinct circular cylinders with an aspect ratio of at least 0.5 and with a mean diameter of at least 0.5 micron.
Claim 31
Independent Claim
96 words
The method of reducing a catalyst comprising a large-pore zeolite and at least one Group-VIII metal, the catalyst initially containing one or more halogens, the method comprising the steps of reducing the catalyst by contacting it with a hydrogen-containing reducing gas at a reducing temperature sufficient to cause reduction of said metal by the hydrogen in said gas, whereby hydrogen halides are formed in said reducing gas, and limiting the concentration of hydrogen in said reducing gas so as to limit the concentration of hydrogen halides in said reducing gas to less than about 1200 vppm.
Claim 32
Independent Claim
96 words
The method of reducing a catalyst comprising a large-pore zeolite and at least one Group-VIII metal, the catalyst initially containing one or more halogens, the method comprising the steps of reducing the catalyst by contacting it with a hydrogen-containing reducing gas at a reducing temperature sufficient to cause reduction of said metal by the hydrogen in said gas, whereby hydrogen halides are formed in said reducing gas, and limiting the concentration of hydrogen in said reducing gas so as to limit the concentration of hydrogen halides in said reducing gas to less than about 1200 vppm.
Claim 33
Dependent Claim
36 words
The method of claim 30 wherein said Group-VIII metal is initially present on said catalyst at least in part in the form of halides or oxyhalides of said metal dispersed in the pores of said zeolite.
Claim 34
Dependent Claim
36 words
The method of claim 30 wherein said limiting step includes the step of monitoring the concentration of hydrogen halides in said reducing gas and controlling the concentration of hydrogen in said reducing gas in response thereto.
Claim 35
Dependent Claim
53 words
The method of claim 32 wherein said monitoring step includes the step of detecting a first momentary increase in the exhaust gas hydrogen halide concentration and said controlling step includes the step of initially increasing the hydrogen concentration in the inlet gas after termination of said first momentary increase in hydrogen halide concentration.
Claim 36
Dependent Claim
34 words
The method of claim 33 wherein said catalyst is maintained at less than about 430° C. during said reducing step until at least after termination of said first momentary increase in hydrogen halide concentration.
Claim 37
Dependent Claim
49 words
The method of claim 34 wherein the hydrogen concentration in the reducing gas supplied to said bed is controlled so as to limit the hydrogen halide concentration in the reducing gas discharged from the bed to less than about 1,200 ppmv at least until termination of said momentary increase.
Claim 38
Dependent Claim
34 words
The method of claim 35 wherein said catalyst is maintained at less than about 430° C. during said reducing step at least until after termination of said first momentary increase in hydrogen halide concentration.
Claim 39
Dependent Claim
55 words
The method of claim 30 wherein said zeolite is a zeolite L and said Group-VIII metal is selected from the group consisting of nickel, ruthenium, rhodium, iridium, palladium, platinum and combinations thereof, and at least part of said metal is present on said zeolite as oxychlorides and chlorides dispersed in the pores of said zeolite.
References Cited (Backward Citations)
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1993-04-02 | 1993-10-02 | 1994-04-03 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1997-04-02 | 1997-10-02 | 1998-04-03 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 2001-04-02 | 2001-10-02 | 2002-04-03 | $7700.00 | Window Closed / Lapsed |