Process for hydrogenating olefins in the presence of ethers
Assignee: IFP Energies nouvelles
•
Filing: 1986-07-15
•
Granted: 1988-04-26
•
Expires: 2006-07-15
Abstract
Abstract This process for hydrogenating an olefin contained in a mixture of said olefin with an ether and optionally with sulfur, comprises reacting hydrogen with said mixture in the presence of a noble metal-containing catalyst, said catalyst containing at least one first noble metal from the palladium, rhodium, iridium and platinum group and at least one second other metal from the gold and platinum group.
Inventors
- 👤 Jean-Paul Boitiaux
- 👤 Jean Cosyns
- 👤 Michel Derrien
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-23 11:20
CPC Classifications
B; B01; B01J; B01J23/00; B01J23/38; B01J23/40; B01J23/48; B01J23/52; C; C07; C07C; C07C5/00; C07C5/02; C07C5/03; C10; C10G; C10G45/00; C07C2521/00; C07C2521/02; C07C2521/04; C07C2523/00; C07C2523/38; C07C2523/40; C07C2523/42; C07C2523/44; C07C2523/46; C07C2523/48; C07C2523/52; Y; Y02; Y02P; Y02P20/00; Y02P20/50; Y02P20/582
Claims Analysis
Total Claims: 10
Claim 1
Independent Claim
113 words
In a process for purifying an olefin-containing ether mixture, said process comprising reacting said mixture with hydrogen in the presence of catalyst containing a noble metal, the improvement wherein the catalyst contains: (a) at least one noble metal selected from the group consisting of palladium, rhodium, iridium and platinum; (b) at least one metal different from (a), selected from the group consisting of gold and platinum; and wherein the reaction is conducted at a temperature of 20°-300° C., a pressure of 1-100 bar and with a space velocity of the mixture of 0.5-10 so as to increase the extent of hydrogenation of the olefin as compared to said process employing component (a) alone.
Claim 2
Dependent Claim
113 words
In a process for purifying an olefin-containing ether mixture, said process comprising reacting said mixture with hydrogen in the presence of catalyst containing a noble metal, the improvement wherein the catalyst contains: (a) at least one noble metal selected from the group consisting of palladium, rhodium, iridium and platinum; (b) at least one metal different from (a), selected from the group consisting of gold and platinum; and wherein the reaction is conducted at a temperature of 20°-300° C., a pressure of 1-100 bar and with a space velocity of the mixture of 0.5-10 so as to increase the extent of hydrogenation of the olefin as compared to said process employing component (a) alone.
Claim 3
Dependent Claim
107 words
In a process for purifying an olefin-containing ether mixture, said process comprising reacting said mixture with hydrogen in the presence of catalyst containing a noble metal, the improvement wherein the catalyst contains: (a) at least one noble metal selected from the group consisting of palladium, rhodium, iridium and platinum, and (b) at least one metal different from (a), selected from the group consisting of gold and platinum; and wherein the reaction is conducted at a temperature of 20°-300° C., a pressure of 1-100 bar and at an hourly space velocity of the mixture of 0.5-10 wherein, in the catalyst, (a) is not palladium when (b) is gold.
Claim 4
Dependent Claim
107 words
In a process for purifying an olefin-containing ether mixture, said process comprising reacting said mixture with hydrogen in the presence of catalyst containing a noble metal, the improvement wherein the catalyst contains: (a) at least one noble metal selected from the group consisting of palladium, rhodium, iridium and platinum, and (b) at least one metal different from (a), selected from the group consisting of gold and platinum; and wherein the reaction is conducted at a temperature of 20°-300° C., a pressure of 1-100 bar and at an hourly space velocity of the mixture of 0.5-10 wherein, in the catalyst, (a) is not palladium when (b) is gold.
Claim 5
Dependent Claim
87 words
In a process for purifying an olefin-containing ether mixture, said process comprising reacting said mixture with hydrogen in the presence of a catalyst containing a noble metal, the improvement wherein the catalyst contains: (a) at least one noble metal selected from the group consisting of palladium, rhodium, iridium and platinum; (b) at least one metal different from (a), selected from the group consisting of gold and platinum so as to increase the extent of hydrogenation of the olefin as compared to said process employing component (a) alone.
Claim 6
Dependent Claim
87 words
In a process for purifying an olefin-containing ether mixture, said process comprising reacting said mixture with hydrogen in the presence of a catalyst containing a noble metal, the improvement wherein the catalyst contains: (a) at least one noble metal selected from the group consisting of palladium, rhodium, iridium and platinum; (b) at least one metal different from (a), selected from the group consisting of gold and platinum so as to increase the extent of hydrogenation of the olefin as compared to said process employing component (a) alone.
Claim 7
Dependent Claim
39 words
A process according to claim 3, wherein the catalyst comprises a carrier, a first metal (a) in a proportion by weight of 0.05 to 2% and a second metal (b) in a proportion by weight from 0.05 to 2%.
Claim 8
Dependent Claim
13 words
A process according to claim 4, wherein the carrier is alumina or silica.
Claim 9
Dependent Claim
80 words
In a process for purifying an olefin-containing ether mixture, said process comprising reacting said mixture with hydrogen in the presence of a catalyst containing a noble metal, the improvement wherein the catalyst contains: (a) at least one noble metal selected from the group consisting of palladium, rhodium, iridium and platinum, and (b) at least one metal different from (a), selected from the group consisting of gold and platinum wherein, in the catalyst, (a) is not palladium when (b) is gold.
Claim 10
Dependent Claim
80 words
In a process for purifying an olefin-containing ether mixture, said process comprising reacting said mixture with hydrogen in the presence of a catalyst containing a noble metal, the improvement wherein the catalyst contains: (a) at least one noble metal selected from the group consisting of palladium, rhodium, iridium and platinum, and (b) at least one metal different from (a), selected from the group consisting of gold and platinum wherein, in the catalyst, (a) is not palladium when (b) is gold.
References Cited (Backward Citations)
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1991-04-26 | 1991-10-26 | 1992-04-26 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1995-04-26 | 1995-10-26 | 1996-04-26 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1999-04-26 | 1999-10-26 | 2000-04-26 | $7700.00 | Window Closed / Lapsed |