Abstract

Abstract A split recoating mold for use in recoating optical waveguide fibers with a UV-curable resin is provided wherein: (1) the mold, when closed, forms a cavity for receiving the portion of the fiber which is to be recoated, the cross-sectional size and shape of the cavity being essentially equal to the cross-sectional size and shape of the original fiber; (2) the mold includes an injection port for introducing a UV-curable resin into the cavity; and (3) the mold includes means for introducing ultraviolet light into the cavity so that resin located in regions of the cavity remote from the injection port will cure prior to resin located in regions of the cavity near the injection port.

Inventors

  • 👤 Lynn G. Amos
  • 👤 Stuart L. Saikkonen
  • 👤 Donald R. Young

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-23 04:51
CPC Classifications
G; G02; G02B; G02B6/00; G02B6/24; G02B6/255; G02B6/2558; B; B29; B29C; B29C35/00; B29C35/02; B29C35/08; B29C35/0888; B29C45/00; B29C45/0053; B29C45/14; B29C45/14549; B29C45/17; B29C45/26; B29C45/27; B29C45/2701; B29C45/2708; B29C70/00; B29C70/68; B29C70/74; C; C03; C03C; C03C25/00; C03C25/10; C03C25/104; C03C25/106; C03C25/12; C03C25/18; G02B6/2553; B29C35/0805; B29C2035/0827; B29C2045/0075; B29C2045/14557; B29C45/2669; B29C2045/2671; B29L; B29L2011/00; B29L2011/0075

Claims Analysis

Total Claims: 20
Claim 1
Independent Claim 148 words
Apparatus for recoating an uncoated section of a coated optical waveguide fiber with a UV-curable resin comprising a split mold which forms, when closed, a cavity for receiving the uncoated section of the fiber, the cross-sectional size and shape of the cavity being essentially equal to the cross-sectional size and shape of the coated fiber so as to prevent resin from flowing onto the coated portions of the fiber adjacent to the section of the fiber to be recoated during the recoating process, said mold including an injection port for introducing UV-curable resin into the cavity under pressure before curing and during the curing process to compensate for resin shrinkage and means for introducing ultraviolet light into the cavity so that resin located in regions of the cavity remote from the injection port will cure prior to resin located in regions of the cavity near the injection port.
Claim 2
Dependent Claim 148 words
Apparatus for recoating an uncoated section of a coated optical waveguide fiber with a UV-curable resin comprising a split mold which forms, when closed, a cavity for receiving the uncoated section of the fiber, the cross-sectional size and shape of the cavity being essentially equal to the cross-sectional size and shape of the coated fiber so as to prevent resin from flowing onto the coated portions of the fiber adjacent to the section of the fiber to be recoated during the recoating process, said mold including an injection port for introducing UV-curable resin into the cavity under pressure before curing and during the curing process to compensate for resin shrinkage and means for introducing ultraviolet light into the cavity so that resin located in regions of the cavity remote from the injection port will cure prior to resin located in regions of the cavity near the injection port.
Claim 3
Dependent Claim 39 words
The apparatus of claim 1 wherein the mold is made of a material which is opaque to ultraviolet light and the introducing means comprises a curing port leading to a region of the cavity remote from the injection port.
Claim 4
Dependent Claim 12 words
The apparatus of claim 2 wherein the mold is made of metal.
Claim 5
Dependent Claim 40 words
The apparatus of claim 2 further including means for passing ultraviolet light through the curing port to selectively illuminate and thus cure either the resin in the region of that port or the resin in the rest of the cavity.
Claim 6
Dependent Claim 58 words
The apparatus of claim 1 wherein the portion of the mold which includes the injection port is made of a material which is opaque to ultraviolet light and wherein the introducing means comprises a portion of the mold which is remote from the injection port and which is made of a material which is transparent to ultraviolet light.
Claim 7
Dependent Claim 27 words
The apparatus of claim 5 wherein the material which is opaque to ultraviolet light is metal and the material which is transparent to ultraviolet light is glass.
Claim 8
Dependent Claim 45 words
The apparatus of claim 1 wherein the injection port includes a primary channel and a plurality of secondary channels which connect the primary channel to the cavity, each of said secondary channels having a cross-sectional area smaller than the cross-sectional area of the primary channel.
Claim 9
Dependent Claim 45 words
The apparatus of claim 7 wherein a portion of the internal surface of the injection port at the junction of that port with the cavity has a unidirectional machine finish and said finish forms the secondary channels which connect the primary channel to the cavity.
Claim 10
Dependent Claim 26 words
The apparatus of claim 8 wherein each of the secondary channels has a cross sectional area of between about 15μ 2 and about 35μ 2 .
Claim 11
Dependent Claim 66 words
Apparatus for coating an optical waveguide fiber with a resin comprising a mold having a cavity and having an injection port for introducing the resin into the cavity, said port including a primary channel and a plurality of secondary channels which connect the primary channel to the cavity, each of said secondary channels having a cross-sectional area smaller than the cross-sectional area of the primary channel.
Claim 12
Dependent Claim 66 words
Apparatus for coating an optical waveguide fiber with a resin comprising a mold having a cavity and having an injection port for introducing the resin into the cavity, said port including a primary channel and a plurality of secondary channels which connect the primary channel to the cavity, each of said secondary channels having a cross-sectional area smaller than the cross-sectional area of the primary channel.
Claim 13
Dependent Claim 44 words
The apparatus of claim 10 wherein a portion of the internal surface of the port at the junction of the port with the cavity has a unidirectional machine finish and said finish forms the secondary channels which connect the primary channel to the cavity.
Claim 14
Dependent Claim 26 words
The apparatus of claim 11 wherein each of the secondary channels has a cross sectional area of between about 15μ 2 and about 35μ 2 .
Claim 15
Independent Claim 111 words
A method for coating a section of an optical waveguide fiber with a resin which shrinks upon curing comprising the steps of: (a) placing the section to be coated into a cavity which is connected to an injection port through which the resin can be introduced into the cavity under pressure; (b) introducing the resin into the cavity through the injection port; and (c) progressively curing the resin in the cavity beginning with the resin in a region remote from the injection port and progressing towards the injection port while introducing additional resin into the cavity under pressure through the injection port to compensate for shrinkage of the resin during curing.
Claim 16
Independent Claim 111 words
A method for coating a section of an optical waveguide fiber with a resin which shrinks upon curing comprising the steps of: (a) placing the section to be coated into a cavity which is connected to an injection port through which the resin can be introduced into the cavity under pressure; (b) introducing the resin into the cavity through the injection port; and (c) progressively curing the resin in the cavity beginning with the resin in a region remote from the injection port and progressing towards the injection port while introducing additional resin into the cavity under pressure through the injection port to compensate for shrinkage of the resin during curing.
Claim 17
Independent Claim 235 words
A method for recoating an uncoated section of a coated optical waveguide fiber with a UV-curable resin which shrinks upon curing comprising the steps of: (a) providing a split mold made of a material which does not transmit ultraviolet light and which forms, when closed, a cavity for receiving the uncoated section of the fiber, the cross-sectional size and shape of the cavity being essentially equal to the cross-sectional size and shape of the coated fiber, said mold including an injection port for introducing the UV-curable resin into the cavity and a curing port for illuminating the cavity with ultraviolet light in order to cure the resin; (b) placing the uncoated section of the fiber into the cavity; (c) introducing UV-curable resin into the cavity under pressure through the injection port until resin flows out of the curing port; (d) sealing off the curing port by passing ultraviolet light through that port to illuminate and thus cure the resin in the region of that port; (e) introducing additional UV-curable resin into the cavity under pressure through the injection port to compensate for the shrinkage of the resin cured in step (d); and (f) passing ultraviolet light through the curing port to illuminate and thus cure the rest of the resin in the cavity while introducing UV-curable resin into the cavity under pressure through the injection port to compensate for shrinkage of the resin during curing.
Claim 18
Independent Claim 235 words
A method for recoating an uncoated section of a coated optical waveguide fiber with a UV-curable resin which shrinks upon curing comprising the steps of: (a) providing a split mold made of a material which does not transmit ultraviolet light and which forms, when closed, a cavity for receiving the uncoated section of the fiber, the cross-sectional size and shape of the cavity being essentially equal to the cross-sectional size and shape of the coated fiber, said mold including an injection port for introducing the UV-curable resin into the cavity and a curing port for illuminating the cavity with ultraviolet light in order to cure the resin; (b) placing the uncoated section of the fiber into the cavity; (c) introducing UV-curable resin into the cavity under pressure through the injection port until resin flows out of the curing port; (d) sealing off the curing port by passing ultraviolet light through that port to illuminate and thus cure the resin in the region of that port; (e) introducing additional UV-curable resin into the cavity under pressure through the injection port to compensate for the shrinkage of the resin cured in step (d); and (f) passing ultraviolet light through the curing port to illuminate and thus cure the rest of the resin in the cavity while introducing UV-curable resin into the cavity under pressure through the injection port to compensate for shrinkage of the resin during curing.
Claim 19
Independent Claim 209 words
A method for recoating an uncoated section of a coated optical waveguide fiber with a UV-curable resin which shrinks upon curing comprising the steps of: (a) providing a split mold which forms, when closed, a cavity for receiving the uncoated section of the fiber, the cross-sectional size and shape of the cavity being essentially equal to the cross-sectional size and shape of the coated fiber, said mold having a first portion which is made of a material which is opaque to ultraviolet light and which includes an injection port for introducing the UV-curable resin into the cavity, and a second portion for introducing ultraviolet light into the cavity, said second portion being made of a material which is transparent to ultraviolet light; (b) placing the uncoated section of the fiber into the cavity; (c) introducing UV-curable resin into the cavity under pressure through the injection port; and (d) introducing ultraviolet light into the cavity through the second portion of the mold to progressively cure the resin in the cavity beginning with the resin in the region of the second portion and progressing towards the injection port while introducing additional UV-curable resin into the cavity under pressure through the injection port to compensate for shrinkage of the resin during curing.
Claim 20
Independent Claim 209 words
A method for recoating an uncoated section of a coated optical waveguide fiber with a UV-curable resin which shrinks upon curing comprising the steps of: (a) providing a split mold which forms, when closed, a cavity for receiving the uncoated section of the fiber, the cross-sectional size and shape of the cavity being essentially equal to the cross-sectional size and shape of the coated fiber, said mold having a first portion which is made of a material which is opaque to ultraviolet light and which includes an injection port for introducing the UV-curable resin into the cavity, and a second portion for introducing ultraviolet light into the cavity, said second portion being made of a material which is transparent to ultraviolet light; (b) placing the uncoated section of the fiber into the cavity; (c) introducing UV-curable resin into the cavity under pressure through the injection port; and (d) introducing ultraviolet light into the cavity through the second portion of the mold to progressively cure the resin in the cavity beginning with the resin in the region of the second portion and progressing towards the injection port while introducing additional UV-curable resin into the cavity under pressure through the injection port to compensate for shrinkage of the resin during curing.

References Cited (Backward Citations)

US4410561A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1990-05-04 1990-11-03 1991-05-05 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1994-05-04 1994-11-03 1995-05-05 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1998-05-04 1998-11-03 1999-05-05 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag