Well cementing method using an AM/AMPS fluid loss additive blend
Assignee: BJ Services Co USA
•
Filing: 1985-12-27
•
Granted: 1986-12-30
•
Expires: 2005-12-27
Abstract
Abstract An additive blend for a well cementing composition is shown which comprises a copolymer of acrylamide and 2-acrylamido-2-methylpropane sulfonate, the sodium salt of naphthalene formaldehyde sulfonate, and polyvinylpyrrolidone polymer. The fluid loss additive is mixed together with a hydraulic cement and water in an amount to produce a pumpable slurry. The cement slurry is pumped to the desired location in the wellbore and allowed to harden to a solid mass.
Inventors
- 👤 Virgilio G. Boncan
- 👤 Richard Gandy
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-23 18:02
CPC Classifications
C; C04; C04B; C04B28/00; C04B28/02; C04B24/00; C04B24/16; C04B24/24; C04B24/26; C09; C09K; C09K8/00; C09K8/42; C09K8/46; C09K8/467; C09K8/487; C04B2103/00; C04B2103/46
Claims Analysis
Total Claims: 7
Claim 1
Independent Claim
72 words
A method of cementing a wellbore, comprising the steps of: mixing together a hydraulic cement, water in an amount to produce a pumpable slurry, and a non-retarding fluid loss additive blend which comprises a copolymer of acrylamide and 2-acrylamido-2-methylpropane sulfonate, the sodium salt of naphthalene formaldehyde sulfonate, and polyvinylpyrrolidone polymer; pumping said cement slurry to the desired location in said wellbore; and allowing said cement slurry to harden to a solid mass.
Claim 2
Independent Claim
72 words
A method of cementing a wellbore, comprising the steps of: mixing together a hydraulic cement, water in an amount to produce a pumpable slurry, and a non-retarding fluid loss additive blend which comprises a copolymer of acrylamide and 2-acrylamido-2-methylpropane sulfonate, the sodium salt of naphthalene formaldehyde sulfonate, and polyvinylpyrrolidone polymer; pumping said cement slurry to the desired location in said wellbore; and allowing said cement slurry to harden to a solid mass.
Claim 3
Independent Claim
114 words
A method of cementing a wellbore, comprising the steps of: mixing together a hydraulic cement, from about 35 to 90 weight percent water, and from about 0.1 to 2.0 weight percent of a non-retarding fluid loss additive blend which comprises a copolymer of acrylamide and 2-acrylamido-2-methylpropane sulfonate, the sodium salt of naphthalene formaldehyde sulfonate, and polyvinylpyrrolidone polymer, all weight percents being based upon the weight of dry cement, and wherein the relative proportion of copolymer to sodium salt of naphthalene formaldehyde sulfonate to polyvinylpyrrolidone polymer in the additive blend is approximately 3:3:1; pumping said cement slurry to the desired location in said wellbore; and allowing said cement slurry to harden to a solid mass.
Claim 4
Independent Claim
114 words
A method of cementing a wellbore, comprising the steps of: mixing together a hydraulic cement, from about 35 to 90 weight percent water, and from about 0.1 to 2.0 weight percent of a non-retarding fluid loss additive blend which comprises a copolymer of acrylamide and 2-acrylamido-2-methylpropane sulfonate, the sodium salt of naphthalene formaldehyde sulfonate, and polyvinylpyrrolidone polymer, all weight percents being based upon the weight of dry cement, and wherein the relative proportion of copolymer to sodium salt of naphthalene formaldehyde sulfonate to polyvinylpyrrolidone polymer in the additive blend is approximately 3:3:1; pumping said cement slurry to the desired location in said wellbore; and allowing said cement slurry to harden to a solid mass.
Claim 5
Dependent Claim
28 words
The method of claim 2, wherein the additive blend is present in the range from about 0.6 to 0.7 weight percent, based upon the weight of dry cement.
Claim 6
Independent Claim
125 words
A method of cementing a wellbore, comprising the steps of: mixing together a hydraulic cement, from about 35 to 90 weight percent water, and about 0.7 weight percent of a non-retarding fluid loss additive blend which comprises about 0.3 weight percent of a copolymer of acrylamide and 2-acrylamido-2-methylpropane sulfonate, about 0.3 weight percent of the sodium salt of naphthalene formaldehyde sulfonate, and about 0.1 weight percent of polyvinylpyrrolidone polymer, all weight percents being based upon the dry weight of dry cement, thereby producing a pumpable cement slurry which is characterized by a viscosity in the range from about 5-9 Bearden units of viscosity; pumping said cement slurry to the desired location in said wellbore; and allowing said cement slurry to harden to a solid mass.
Claim 7
Independent Claim
125 words
A method of cementing a wellbore, comprising the steps of: mixing together a hydraulic cement, from about 35 to 90 weight percent water, and about 0.7 weight percent of a non-retarding fluid loss additive blend which comprises about 0.3 weight percent of a copolymer of acrylamide and 2-acrylamido-2-methylpropane sulfonate, about 0.3 weight percent of the sodium salt of naphthalene formaldehyde sulfonate, and about 0.1 weight percent of polyvinylpyrrolidone polymer, all weight percents being based upon the dry weight of dry cement, thereby producing a pumpable cement slurry which is characterized by a viscosity in the range from about 5-9 Bearden units of viscosity; pumping said cement slurry to the desired location in said wellbore; and allowing said cement slurry to harden to a solid mass.
References Cited (Backward Citations)
US4015991A
Cited
US4258790A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1989-12-29 | 1990-06-30 | 1990-12-30 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1993-12-29 | 1994-06-30 | 1994-12-30 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1997-12-29 | 1998-06-30 | 1998-12-30 | $7700.00 | Window Closed / Lapsed |