Abstract

Abstract Polyamide plastic fuel lines which are dimensionally stable and resistant to fuels, alcoholic fuels and alcohols as fuels are prepared from aliphatic high molecular weight polyamides. The fuel lines are prepared by extruding a hot melt of the polyamide, sizing through a die having a diameter in excess of the given diameter of the fuel line, cooling the fuel line in a cooling bath, removing the fuel line from the bath and sizing the fuel line adiabatically through a disk having a diameter less than the given diameter.

Inventors

  • 👤 Klaus Michel
  • 👤 Armin Gude

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-23 16:26
CPC Classifications
B; B29; B29C; B29C55/00; B29C55/30; B29C48/00; B29C48/03; B29C48/09; B29C48/25; B29C48/88; B29C48/90; B29C48/901; B29C48/908; B29C48/919; B29C48/10; B29K; B29K2077/00; Y; Y10; Y10S; Y10S138/00; Y10S138/07; Y10S264/00; Y10S264/61; Y10T; Y10T428/00; Y10T428/13; Y10T428/1352; Y10T428/139

Claims Analysis

Total Claims: 8
Claim 1
Independent Claim 142 words
The product obtained by the method for manufacturing shaped, hollow sections of polyamide plastics dimensionally stable under influence of fuels for internal combustion engines and having a given diameter consisting of: (a) extruding a hot melt of aliphatic polyamides having at least 5 carbon atoms per carbon amide group or polyamides from an aliphatic dicarboxylic acid and an aliphatic diamine which together have at least 12 carbon atoms through a tube die; (b) sizing said hot melt through a first gauging device having an inside diameter greater than said given diameter; (c) cooling said shaped, hollow sections obtained in a cooling bath; (d) removing the cooled, shaped hollow sections from the cooling bath; and (e) sizing the cooled, shaped hollow sections adiabatically through a second gauging device having an inside diameter less than said given diameter whereby said given diameter is achieved.
Claim 2
Dependent Claim 142 words
The product obtained by the method for manufacturing shaped, hollow sections of polyamide plastics dimensionally stable under influence of fuels for internal combustion engines and having a given diameter consisting of: (a) extruding a hot melt of aliphatic polyamides having at least 5 carbon atoms per carbon amide group or polyamides from an aliphatic dicarboxylic acid and an aliphatic diamine which together have at least 12 carbon atoms through a tube die; (b) sizing said hot melt through a first gauging device having an inside diameter greater than said given diameter; (c) cooling said shaped, hollow sections obtained in a cooling bath; (d) removing the cooled, shaped hollow sections from the cooling bath; and (e) sizing the cooled, shaped hollow sections adiabatically through a second gauging device having an inside diameter less than said given diameter whereby said given diameter is achieved.
Claim 3
Dependent Claim 139 words
Fuel lines for conducting fuels to internal combustion engines obtained by the method of manufacturing dimensionally stable fuel lines of polyamide plastics having a given diameter consisting of: (a) extruding a hot melt of aliphatic polyamides having at least 5 carbon atoms per carbon amide group or polyamides from an aliphatic dicarboxylic acid and an aliphatic diamine which together have at least 12 carbon atoms through a tube die; (b) sizing said hot melt through a first gauging device having an inside diameter greater than said given diameter; (c) cooling said shaped, hollow sections obtained in a cooling bath; (d) removing the cooled, shaped hollow sections from the cooling bath; and (e) sizing the cooled, shaped hollow sections adiabatically through a second gauging device having an inside diameter less than said given diameter whereby said given diameter is achieved.
Claim 4
Dependent Claim 139 words
Fuel lines for conducting fuels to internal combustion engines obtained by the method of manufacturing dimensionally stable fuel lines of polyamide plastics having a given diameter consisting of: (a) extruding a hot melt of aliphatic polyamides having at least 5 carbon atoms per carbon amide group or polyamides from an aliphatic dicarboxylic acid and an aliphatic diamine which together have at least 12 carbon atoms through a tube die; (b) sizing said hot melt through a first gauging device having an inside diameter greater than said given diameter; (c) cooling said shaped, hollow sections obtained in a cooling bath; (d) removing the cooled, shaped hollow sections from the cooling bath; and (e) sizing the cooled, shaped hollow sections adiabatically through a second gauging device having an inside diameter less than said given diameter whereby said given diameter is achieved.
Claim 5
Dependent Claim 151 words
Fuel lines for conducting fuels selected from the group consisting of alcoholic fuels and alcohols as fuels to internal combustion engines obtained by the method of manufacturing dimensionally stable fuel lines of polyamide plastics having a given diameter consisting of: (a) extruding a hot melt of aliphatic polyamides having at least 5 carbon atoms per carbon amide group or polyamides from an aliphatic dicarboxylic acid and an aliphatic diamine which together have at least 12 carbon atoms through a tube die; (b) sizing said hot melt through a first gauging device having an inside diameter greater than said given diameter; (c) cooling said shaped, hollow sections obtained in a cooling bath; (d) removing the cooled, shaped hollow sections from the cooling bath; and (e) sizing the cooled, shaped hollow sections adiabatically through a second gauging device having an inside diameter less than said given diameter whereby said given diameter is achieved.
Claim 6
Dependent Claim 151 words
Fuel lines for conducting fuels selected from the group consisting of alcoholic fuels and alcohols as fuels to internal combustion engines obtained by the method of manufacturing dimensionally stable fuel lines of polyamide plastics having a given diameter consisting of: (a) extruding a hot melt of aliphatic polyamides having at least 5 carbon atoms per carbon amide group or polyamides from an aliphatic dicarboxylic acid and an aliphatic diamine which together have at least 12 carbon atoms through a tube die; (b) sizing said hot melt through a first gauging device having an inside diameter greater than said given diameter; (c) cooling said shaped, hollow sections obtained in a cooling bath; (d) removing the cooled, shaped hollow sections from the cooling bath; and (e) sizing the cooled, shaped hollow sections adiabatically through a second gauging device having an inside diameter less than said given diameter whereby said given diameter is achieved.
Claim 7
Dependent Claim 140 words
Fuel lines for conducting alcoholic fuels to internal combustion engines obtained by the method of manufacturing dimensionally stable fuel lines of polyamide plastics having a given diameter consisting of: (a) extruding a hot melt of aliphatic polyamides having at least 5 carbon atoms per carbon amide group or polyamides from an aliphatic dicarboxylic acid and an aliphatic diamine which together have at least 12 carbon atoms through a tube die; (b) sizing said hot melt through a first gauging device having an inside diameter greater than said given diameter; (c) cooling said shaped, hollow sections obtained in a cooling bath; (d) removing the cooled, shaped hollow sections from the cooling bath; and (e) sizing the cooled, shaped hollow sections adiabatically through a second gauging device having an inside diameter less than said given diameter whereby said given diameter is achieved.
Claim 8
Dependent Claim 140 words
Fuel lines for conducting alcoholic fuels to internal combustion engines obtained by the method of manufacturing dimensionally stable fuel lines of polyamide plastics having a given diameter consisting of: (a) extruding a hot melt of aliphatic polyamides having at least 5 carbon atoms per carbon amide group or polyamides from an aliphatic dicarboxylic acid and an aliphatic diamine which together have at least 12 carbon atoms through a tube die; (b) sizing said hot melt through a first gauging device having an inside diameter greater than said given diameter; (c) cooling said shaped, hollow sections obtained in a cooling bath; (d) removing the cooled, shaped hollow sections from the cooling bath; and (e) sizing the cooled, shaped hollow sections adiabatically through a second gauging device having an inside diameter less than said given diameter whereby said given diameter is achieved.

References Cited (Backward Citations)

US2661499A Cited
US3182108A Cited
US4303711A Cited
US4508769A Cited
US4508769B Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1989-09-22 1990-03-24 1990-09-23 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1993-09-22 1994-03-24 1994-09-23 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1997-09-22 1998-03-24 1998-09-23 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag