Thin, soft, absorbent product
Assignee: Personal Products Co
•
Filing: 1984-08-17
•
Granted: 1985-12-17
•
Expires: 2004-08-17
Abstract
Abstract An absorbent structure is provided, which is comprised of a fibrous web, having an initial dry bulk of at least about 20 cc/gm., a dry bulk recovery of at least about 30 percent, and a wet bulk of at least about 30 cc/gm., and a basis weight less than about 4 oz/sq. yd. containing at least about 200 percent by weight superabsorbent. The structure is microcorrugated to provide a softness having a Taber stiffness value less than about 50.
Inventors
- 👤 Michael J. Iskra
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-23 10:39
CPC Classifications
A; A61; A61F; A61F13/00; A61F13/15; A61F13/53; A61F13/534; A61F13/535; A61F13/536; A61F13/15203; A61F13/51; A61F13/511; A61F13/51104; A61F13/51121; A61F13/531; A61F13/532; A61F13/533; A61F13/537; A61F13/539; A61F2013/530131; A61F2013/530481; A61F2013/530489; A61F2013/530496; A61F2013/530868; A61F2013/530927; A61F2013/530934; A61F2013/530941; A61F2013/53445; A61F13/53708; A61F2013/53721; A61F2013/53966
Claims Analysis
Total Claims: 14
Claim 1
Independent Claim
89 words
An absorbent structure comprising a fibrous web of resilient fibers, said web having a basis weight less than about 4 oz/sq. yd., an initial dry bulk of at least about 20 cc/gm., a dry bulk recovery of at least about 30 percent and a wet bulk of at least about 30 cc/gm., and superabsorbent disposed in amongst the fibers of said web in an amount of at least about 200 percent by weight based on said web weight, said structure having a Taber stiffness value less than about 50.
Claim 2
Dependent Claim
89 words
An absorbent structure comprising a fibrous web of resilient fibers, said web having a basis weight less than about 4 oz/sq. yd., an initial dry bulk of at least about 20 cc/gm., a dry bulk recovery of at least about 30 percent and a wet bulk of at least about 30 cc/gm., and superabsorbent disposed in amongst the fibers of said web in an amount of at least about 200 percent by weight based on said web weight, said structure having a Taber stiffness value less than about 50.
Claim 3
Dependent Claim
16 words
The absorbent structure of claim 1 wherein said Taber stiffness value is less than about 25.
Claim 4
Dependent Claim
25 words
The absorbent structure of claim 1 wherein a layer of wood pulp fibers has been placed on at least one side of said absorbent structure.
Claim 5
Dependent Claim
21 words
The product of claim 3 wherein a layer of wood pulp fibers is placed on both sides of said absorbent structure.
Claim 6
Dependent Claim
16 words
The absorbent structure of claim 1 wherein said fibrous web is a web of polyester fibers.
Claim 7
Dependent Claim
81 words
A disposable diaper containing as the absorbing layer an absorbent structure comprising a fibrous web, said we having of at least about 20 cc/gm., a dry bulk recovery of at least about 30 percent, and a wet bulk of at least about 30 cc/gm., and superabsorbent disposed in amongst the fibers of said web in an amount of at least about 200 percent by weight based on said web weight, said structure having a Taber stiffness value less than about 50.
Claim 8
Dependent Claim
81 words
A disposable diaper containing as the absorbing layer an absorbent structure comprising a fibrous web, said we having of at least about 20 cc/gm., a dry bulk recovery of at least about 30 percent, and a wet bulk of at least about 30 cc/gm., and superabsorbent disposed in amongst the fibers of said web in an amount of at least about 200 percent by weight based on said web weight, said structure having a Taber stiffness value less than about 50.
Claim 9
Dependent Claim
90 words
A sanitary napkin having as the absorbent layer an absorbent structure comprising a fibrous web having a basis weight less than about 4 oz/sq. yd., an initial dry bulk of at least about 20 cc/gm., a dry bulk recovery of at least 30 percent, and a wet bulk of at least about 30 cc/gm., and superabsorbent disposed in amongst the fibers of said web in an amount at least about 200 percent by weight based on said web weight, said structure having a Taber stiffness value less than about 50.
Claim 10
Dependent Claim
90 words
A sanitary napkin having as the absorbent layer an absorbent structure comprising a fibrous web having a basis weight less than about 4 oz/sq. yd., an initial dry bulk of at least about 20 cc/gm., a dry bulk recovery of at least 30 percent, and a wet bulk of at least about 30 cc/gm., and superabsorbent disposed in amongst the fibers of said web in an amount at least about 200 percent by weight based on said web weight, said structure having a Taber stiffness value less than about 50.
Claim 11
Independent Claim
106 words
A method for preparing an absorbent structure being capable of absorbing at least about 5 cc/gm. of liquid and being a nonwoven web having a basis weight of less than about 4 oz/sq. yd., an initial dry bulk of at least about 20 cc/gm., a dry bulk recovery of at least about 30 percent, and a wet bulk of at least about 30 cc/gm., said web containing at least about 200 percent by weight superabsorbent comprising: (a) drying said web containing superabsorbent to a moisture content less than about 25 percent, and (b) microcorrugating said web to provide a Taber stiffness of less than about 50.
Claim 12
Independent Claim
106 words
A method for preparing an absorbent structure being capable of absorbing at least about 5 cc/gm. of liquid and being a nonwoven web having a basis weight of less than about 4 oz/sq. yd., an initial dry bulk of at least about 20 cc/gm., a dry bulk recovery of at least about 30 percent, and a wet bulk of at least about 30 cc/gm., said web containing at least about 200 percent by weight superabsorbent comprising: (a) drying said web containing superabsorbent to a moisture content less than about 25 percent, and (b) microcorrugating said web to provide a Taber stiffness of less than about 50.
Claim 13
Dependent Claim
15 words
The method of claim 8 wherein said Taber stiffness value is less than about 25.
Claim 14
Dependent Claim
20 words
The method of claim 8 wherein said Taber stiffness value is less than about 10 in at least one direction.
References Cited (Backward Citations)
US26151A
Cited
US2788003A
Cited
USRE26151E
Cited
US4102340A
Cited
US4186165A
Cited
US4340057A
Cited
US4500315A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1988-12-16 | 1989-06-17 | 1989-12-17 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1992-12-16 | 1993-06-17 | 1993-12-17 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1996-12-16 | 1997-06-17 | 1997-12-17 | $7700.00 | Window Closed / Lapsed |