← Back to Patent Explorer
US4537663A Expired / Lapsed US ⏱️ 0.0 years remaining

Method of and apparatus for plating using controlled progressive immersion

Assignee: AT&T Inc
•
Filing: 1982-07-27
•
Granted: 1985-08-27
•
Expires: 2002-07-27
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Gold films (18) of essentially uniform thickness are plated onto respective previously formed palladium films (16) on substrates (10) by loading the substrates into a box plater (20) in opposed relationship to respective anode plates (22). In a plating operation, a plating potential initially is applied across upper end portions of the palladium films (16) and the anode plates (22). The loaded box plater (20) then is lowered into a gold plating bath (28) at a preselected rate to progressively immerse the substrates (10) and the anode plates (22) into the plating bath, such that gold plates onto each palladium film (16) to an essentially uniform thickness. The substrates (10) and anode plates (22) then are left immersed in the plating bath (28) for a total time period dependent upon the desired final thickness of the gold films (18).

Inventors

  • 👤 David I. Macdonald

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-23 02:20
CPC Classifications
C; C25; C25D; C25D5/00; C25D5/04; H; H05; H05K; H05K3/00; H05K3/22; H05K3/24; H05K3/241

Claims Analysis

Total Claims: 13
Claim 1
Independent Claim 195 words
A method of plating an essentially uniform thickness of an electrically conductive material onto an electrically conductive portion of an article, which comprises the steps of: supporting the article above an electroplating bath containing the electrically conductive material such that a lower end of the electrically conductive portion of the article is adjacent the electroplating bath; electrically contacting the electrically conductive portion of the article adjacent only an upper end thereof to apply electrical plating potential to the article portion; and progressively immersing the article portion, lower end first, at a preselected rate into the electroplating bath as the electrical plating potential to being applied to the article portion, such that successive sections of the article portion between the upper and lower ends thereof are continuously immersed in the electroplating bath for progressively increasing time periods, with the lower end of the article portion being continuously immersed in the electroplating bath for the longest time period and the upper end of the article portion being continuously immersed in the electroplating bath for the shortest time period, respectively, to form a layer of the electrically conductive material of an essentially uniform thickness on the article portion.
Claim 2
Independent Claim 195 words
A method of plating an essentially uniform thickness of an electrically conductive material onto an electrically conductive portion of an article, which comprises the steps of: supporting the article above an electroplating bath containing the electrically conductive material such that a lower end of the electrically conductive portion of the article is adjacent the electroplating bath; electrically contacting the electrically conductive portion of the article adjacent only an upper end thereof to apply electrical plating potential to the article portion; and progressively immersing the article portion, lower end first, at a preselected rate into the electroplating bath as the electrical plating potential to being applied to the article portion, such that successive sections of the article portion between the upper and lower ends thereof are continuously immersed in the electroplating bath for progressively increasing time periods, with the lower end of the article portion being continuously immersed in the electroplating bath for the longest time period and the upper end of the article portion being continuously immersed in the electroplating bath for the shortest time period, respectively, to form a layer of the electrically conductive material of an essentially uniform thickness on the article portion.
Claim 3
Dependent Claim 118 words
The method as recited in claim 1, which further comprises the steps of: disposing an anode above the electroplating bath such that a lower end of the anode is adjacent the electroplating bath and an upper end of the anode is further removed from the electroplating bath; disposing the article portion to be plated in opposed relationship to the anode; electrically contacting the article portion and the anode adjacent only the upper ends thereof to apply the electrical plating potential across the article portion and the anode; and progressively immersing the opposed article portion and anode, lower ends first, into the electroplating bath simultaneously as the plating potential is being applied across the article portion and the anode.
Claim 4
Dependent Claim 106 words
The method as recited in claim 1, in which the electrically conductive portion of the article has a higher electrical resistivity than the electrically conductive material, in which the progressive immersion of the article portion in the electroplating bath forms the layer of the electrically conductive material on the article portion to an essentially uniform initial thickness, and which further comprises the step of: continuing to plate additional electrically conductive material onto the article portion after the article portion has been fully immersed in the electroplating bath, to form the layer of the electrically conductive material on the article portion to an essentially uniform final thickness.
Claim 5
Dependent Claim 44 words
The method as recited in claim 3, in which: the article is a thin film substrate; the article portion to be plated is a palladium film formed on the substrate; and the electrically conductive material which is plated onto the article portion is gold.
Claim 6
Dependent Claim 30 words
The method as recited in claim 1, in which: the article portion is progressively immersed into the electroplating bath at a rate on the order of 3.6 inches per minute.
Claim 7
Dependent Claim 258 words
Apparatus for plating an essentially uniform thickness of an electrically conductive material on an electrically conductive portion of an article, which comprises: an anode; means for mounting the anode and the electrically conductive portion of the article in spaced opposed relationship above an electroplating bath containing the electrically conductive material such that lower ends of the article portion and the anode are adjacent the electroplating bath; means for electrically contacting the electrically conductive portion of the article and the anode adjacent only upper ends of the article portion and the anode, to apply electrical plating potential across the article portion and the anode; drive means for lowering the mounting means and progessively immersing the article portion and the anode, lower ends first, at a preselected rate into the electroplating bath simultaneously as the plating potential is being applied across the article portion and the anode, such that successive sections of the article portion between the upper and lower ends thereof are continuously immersed in the electroplating bath for progressively increasing time periods, with the lower end of the article portion being continuously immersed in the electroplating bath for the longest time period and the upper end of the article portion being continuously immersed in the electroplating bath for the shortest time period, respectively, to form a layer of the electrically conductive material of an essentially uniform thickness on the article portion; and means responsive to the lowering of the mounting means for de-energizing the drive means when the article portion has become fully immersed in the electroplating bath.
Claim 8
Dependent Claim 258 words
Apparatus for plating an essentially uniform thickness of an electrically conductive material on an electrically conductive portion of an article, which comprises: an anode; means for mounting the anode and the electrically conductive portion of the article in spaced opposed relationship above an electroplating bath containing the electrically conductive material such that lower ends of the article portion and the anode are adjacent the electroplating bath; means for electrically contacting the electrically conductive portion of the article and the anode adjacent only upper ends of the article portion and the anode, to apply electrical plating potential across the article portion and the anode; drive means for lowering the mounting means and progessively immersing the article portion and the anode, lower ends first, at a preselected rate into the electroplating bath simultaneously as the plating potential is being applied across the article portion and the anode, such that successive sections of the article portion between the upper and lower ends thereof are continuously immersed in the electroplating bath for progressively increasing time periods, with the lower end of the article portion being continuously immersed in the electroplating bath for the longest time period and the upper end of the article portion being continuously immersed in the electroplating bath for the shortest time period, respectively, to form a layer of the electrically conductive material of an essentially uniform thickness on the article portion; and means responsive to the lowering of the mounting means for de-energizing the drive means when the article portion has become fully immersed in the electroplating bath.
Claim 9
Dependent Claim 123 words
Apparatus as recited in claim 6, in which the electrically conductive portion of the article has a higher electrical resistivity than the electrically conductive material, in which the progressive immersion of the article portion in the electroplating bath by the drive means forms the layer of the electrically conductive material on the article portion to an essentially uniform initial thickness, and in which: the electrically contacting means continues to apply electrical plating potential across the article portion and the anode to cause plating of additional electrically conductive material onto the article portion after the article portion has been fully immersed in the electroplating bath, to form the layer of the electrically conductive material on the article portion to an essentially uniform final thickness.
Claim 10
Dependent Claim 98 words
Apparatus as recited in claim 6, in which the plating potential applying means includes: a cathode bar slidably mounted on the mounting means; an electrical contact member depending from the cathode bar and engageable with only one side of the article portion adjacent the upper end of the article portion, the contact member being movable with the slidable cathode bar between positions for clamping the article on the mounting means and for releasing the article for removal from the mounting means; and means for releasably clamping the cathode bar and the contact member in the article clamping position.
Claim 11
Independent Claim 191 words
A method of plating an essentially uniform thickness of an electrically conductive material onto an electrically conductive portion of an article, which comprises the steps of: supporting the article adjacent an electroplating bath containing the electrically conductive material such that the electrically conductive portion of the article has an upper end and a lower end; electrically contacting the electrically conductive portion of the article adjacent only the upper end thereof, to apply electrical plating potential to the article portion; and immersing the article portion in the electroplating bath in a manner such that successive portions of the article portion between the upper and lower ends of the article portion are immersed in the electroplating bath for progressively increasing time periods as the electrical plating potential is being applied to the article portion, with the lower end of the article portion being continuously immersed in the electroplating bath for the longest time period and the upper end of the article portion being continuously immersed in the electroplating bath for the shortest time period, respectively, to form a layer of the electrically conductive material of an essentially uniform thickness on the article portion.
Claim 12
Independent Claim 191 words
A method of plating an essentially uniform thickness of an electrically conductive material onto an electrically conductive portion of an article, which comprises the steps of: supporting the article adjacent an electroplating bath containing the electrically conductive material such that the electrically conductive portion of the article has an upper end and a lower end; electrically contacting the electrically conductive portion of the article adjacent only the upper end thereof, to apply electrical plating potential to the article portion; and immersing the article portion in the electroplating bath in a manner such that successive portions of the article portion between the upper and lower ends of the article portion are immersed in the electroplating bath for progressively increasing time periods as the electrical plating potential is being applied to the article portion, with the lower end of the article portion being continuously immersed in the electroplating bath for the longest time period and the upper end of the article portion being continuously immersed in the electroplating bath for the shortest time period, respectively, to form a layer of the electrically conductive material of an essentially uniform thickness on the article portion.
Claim 13
Dependent Claim 101 words
The method as recited in claim 9, in which the electrically conductive portion of the article has a higher electrical resistivity than the electrically conductive material, in which the immersion of the article portion in the electroplating bath forms the layer of the electrically conductive material on the article portion to an essentially uniform initial thickness, and which further comprises the step of: plating additional electrically conductive material on the article portion with the article portion fully immersed in the electroplating bath, to form the layer of the electrically conductive material on the article portion to an essentially uniform final thickness.

References Cited (Backward Citations)

US1939902A Cited
US2750332A Cited
US3388047A Cited
US4028198A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1988-08-26 1989-02-25 1989-08-27 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1992-08-26 1993-02-25 1993-08-27 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1996-08-26 1997-02-25 1997-08-27 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag