Method for making multi-layer metal core circuit board laminate with a controlled thermal coefficient of expansion

Assignee: General Electric Co
•
Filing: 1982-11-22
•
Granted: 1985-06-11
•
Expires: 2002-11-22
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A multi-layer circuit board laminate is disclosed having a controlled thermal coefficient of expansion which is particularly useful in conjunction with leadless components. The subject invention includes incorporating one or more stabilizing metal sheets into a composite multi-layer circuit board laminate assembly. The stabilizing metal sheets function to significantly reduce the circuit board laminate's thermal coefficient of expansion, thereby enabling the laminate to be used in conjunction with leadless electronic components. In addition, a novel method is disclosed for fabricating one embodiment of the subject invention and includes a unique two-step lamination process which permits apertures to be provided in the metal stabilizing layer and allows the bonding epoxy resin to solidify within the apertures, while simultaneously preventing the entrapment of air. In another embodiment of the subject invention the stabilizing layer is formed of a composite metal-dielectric laminate enabling the layer to be provided with a non-contiguous floating type pattern.

Inventors

  • 👤 John R. Hanson
  • 👤 James L. Hauser
  • 👤 James F. Kilfeather, Jr.
  • 👤 Hendrik B. Hendriks

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-23 14:44
CPC Classifications
B; B32; B32B; B32B15/00; B32B15/14; H; H05; H05K; H05K1/00; H05K1/02; H05K1/03; H05K2201/00; H05K2201/03; H05K2201/0332; H05K2201/0335; H05K2201/0355; H05K2201/06; H05K2201/068; H05K2201/09; H05K2201/09209; H05K2201/0929; H05K2201/09309; H05K2201/09654; H05K2201/09781; H05K3/00; H05K3/40; H05K3/42; H05K3/429; H05K3/46; H05K3/4611; Y; Y10; Y10S; Y10S428/00; Y10S428/901; Y10T; Y10T29/00; Y10T29/49; Y10T29/49002; Y10T29/49117; Y10T29/49124; Y10T29/49155; Y10T428/00; Y10T428/12; Y10T428/12389; Y10T428/12396

Claims Analysis

Total Claims: 6
Claim 1
Independent Claim 211 words
A method of making a multi-layer metal core circuit board laminate having a thermal coefficient of expansion less than that of a non-metal core laminate and conductive layers for use with leadless components, said method comprising the steps of: a. providing an uppermost planar copper foil conductive layer and a stabilizing layer formed of a metal having a thermal coefficient of expansion less than that of the non-metal portions of the laminate and copper conductive layer; b. providing a bonding layer interposed between said copper conductive layer and said stabilizing layer, said bonding layer being formed of resin impregnated glass cloth; c. laminating said layers to form a partial composite laminate structure; d. providing a printed circuit board layer and a lowermost planar copper foil layer; e. providing a second bonding layer between said printed circuit board layer and said lowermost copper foil layer; f. providing a third bonding layer between the lower surface of said stabilizing layer and the upper surface of said printed circuit board layer, said second and third bonding layers being formed of resin impregnated glass cloth; and g. laminating said layers to provide a complete composite laminate structure having a thermal coefficient of expansion less than that of the bonding layers and the copper conductive layers.
Claim 2
Independent Claim 211 words
A method of making a multi-layer metal core circuit board laminate having a thermal coefficient of expansion less than that of a non-metal core laminate and conductive layers for use with leadless components, said method comprising the steps of: a. providing an uppermost planar copper foil conductive layer and a stabilizing layer formed of a metal having a thermal coefficient of expansion less than that of the non-metal portions of the laminate and copper conductive layer; b. providing a bonding layer interposed between said copper conductive layer and said stabilizing layer, said bonding layer being formed of resin impregnated glass cloth; c. laminating said layers to form a partial composite laminate structure; d. providing a printed circuit board layer and a lowermost planar copper foil layer; e. providing a second bonding layer between said printed circuit board layer and said lowermost copper foil layer; f. providing a third bonding layer between the lower surface of said stabilizing layer and the upper surface of said printed circuit board layer, said second and third bonding layers being formed of resin impregnated glass cloth; and g. laminating said layers to provide a complete composite laminate structure having a thermal coefficient of expansion less than that of the bonding layers and the copper conductive layers.
Claim 3
Dependent Claim 21 words
The method of claim 1 wherein the thickness of the metal stabilizing layer is from about 0.005 to about 0.015 inches.
Claim 4
Dependent Claim 12 words
The method of claim 1 wherein the resin is an epoxy resin.
Claim 5
Dependent Claim 20 words
The method of claim 2 wherein the metal stabilizing layer is coated with copper oxide on at least one surface.
Claim 6
Dependent Claim 38 words
The method of claim 1 wherein at least two metal stabilizing layers separated by resin impregnated glass are laminated first to produce the metal having a thermal coefficient less than that of the non-metal portions of the laminate.

References Cited (Backward Citations)

US1609222A Cited
US1766471A Cited
US2217423A Cited
US3113435A Cited
US3345145A Cited
US3507739A Cited
US3666578A Cited
US3958317A Cited
US4170819A Cited
US4201616A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1988-06-10 1988-12-10 1989-06-11 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1992-06-10 1992-12-10 1993-06-11 $3760.00 Window Closed / Lapsed