US4309525A Expired / Lapsed US ⏱️ 0.0 years remaining

Production of sphere-formed powdery copolymers

Assignee: Ramot at Tel Aviv University Ltd
•
Filing: 1980-05-15
•
Granted: 1982-01-05
•
Expires: 2000-05-15
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A spherical powder of a hydrolyzed ethylene-vinyl acetate copolymer or its carboxyl modified product, is prepared by a method which comprises mixing 100 parts by weight of (1) a hydrolyzed product of an ethylene-vinyl acetate copolymer having 5 to 50% by weight of vinyl acetate group content or (2) a carboxyl modified product of the aforementioned hydrolyzed product obtained by reacting said hydrolyzed product with an unsaturated carboxylic acid or cyclic acid anhydride, with 10 to 100 parts by weight of an organic solvent capable of dissolving said hydrolyzed product or its carboxyl modified product, the solvent being not freely miscible with water and having a boiling point of not lower than 80 DEG C., 300 to 1000 parts by weight of water and 0.1 to 10 parts by weight of an alkylphenol ethylene oxide adduct having an HLB value of 10 to 20, emulsifying said mixture while it is maintained at a temperature of not lower than the softening point of said hydrolyzed product or carboxyl modified product, and decreasing the temperature of the system under stirring down to not higher than said softening point. The resultant powder is virtually spherical in its particle form, the particles are of almost equal size, and their particle size distribution is such that not less than 70% fall between 70 and 300 mu . Such spherical powder, when used in electrostatic coating, can provide beautiful coating films.

Inventors

  • 👤 Masamitsu Nakabayashi
  • 👤 Fumihiro Doura
  • 👤 Yuzo Furukawa

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-23 04:52
CPC Classifications
C; C08; C08J; C08J3/00; C08J3/12; C08J3/16; C08J2323/00; C08J2323/02; C08J2323/04; C08J2323/08

Claims Analysis

Total Claims: 11
Claim 1
Independent Claim 246 words
A method for producing spherical powder of a hydrolyzed ethylene-vinyl acetate copolymer or its carboxyl modified product, which comprises mixing (A) 100 parts by weight of (1) a hydrolyzed product of an ethylene-vinyl acetate copolymer having 5 to 50% by weight of vinyl acetate group content or (2) a carboxyl modified product of said hydrolyzed product obtained by reacting said hydrolyzed product with an unsaturated carboxylic acid or cyclic acid anhydride, both of said (1) and (2) containing sodium acetate as an impurity, with (B) 10 to 100 parts by weight of an organic solvent which is capable of dissolving said hydrolyzed product or said carboxyl modified product, said solvent being not freely miscible with water and having a boiling point of not lower than 80° C., (C) 300 to 1000 parts by weight of water, (D) 0.1 to 10 parts by weight of an alkylphenol ethylene oxide adduct having an HLB value of 10 to 20, and (E) an alkylbenzene sulfonic acid, emulsifying the resultant mixture while maintaining said mixture at a temperature of not lower than the softening point of said hydrolyzed product or said carboxyl modified product, and not higher than 95° C., and decreasing the temperature of the resultant system, under stirring, down to not higher than said softening point, to produce said powder which has a virtually spherical particle form and which has a particle size distribution such that not less than 70% of the particles are between 70 and 300μ.
Claim 2
Independent Claim 246 words
A method for producing spherical powder of a hydrolyzed ethylene-vinyl acetate copolymer or its carboxyl modified product, which comprises mixing (A) 100 parts by weight of (1) a hydrolyzed product of an ethylene-vinyl acetate copolymer having 5 to 50% by weight of vinyl acetate group content or (2) a carboxyl modified product of said hydrolyzed product obtained by reacting said hydrolyzed product with an unsaturated carboxylic acid or cyclic acid anhydride, both of said (1) and (2) containing sodium acetate as an impurity, with (B) 10 to 100 parts by weight of an organic solvent which is capable of dissolving said hydrolyzed product or said carboxyl modified product, said solvent being not freely miscible with water and having a boiling point of not lower than 80° C., (C) 300 to 1000 parts by weight of water, (D) 0.1 to 10 parts by weight of an alkylphenol ethylene oxide adduct having an HLB value of 10 to 20, and (E) an alkylbenzene sulfonic acid, emulsifying the resultant mixture while maintaining said mixture at a temperature of not lower than the softening point of said hydrolyzed product or said carboxyl modified product, and not higher than 95° C., and decreasing the temperature of the resultant system, under stirring, down to not higher than said softening point, to produce said powder which has a virtually spherical particle form and which has a particle size distribution such that not less than 70% of the particles are between 70 and 300μ.
Claim 3
Dependent Claim 21 words
A method as claimed in claim 1, wherein the alkylphenol ethylene oxide adduct has an HLB value of 13 to 19.
Claim 4
Dependent Claim 21 words
A method as claimed in claim 1, wherein the organic solvent is an aromatic hydrocarbon having 6 to 14 carbon atoms.
Claim 5
Dependent Claim 15 words
A method as claimed in claim 1, wherein the unsaturated carboxylic acid is acrylic acid.
Claim 6
Dependent Claim 15 words
A method as claimed in claim 1, wherein the cyclic acid anhydride is maleic anhydride.
Claim 7
Dependent Claim 24 words
A method as claimed in claim 1, wherein the hydrolyzed product of an ethylene-vinyl acetate copolymer has a 5 to 95% degree of hydrolysis.
Claim 8
Dependent Claim 43 words
A method as claimed in claim 1, wherein the carboxyl modified product is obtained by reacting the hydrolyzed product with 0.1 to 15% by weight of the unsaturated carboxylic acid or the cyclic acid anhydride based on the weight of the hydrolized product.
Claim 9
Dependent Claim 21 words
A method as claimed in claim 1, wherein the amount of the organic solvent is 20 to 80 parts by weight.
Claim 10
Dependent Claim 23 words
A method as claimed in claim 1, wherein the amount of the alkylphenol ethylene oxide adduct is 0.2 to 2.0 parts by weight.
Claim 11
Dependent Claim 20 words
A method as claimed in claim 1, wherein the amount of the water is 400 to 800 parts by weight.

References Cited (Backward Citations)

US3622555A Cited
CA1023094A Cited
US3972865A Cited
US4027079A Cited
US4212966A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1985-01-04 1985-07-06 1986-01-05 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1989-01-04 1989-07-06 1990-01-05 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1993-01-04 1993-07-06 1994-01-05 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag