Laser cutting of ceramic tubing
Assignee: General Electric Co
•
Filing: 1979-08-02
•
Granted: 1981-02-03
•
Expires: 1999-08-02
Abstract
Abstract Polycrystalline alumina tubing is scribed by means of laser pulses which are reiteratively focused on the same spots at spaced time intervals. By drilling small holes, the laser need be on for a very short period of time only, and only the surface layers are vaporized, thereby minimizing heat shock. The holes are deepened by repeating the series of pulses and directing them sequentially into the same holes. For tubing, an encoder is used which senses the angular position of the tubing as it is rotated and causes the laser to deliver pulses at the same angles at every revolution. When the holes have been sufficiently deepened, the tubing is snapped and breaks clean in the plane of the holes.
Inventors
- 👤 Edward M. Clausen
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-23 11:42
CPC Classifications
B; B23; B23K; B23K26/00; B23K26/08; B23K26/0823; B23K26/36; B23K26/40; B28; B28D; B28D5/00; B28D5/0005; B28D5/0011; B23K2103/00; B23K2103/50; B23K2103/52; Y; Y10; Y10T; Y10T225/00; Y10T225/10; Y10T225/12; Y10T225/30; Y10T225/307; Y10T225/321; Y10T225/325
Claims Analysis
Total Claims: 7
Claim 1
Independent Claim
60 words
The method of cutting ceramic material which comprises: drilling a series of fine shallow holes in the material by focusing a pulsed laser beam thereagainst at a series of spaced spots, deepening said holes by repeatedly directing the beam into the identical spots at spaced time intervals, and breaking said material along the line of weakness determined by said holes.
Claim 2
Independent Claim
60 words
The method of cutting ceramic material which comprises: drilling a series of fine shallow holes in the material by focusing a pulsed laser beam thereagainst at a series of spaced spots, deepening said holes by repeatedly directing the beam into the identical spots at spaced time intervals, and breaking said material along the line of weakness determined by said holes.
Claim 3
Dependent Claim
50 words
The method of claim 1 wherein the ceramic material is continuously displaced relative to the laser beam, and the laser beam is pulsed for short enough time intervals that relative movement between the material and the laser beam during said intervals will not appreciably reduce the definition of the holes.
Claim 4
Dependent Claim
12 words
The method of claim 1 wherein said ceramic material is polycrystalline alumina.
Claim 5
Independent Claim
75 words
The method of cutting polycrystalline alumina ceramic tubing which comprises: seizing the tubing in a rotary fixture and causing it to rotate, focusing a laser beam which can be pulsed on the tubing, pulsing the laser in coincidence with selected angular positions of the fixture whereby a series of fine holes are drilled in the tubing which are deepened at every revolution, and breaking the tubing along the plane of weakness determined by said holes.
Claim 6
Independent Claim
75 words
The method of cutting polycrystalline alumina ceramic tubing which comprises: seizing the tubing in a rotary fixture and causing it to rotate, focusing a laser beam which can be pulsed on the tubing, pulsing the laser in coincidence with selected angular positions of the fixture whereby a series of fine holes are drilled in the tubing which are deepened at every revolution, and breaking the tubing along the plane of weakness determined by said holes.
Claim 7
Dependent Claim
33 words
The method of claim 4 wherein a shaft encoder is coupled to said rotary fixture and provides a signal to an electronic controller for pulsing said laser in coincidence with said angular positions.
References Cited (Backward Citations)
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1984-02-03 | 1984-08-04 | 1985-02-03 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1988-02-03 | 1988-08-04 | 1989-02-03 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1992-02-03 | 1992-08-04 | 1993-02-03 | $7700.00 | Window Closed / Lapsed |