← Back to Patent Explorer
US4134872A Expired / Lapsed US ⏱️ 0.0 years remaining

Heterogeneous polymer particles comprising an interpolymer domain of a monovinylidene aromatic monomer, an open chain aliphatic conjugated diene and a monoethylenically unsaturated acid

Assignee: Dow Chemical Co
•
Filing: 1977-05-20
•
Granted: 1979-01-16
•
Expires: 1997-05-20
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Aqueous latexes of heterogeneous polymer particles comprising (1) a soft interpolymer domain of a monovinylidene aromatic monomer, such as styrene, an open chain aliphatic conjugated diene, such as 1,3-butadiene, and monoethylenically unsaturated carboxylic acid, such as acrylic acid, and (2) a hard resinous polymer domain (e.g., polystyrene) are useful binders for pigmented paper coatings having an improved combination of properties.

Inventors

  • 👤 Do I. Lee

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-23 12:52
CPC Classifications
D; D21; D21H; D21H19/00; D21H19/36; D21H19/44; D21H19/56; D21H19/58; C; C08; C08L; C08L25/00; C08L25/02; C08L25/04; C08L25/08; C08L25/10; C08L9/00; C08L9/06; C08L9/08; Y; Y10; Y10T; Y10T428/00; Y10T428/31504; Y10T428/3154

Claims Analysis

Total Claims: 15
Claim 1
Independent Claim 169 words
An aqueous polymer latex, (A) the dispersed polymer particles of which are heterogeneous and individually comprise per 100 parts by weight of the polymer particle: (1) from about 50 to about 90 parts by weight of a soft interpolymer domain having a glass transition temperature equal to or less than about 25° C. and comprising, based upon the total soft interpolymer: (a) from about 30 to about 69 weight percent of a monovinylidene aromatic monomer; (b) from about 30 to about 60 weight percent of an open-chain aliphatic conjugated diene having from 4 to about 9 carbon atoms; and (c) from about 1 to about 10 weight percent of a monoethylenically unsaturated carboxylic acid; and (2) from about 10 to about 50 parts by weight of a hard resinous polymer domain having a glass transition temperature of at least about 85° C.; and (B) which is prepared by emulsion polymerizing the monomers of the soft interpolymer domain in an aqueous medium comprising dispersed particles of the hard resinous polymer.
Claim 2
Dependent Claim 169 words
An aqueous polymer latex, (A) the dispersed polymer particles of which are heterogeneous and individually comprise per 100 parts by weight of the polymer particle: (1) from about 50 to about 90 parts by weight of a soft interpolymer domain having a glass transition temperature equal to or less than about 25° C. and comprising, based upon the total soft interpolymer: (a) from about 30 to about 69 weight percent of a monovinylidene aromatic monomer; (b) from about 30 to about 60 weight percent of an open-chain aliphatic conjugated diene having from 4 to about 9 carbon atoms; and (c) from about 1 to about 10 weight percent of a monoethylenically unsaturated carboxylic acid; and (2) from about 10 to about 50 parts by weight of a hard resinous polymer domain having a glass transition temperature of at least about 85° C.; and (B) which is prepared by emulsion polymerizing the monomers of the soft interpolymer domain in an aqueous medium comprising dispersed particles of the hard resinous polymer.
Claim 3
Dependent Claim 51 words
The polymer latex of claim 1 wherein the heterogeneous polymer particles comprise from about 50 to about 85 parts by weight of the soft interpolymer domain and from about 15 to about 50 parts by weight of the hard resinous polymer domain per 100 parts by weight of heterogeneous polymer particle.
Claim 4
Dependent Claim 63 words
The polymer latex of claim 1 wherein the soft interpolymer domain comprises, based upon the total soft interpolymer: (1) from about 50 to about 63 weight percent of a monovinylidene aromatic monomer; (2) from about 35 to about 45 weight percent of an open-chain aliphatic conjugated diene; and (3) from about 2 to about 5 weight percent of a monoethylenically unsaturated carboxylic acid.
Claim 5
Dependent Claim 23 words
The polymer latex of claim 1 wherein: (1) the monovinylidene aromatic monomer is styrene; and (2) the open-chain aliphatic conjugated diene is 1,3-butadiene.
Claim 6
Dependent Claim 27 words
The polymer latex of claim 4 wherein the monoethylenically unsaturated carboxylic acid is acrylic acid, methacrylic acid, itaconic acid, fumaric acid, maleic acid, or a combination thereof.
Claim 7
Dependent Claim 41 words
The polymer latex of claim 1 wherein the hard resinous polymer is a copolymer comprising a predominant amount of styrene and from about 1 to about 10 weight percent of a monoethylenically unsaturated carboxylic acid based upon the total copolymer weight.
Claim 8
Dependent Claim 42 words
The polymer latex of claim 1 wherein the soft interpolymer domain further comprises from about 1 to about 20 weight percent, based upon the total soft interpolymer, of a hydroxyalkylacrylate containing from 2 to about 4 carbon atoms in the alkyl group.
Claim 9
Dependent Claim 30 words
The polymer latex of claim 1 wherein the soft interpolymer domain further comprises from about 1 to about 10 weight percent, based upon the total soft interpolymer of 2-hydroxyethyl acrylate.
Claim 10
Dependent Claim 26 words
The polymer latex of claim 1 wherein the dispersed heterogeneous polymer particles constitute from about 20 to about 65 weight percent of the total polymer latex.
Claim 11
Dependent Claim 24 words
The polymer latex of claim 1 wherein the dispersed heterogeneous polymer particles have an average diameter of from about 0.08 to about 0.3 micrometer.
Claim 12
Dependent Claim 20 words
An improved aqueous paper-coating dispersion comprising: (1) a pigment; and (2) the polymer latex of claim 1 as a binder.
Claim 13
Dependent Claim 39 words
The aqueous paper-coating dispersion of claim 11 wherein the amount of dispersed heterogeneous polymer particles is from about 5 to about 30 parts by weight per 100 parts by weight of pigment, all parts being on a dry basis.
Claim 14
Dependent Claim 35 words
An improved coated paper product comprising a paper sheet carrying a dried deposit of a coating composition comprising: (1) a pigment; and (2) a binder comprising the polymer solids of the latex of claim 1.
Claim 15
Dependent Claim 30 words
The paper product of claim 13 wherein amount of polymer solids is from about 5 parts to about 30 parts by weight per 100 parts by weight of the pigment.

References Cited (Backward Citations)

CA501656A Cited
US2538779A Cited
US2614089A Cited
US2643987A Cited
US2711400A Cited
GB649166A Cited
US2927095A Cited
US2944044A Cited
US3095320A Cited
US3234302A Cited
US3409569A Cited
US3847856A Cited
US3849183A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1982-01-15 1982-07-17 1983-01-16 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1986-01-15 1986-07-17 1987-01-16 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1990-01-15 1990-07-17 1991-01-16 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag