Method of inhibiting scale formation
Assignee: Olin Corp
•
Filing: 1975-09-24
•
Granted: 1978-05-02
•
Expires: 1995-09-24
Abstract
Abstract Novel compositions comprising calcium hypochlorite and a proportion of a polyacrylic acid compound have been produced. the compositions provide accurately controlled concentrations of available chlorine to bodies of water such as swimming pools by reducing the solubility off the calcium hypochlorite. In addition, when employing dispensers for water soluble chemicals in treating very hard or highly alkaline water, inhibition of scale formation and prevention of scale build-up in the dispenser is achieved when the novel compositions are used.
Inventors
- 👤 John P. Faust
- 👤 Henry R. Cramer
- 👤 John M. Casberg
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-23 15:28
CPC Classifications
C; C02; C02F; C02F5/00; C02F5/08; C02F5/10; C02F5/105; C02F1/00; C02F1/72; C02F1/76; C02F2103/00; C02F2103/42
Claims Analysis
Total Claims: 11
Claim 1
Independent Claim
70 words
An agglomerate composition consisting essentially of calcium hypochlorite and a solubility reducing proportion of a polyacrylic acid compound having a molecular weight of from about 700 to about 3000 selected from the group consisting of polyacrylic acid, alkali metal salts of polyacrylic acid and mixtures thereof, wherein said solubility reducing proportion of said polyacrylic acid compound is from about 0.0001 to about 10 percent by weight of said calcium hypochlorite.
Claim 2
Dependent Claim
70 words
An agglomerate composition consisting essentially of calcium hypochlorite and a solubility reducing proportion of a polyacrylic acid compound having a molecular weight of from about 700 to about 3000 selected from the group consisting of polyacrylic acid, alkali metal salts of polyacrylic acid and mixtures thereof, wherein said solubility reducing proportion of said polyacrylic acid compound is from about 0.0001 to about 10 percent by weight of said calcium hypochlorite.
Claim 3
Dependent Claim
29 words
The agglomerate composition of claim 1 in which said alkali metal salt of polyacrylic acid is selected from the group consisting of sodium polyacrylate, potassium polyacrylate and lithium polyacrylate.
Claim 4
Dependent Claim
18 words
The agglomerate composition of claim 2 in which said alkali metal salt of polyacrylic acid is sodium polyacrylate.
Claim 5
Dependent Claim
22 words
The agglomerate composition of claim 3 in which said molecular weight of said sodium polyacrylate is from about 900 to about 2600.
Claim 6
Dependent Claim
26 words
The agglomerate composition of claim 4 in which said solubility reducing proportion is from about 0.001 to about 8 percent by weight of said calcium hypochlorite.
Claim 7
Dependent Claim
15 words
The agglomerate composition of claim 1 wherein said agglomerate is a granule, pellet or tablet.
Claim 8
Dependent Claim
12 words
The agglomerate composition of claim 6 wherein said agglomerate is a tablet.
Claim 9
Independent Claim
110 words
A method for inhibiting calcium scale formation in a dispenser for adding calcium hypochlorite to water to form an aqueous solution of calcium hypochlorite, comprising: adding to said dispenser an agglomerate composition consisting essentially of calcium hypochlorite and a proportion of a polyacrylic acid compound having a molecular weight of from about 700 to about 3000 selected from the group consisting polyacrylic acid, alkali metal salts of polyacrylic acid and mixtures thereof, wherein said proportion of said polyacrylic acid compound is from about 0.0001 to about 10 percent by weight of said calcium hypochlorite, and contacting said agglomerate composition with said water to form said aqueous solution of calcium hypochlorite.
Claim 10
Independent Claim
110 words
A method for inhibiting calcium scale formation in a dispenser for adding calcium hypochlorite to water to form an aqueous solution of calcium hypochlorite, comprising: adding to said dispenser an agglomerate composition consisting essentially of calcium hypochlorite and a proportion of a polyacrylic acid compound having a molecular weight of from about 700 to about 3000 selected from the group consisting polyacrylic acid, alkali metal salts of polyacrylic acid and mixtures thereof, wherein said proportion of said polyacrylic acid compound is from about 0.0001 to about 10 percent by weight of said calcium hypochlorite, and contacting said agglomerate composition with said water to form said aqueous solution of calcium hypochlorite.
Claim 11
Dependent Claim
19 words
The method of claim 8 in which said water has a hardness in excess of 400 parts per million.
References Cited (Backward Citations)
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1981-05-01 | 1981-10-31 | 1982-05-02 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1985-05-01 | 1985-10-31 | 1986-05-02 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1989-05-01 | 1989-10-31 | 1990-05-02 | $7700.00 | Window Closed / Lapsed |