Claims Analysis
Total Claims: 11
Claim 1
Independent Claim
219 words
A method for obtaining a filled, fluid barrier resistant plastic container wherein said container is exposed to a temperature in excess of 175° F. while retaining the barrier resistant characteristics thereof which comprises: preparing a seamless, multilayered, hollow plastic container having an open molded neck and having an outer pressure molded first portion of a thermoplastic material resistant to temperatures in excess of 175° F., an inner second portion of a thermoplastic material resistant to temperatures in excess of 175° F., and a third portion fluid barrier layer of a thermoplastic material between said first and second layers and co-extensive therewith throughout the extent thereof, said barrier layer having a lower temperature resistance than said first and second layers so that said container has the property that when exposed to an elevated temperature in excess of 175° F. but below the temperature resistance of said first and second positions said barrier layer softens or melts, but reforms in place upon cooling to retain its barrier resistant characteristics; filling said container through said open neck; exposing said container to an elevated temperature in excess of 175° F. but below the temperature resistance of said first and second portions followed be cooling the container to ambient temperature to utilize said property of the container and provide a filled, barrier resistant container.
Claim 2
Independent Claim
219 words
A method for obtaining a filled, fluid barrier resistant plastic container wherein said container is exposed to a temperature in excess of 175° F. while retaining the barrier resistant characteristics thereof which comprises: preparing a seamless, multilayered, hollow plastic container having an open molded neck and having an outer pressure molded first portion of a thermoplastic material resistant to temperatures in excess of 175° F., an inner second portion of a thermoplastic material resistant to temperatures in excess of 175° F., and a third portion fluid barrier layer of a thermoplastic material between said first and second layers and co-extensive therewith throughout the extent thereof, said barrier layer having a lower temperature resistance than said first and second layers so that said container has the property that when exposed to an elevated temperature in excess of 175° F. but below the temperature resistance of said first and second positions said barrier layer softens or melts, but reforms in place upon cooling to retain its barrier resistant characteristics; filling said container through said open neck; exposing said container to an elevated temperature in excess of 175° F. but below the temperature resistance of said first and second portions followed be cooling the container to ambient temperature to utilize said property of the container and provide a filled, barrier resistant container.
Claim 3
Dependent Claim
37 words
A method according to claim 1 wherein said container is filled with a material at a temperature in excess of 175° F. and wherein said filled container is cooled to ambient temperature to reform said barrier layer.
Claim 4
Dependent Claim
15 words
A method according to claim 2 wherein said second portion is a drawn thermoplastic material.
Claim 5
Dependent Claim
16 words
A method according to claim 3 wherein said second and third layers are drawn thermoplastic materials.
Claim 6
Dependent Claim
35 words
A method according to claim 2 wherein said first and second portions are resistant to temperature in excess of 220° F. and wherein said container is filled with a material in excess of 220° F.
Claim 7
Dependent Claim
31 words
A method according to claim 2 wherein said first and second portions are independently selected from the group consisting of polyolefins, polycarbonates, polysulfones, phenoxy resins, polyimines, ionomeric resins and acetal polymers.
Claim 8
Dependent Claim
28 words
A method according to claim 2 wherein said third portion barrier layer is selected from the group consisting of polyvinylidene chloride, polyvinyl acetate, acrylonitrile polymers and methacrylonitrile polymers.
Claim 9
Dependent Claim
33 words
A method according to claim 2 wherein said container has a fourth portion of a thermoplastic material resistant to temperatures in excess of 175° F. between said first portion and said third portion.
Claim 10
Dependent Claim
35 words
A method according to claim 2 including the step of securing a cap to said open molded neck after said container has been filled with a material at a temperature in excess of 175° F.
Claim 11
Dependent Claim
38 words
A method according to claim 1 wherein said container is exposed to an elevated temperature in excess of 175° F. subsequent to filling and wherein the filled container is cooled to ambient temperature to reform said barrier layer.