Block copolymer blends

Assignee: Shell USA Inc
•
Filing: 1977-02-11
•
Granted: 1977-08-02
•
Expires: 1997-02-11
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Block copolymer blends exhibiting improved (reduced) delamination characteristics comprise 65-90 parts of certain block copolymers having an average total molecular weight of 130,000 - 250,000 with a monoalkenyl arene block mol. wt. of 20,000 - 30,000 blended with 35-10 parts of a second block polymer having an average total molecular weight between about 60,000 and 100,000 with a monoalkenyl arene block mol. wt. between about 5,000 and 15,000.

Inventors

  • 👤 Glenn R. Himes
  • 👤 Luis Enrique Mendoza

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-23 00:06
CPC Classifications
C; C08; C08L; C08L53/00; C08L53/02

Claims Analysis

Total Claims: 9
Claim 1
Independent Claim 115 words
An unvulcanized block copolymer composition suitable for the manufacture of shoe heels comprising: a. 65 to 90 parts by weight of a first block copolymer having an average total molecular weight between about 170,000 and 210,000 and a monoalkenyl arene block mol. wt. between about 20,000 and 30,000; and b. 35 to 10 parts by weight of a second block copolymer having an average total molecular weight between about 70,000 and 90,000 and a monoalkenyl arene block mol. wt. between about 5,000 and 15,000; both of said block copolymers having at least two monoalkenyl arene polymer blocks and at least one conjugated diene polymer block and both of said block copolymers not having been hydrogenated.
Claim 2
Dependent Claim 115 words
An unvulcanized block copolymer composition suitable for the manufacture of shoe heels comprising: a. 65 to 90 parts by weight of a first block copolymer having an average total molecular weight between about 170,000 and 210,000 and a monoalkenyl arene block mol. wt. between about 20,000 and 30,000; and b. 35 to 10 parts by weight of a second block copolymer having an average total molecular weight between about 70,000 and 90,000 and a monoalkenyl arene block mol. wt. between about 5,000 and 15,000; both of said block copolymers having at least two monoalkenyl arene polymer blocks and at least one conjugated diene polymer block and both of said block copolymers not having been hydrogenated.
Claim 3
Dependent Claim 24 words
A composition according to claim 1 wherein the first block copolymer is present in an amount between about 75 and 85 parts by weight.
Claim 4
Dependent Claim 24 words
A composition according to claim 1 wherein the second block copolymer is present in an amount between about 25 to 15 parts by weight.
Claim 5
Dependent Claim 22 words
A composition according to claim 1 wherein the first block copolymer has a styrene block mol. wt. between about 23,000 and 27,000.
Claim 6
Dependent Claim 22 words
A composition according to claim 1 wherein the second block copolymer has a styrene block mol. wt. between about 8,000 and 12,000.
Claim 7
Dependent Claim 41 words
A composition according to claim 1 comprising in addition 25-150 parts by weight, per 100 parts of block copolymers, of a thermoplastic polymer of the group consisting of polystyrene, poly (alphamethylstyrene), poly (alpha olefins) and copolymers of ethylene with vinyl acetate.
Claim 8
Dependent Claim 23 words
A composition according to claim 1 comprising in addition 10-50 parts by weight per 100 parts of block copolymers, of an extending oil.
Claim 9
Dependent Claim 85 words
An extrudable composition according to claim 1 comprising ______________________________________ Parts by weight ______________________________________ a) a first block copolymer of styrene and 75-85 butadiene having an average total mole- cular weight between 170,000 and 210,000 and a styrene block mol. wt. of 23,000- 27,000; b) a second block copolymer of styrene and 15-25 butadiene having an average total mole- cular weight between 70,000 and 90,000 and a styrene block mol. wt. of 8,000- 12,000; c) Polystyrene 75-125 d) Naphthenic oil extender 15-35 e) Antioxidant 0.5-1.5 ______________________________________

References Cited (Backward Citations)

US3519585A Cited
US3497572A Cited
US3646161A Cited
US3614836A Cited
US3607977A Cited
US3823203A Cited
US3932327A Cited
US3865776A Cited
US4006116A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1980-08-01 1981-01-31 1981-08-02 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1984-08-01 1985-01-31 1985-08-02 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1988-08-01 1989-01-31 1989-08-02 $7700.00 Window Closed / Lapsed