Patent US3407817A successfully refreshed from Google Patents.
← Back to Patent Explorer
US3300543A Expired / Lapsed US ⏱️ 0.0 years remaining

Stabilized pressure sensitive adhesive consisting of saturated polyester and vinyl chloride polymer

Assignee: Avery Products Corp
•
Filing: 1961-08-17
•
Granted: 1967-01-24
•
Expires: 1981-08-17
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

No abstract record available.

Inventors

  • 👤 Turner Stanley

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-23 14:25
CPC Classifications
C; C09; C09J; C09J163/00; C08; C08F; C08F8/00; C08G; C08G63/00; C08G63/02; C08G63/12; C08G63/16; C09J167/00; C09J7/00; C09J7/20; C09J7/21; C09J7/30; C09J7/38; C08L; C08L2666/00; C08L2666/02; C08L2666/04; Y; Y10; Y10T; Y10T428/00; Y10T428/26; Y10T428/263

Claims Analysis

Total Claims: 4
Claim 1
Independent Claim 129 words
A PRESSURE SENSITIVE ADHESIVE WHICH CONSISTS ESSENTIALLY OF THE PRODUCT OBTAINED BY REACTING AT A TEMPERATURE IN THE RANGE FROM 140*C. TO 220*C. A SATURATED POLYESTER OF AN ORGANIC ACID SELECTED FROM THE GROUP CONSISTING OF SATURATED MONOCARBOXYLIC AND DICARBOXYLIC ACIDS AND A POLYHYDRIC ALCOHOL, SAID POLYESTER HAVING A MOLECULAR WEIGHT GREATER THAN ABOUT 1000, WITH A POLYVINYL RESIN SELECTED FROM THE GROUP CONSISTING OF HOMOPOLYMERS OF VINYL CHLORIDE AND COPOLYMERS HAVING AT LEAST 50% VINYL CHLORIDE, THE BALANCE COMPRISING COMPONENTS SELECTED FROM THE GROUP CONSISTING OF ESTERS AND VINYL ALCOHOL, THE REACTION MIXTURE CONTAINING BY WEIGHT FROM ABOUT 60% TO 90% POLYESTER AND FROM ABOUT 10% TO 40% POLYVINYL RESIN, SAID PRODUCT INCLUDING A STABILIZING COMPOUND THAT IS AN ACCEPTOR FOR HYDROGEN CHLORIDE EVOLVED FROM THE POLYVINYL RESIN.
Claim 2
Dependent Claim 129 words
A PRESSURE SENSITIVE ADHESIVE WHICH CONSISTS ESSENTIALLY OF THE PRODUCT OBTAINED BY REACTING AT A TEMPERATURE IN THE RANGE FROM 140*C. TO 220*C. A SATURATED POLYESTER OF AN ORGANIC ACID SELECTED FROM THE GROUP CONSISTING OF SATURATED MONOCARBOXYLIC AND DICARBOXYLIC ACIDS AND A POLYHYDRIC ALCOHOL, SAID POLYESTER HAVING A MOLECULAR WEIGHT GREATER THAN ABOUT 1000, WITH A POLYVINYL RESIN SELECTED FROM THE GROUP CONSISTING OF HOMOPOLYMERS OF VINYL CHLORIDE AND COPOLYMERS HAVING AT LEAST 50% VINYL CHLORIDE, THE BALANCE COMPRISING COMPONENTS SELECTED FROM THE GROUP CONSISTING OF ESTERS AND VINYL ALCOHOL, THE REACTION MIXTURE CONTAINING BY WEIGHT FROM ABOUT 60% TO 90% POLYESTER AND FROM ABOUT 10% TO 40% POLYVINYL RESIN, SAID PRODUCT INCLUDING A STABILIZING COMPOUND THAT IS AN ACCEPTOR FOR HYDROGEN CHLORIDE EVOLVED FROM THE POLYVINYL RESIN.
Claim 3
Dependent Claim 128 words
A PRESSURE SENSITIVE ADHESIVE WHICH CONSISTS ESSENTIALLY OF THE PRODUCT OBTAINED BY FIRST REACTING A SATURATED POLYESTER OF AN ORGANIC ACID SELECTED FROM THE GROUP CONSISTING OF SATURATED MONOCARBOXYLIC AND DICARBOXYLIC ACIDS AND A POLYHYDRIC ALCOHOL WITH AN EPOXY COMPOUND TO FORM AN EPOXY POLYESTER, SAID POLYESTER HAVING A MOLECULAR WEIGHT GREATER THAN ABOUT 1000, AND BY THEN REACTING THE POLYESTER AT A TEMPERATURE IN THE RANGE FROM 140*C. TO 220*C. WITH A POLYVINYL RESIN SELECTED FROM THE GROUP CONSISTING OF HOMOPOLYMERS OF VINYL CHLORIDE AND COPOLYMERS HAVING AT LEAST 50% VINYL CHLORIDE, THE BALANCE COMPRISING COMPONENTS SELECTED FROM THE GROUP CONSISTING OF ESTERS AND VINYL ALCOHOL, THE SECOND REACTION MIXTURE CONTAINING BY WEIGHT FROM ABOUT 60% TO 90% POLYESTER AND FROM ABOUT 10% TO 40% POLYVINYL RESIN.
Claim 4
Dependent Claim 128 words
A PRESSURE SENSITIVE ADHESIVE WHICH CONSISTS ESSENTIALLY OF THE PRODUCT OBTAINED BY FIRST REACTING A SATURATED POLYESTER OF AN ORGANIC ACID SELECTED FROM THE GROUP CONSISTING OF SATURATED MONOCARBOXYLIC AND DICARBOXYLIC ACIDS AND A POLYHYDRIC ALCOHOL WITH AN EPOXY COMPOUND TO FORM AN EPOXY POLYESTER, SAID POLYESTER HAVING A MOLECULAR WEIGHT GREATER THAN ABOUT 1000, AND BY THEN REACTING THE POLYESTER AT A TEMPERATURE IN THE RANGE FROM 140*C. TO 220*C. WITH A POLYVINYL RESIN SELECTED FROM THE GROUP CONSISTING OF HOMOPOLYMERS OF VINYL CHLORIDE AND COPOLYMERS HAVING AT LEAST 50% VINYL CHLORIDE, THE BALANCE COMPRISING COMPONENTS SELECTED FROM THE GROUP CONSISTING OF ESTERS AND VINYL ALCOHOL, THE SECOND REACTION MIXTURE CONTAINING BY WEIGHT FROM ABOUT 60% TO 90% POLYESTER AND FROM ABOUT 10% TO 40% POLYVINYL RESIN.

References Cited (Backward Citations)

US1867558A Cited
US1924994A Cited
US2036009A Cited
US2160230A Cited
US2460181A Cited
US2572085A Cited
US2512723A Cited
US2912397A Cited
US3075863A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1970-01-23 1970-07-25 1971-01-24 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1974-01-23 1974-07-25 1975-01-24 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1978-01-23 1978-07-25 1979-01-24 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag