Abstract

No abstract record available.

Inventors

  • 👤 Walter G Taschek

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-22 20:15
CPC Classifications
H; H01; H01M; H01M4/00; H01M4/86; H01M4/96; Y; Y02; Y02E; Y02E60/00; Y02E60/30; Y02E60/50

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 158 words
THE METHOD OF PREPARING A CARBON ELECTRODE FOR USE IN A FUEL CELL USING AN ACID ELECTROLYTE INCLUDING THE STEPS OF (1) WEIGHTING THE CARBON ELECTRODE, (2) FIRING THE CARBON ELECTRODE IN AN OXIDIZING ATMOSPHERE FOR CONTROLLED OXIDATION OF THE CARBON, (3) COOLING THE CARBON ELECTRODE, (4) REWEIGHING THE CARBON ELECTRODE AND DETERMINING THAT A TOTAL WEIGHT LOSS OF 7 TO 10 PERCENT HAS OCCURRED, (5) DUSTING OFF THE ACTIVATED ELECTRODES, (6) INSERTING THE ACTIVATED ELECTRODES IN A WET PROOFING SOLUTION (7) DRYING THE ELECTRODES WITH A VACUM PUMP TO INSURE A DEY PORE STRUCTURE, (8) HEATING THE WET PROFFED ELECTRODES IN AN OVEN AT 200* C FOR TWO HOURS, (9) APPLYING A CHLOROPLATINIC ACID SOLUTION CONTAINING ABOUT 90 MG. OF PLATINUM PER ML. OF SOLUTION ON THE HOT ELECTRODE SO THAT ONE SQUARE CENTIMETER OF ELECTORDE AREA CONTAINS 2 MG. OF PLAYINUM, AND (10) PLACING THE ELECTRODE IN A VACUUM OVEN AT 200* C. FOR SIX HOURS.
Claim 2
Independent Claim 158 words
THE METHOD OF PREPARING A CARBON ELECTRODE FOR USE IN A FUEL CELL USING AN ACID ELECTROLYTE INCLUDING THE STEPS OF (1) WEIGHTING THE CARBON ELECTRODE, (2) FIRING THE CARBON ELECTRODE IN AN OXIDIZING ATMOSPHERE FOR CONTROLLED OXIDATION OF THE CARBON, (3) COOLING THE CARBON ELECTRODE, (4) REWEIGHING THE CARBON ELECTRODE AND DETERMINING THAT A TOTAL WEIGHT LOSS OF 7 TO 10 PERCENT HAS OCCURRED, (5) DUSTING OFF THE ACTIVATED ELECTRODES, (6) INSERTING THE ACTIVATED ELECTRODES IN A WET PROOFING SOLUTION (7) DRYING THE ELECTRODES WITH A VACUM PUMP TO INSURE A DEY PORE STRUCTURE, (8) HEATING THE WET PROFFED ELECTRODES IN AN OVEN AT 200* C FOR TWO HOURS, (9) APPLYING A CHLOROPLATINIC ACID SOLUTION CONTAINING ABOUT 90 MG. OF PLATINUM PER ML. OF SOLUTION ON THE HOT ELECTRODE SO THAT ONE SQUARE CENTIMETER OF ELECTORDE AREA CONTAINS 2 MG. OF PLAYINUM, AND (10) PLACING THE ELECTRODE IN A VACUUM OVEN AT 200* C. FOR SIX HOURS.

References Cited (Backward Citations)

US2384463A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1966-07-22 1967-01-21 1967-07-23 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1970-07-22 1971-01-21 1971-07-23 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1974-07-22 1975-01-21 1975-07-23 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag