Patent US2266995A successfully refreshed from Google Patents.
US3017670A
Expired / Lapsed
US
⏱️ 0.0 years remaining
Process for producing plastic articles
Assignee: Hexion Inc
•
Filing: 1957-04-04
•
Granted: 1962-01-23
•
Expires: 1977-04-04
Abstract
No abstract record available.
Inventors
- 👤 Zweig Samuel
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-23 11:02
CPC Classifications
C; C08; C08J; C08J5/00; C08J5/12; C08J5/121; C08J2327/00; C08J2327/02; C08J2327/04; C08J2327/06
Claims Analysis
Total Claims: 2
Claim 1
Independent Claim
173 words
IN MAKING, WITHIN A MOLD, AN ARTICLE INCLUDING POLYVINYL CHLORIDE AND MIGRATORY PLASTICIZER THEREFOR AND PROTECTING THE ARTICLE AGAINST EXUDATION OF PLASTICIZER FROM THE OUTER SURFACE OF THE ARTICLE, THE PROCESS WHICH COMPRISES COATING THE INTERIOR OF THE MOLD WITH AN UNPLASTICIZED SEALING FILM ABOUT 0.00005-0.001 INCH THICK OF THERMOSPLASTIC MATERIAL THAT IS SOLUBLE IN THE SAID PLASTICIZER AND THAT, WITHOUT BECOMING TACKY, TOLERATES THE SAID PLASTICIZER IN PROPORTION THEREOF IN EXCESS OF THE PROPORTION TOLERATED BY THE POLYVINYL CHLORIDE AND THAT IS OF INTRINSIC VICOSITY AT LEAST 0.8 I CYCLOHEXANONE AT 20* C., MOLDING AGAINST THE SEALING FILM A MIXTURE OF THE SAID POLYVINYL CHROLIDE AND MIGRATORY PLASTICIZER THEREFOR, HEATING THE WHOLE TO A TEMPERATURE OF FLUIDIZING THE SAID MIXTURE AND SOFTENING THE SURFACE UNION OF THE SEALING FILM TO THE RESULTING PLASTICIZED POLYVINYL CHLORIDE PLASTIC, AND THEN COOLING THE PRODUCT BEFORE THE SAID PLASTICIZER PENETRATES THROUGH THE SEALING FILM, THE PLASTICIZED POLYVINYL CHLORIDE PLASTIC AFTER THE COOLING HAVING AN INTRINSIC VICOSITY SUBSTANTIALLY LESS THAN THAT OF THE MATERIAL OF THE FILM.
Claim 2
Dependent Claim
173 words
IN MAKING, WITHIN A MOLD, AN ARTICLE INCLUDING POLYVINYL CHLORIDE AND MIGRATORY PLASTICIZER THEREFOR AND PROTECTING THE ARTICLE AGAINST EXUDATION OF PLASTICIZER FROM THE OUTER SURFACE OF THE ARTICLE, THE PROCESS WHICH COMPRISES COATING THE INTERIOR OF THE MOLD WITH AN UNPLASTICIZED SEALING FILM ABOUT 0.00005-0.001 INCH THICK OF THERMOSPLASTIC MATERIAL THAT IS SOLUBLE IN THE SAID PLASTICIZER AND THAT, WITHOUT BECOMING TACKY, TOLERATES THE SAID PLASTICIZER IN PROPORTION THEREOF IN EXCESS OF THE PROPORTION TOLERATED BY THE POLYVINYL CHLORIDE AND THAT IS OF INTRINSIC VICOSITY AT LEAST 0.8 I CYCLOHEXANONE AT 20* C., MOLDING AGAINST THE SEALING FILM A MIXTURE OF THE SAID POLYVINYL CHROLIDE AND MIGRATORY PLASTICIZER THEREFOR, HEATING THE WHOLE TO A TEMPERATURE OF FLUIDIZING THE SAID MIXTURE AND SOFTENING THE SURFACE UNION OF THE SEALING FILM TO THE RESULTING PLASTICIZED POLYVINYL CHLORIDE PLASTIC, AND THEN COOLING THE PRODUCT BEFORE THE SAID PLASTICIZER PENETRATES THROUGH THE SEALING FILM, THE PLASTICIZED POLYVINYL CHLORIDE PLASTIC AFTER THE COOLING HAVING AN INTRINSIC VICOSITY SUBSTANTIALLY LESS THAN THAT OF THE MATERIAL OF THE FILM.
References Cited (Backward Citations)
US2184876A
Cited
US2176997A
Cited
GB516368A
Cited
US2491102A
Cited
GB595632A
Cited
US2453052A
Cited
US2729585A
Cited
US2744340A
Cited
US2792322A
Cited
US2815896A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1965-01-22 | 1965-07-24 | 1966-01-23 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1969-01-22 | 1969-07-24 | 1970-01-23 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1973-01-22 | 1973-07-24 | 1974-01-23 | $7700.00 | Window Closed / Lapsed |