Patent US2192061A successfully refreshed from Google Patents.
US2861046A
Expired / Lapsed
US
⏱️ 0.0 years remaining
Process of foaming a mixture of a thermoplastic resin and a binding agent
Assignee: BASF SE
•
Filing: 1957-02-06
•
Granted: 1958-11-18
•
Expires: 1977-02-06
Abstract
No abstract record available.
Inventors
- 👤 Stastny Fritz
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-22 23:21
CPC Classifications
C; C08; C08J; C08J9/00; C08J9/22; C08J9/228; C08J9/236
Claims Analysis
Total Claims: 2
Claim 1
Independent Claim
144 words
AN IMPROVED PROCESS FOR THE PRODUCTION OF A LIGHTWEIGHT EXPANDED MATERIAL WHICH COMPRISES: MIXING (A) 10 TO 90 PARTS BY WEIGHT OF EXPANDABLE INDIVIDUAL PARTICLES OF A THERMOPLASTIC RESIN SELECTED FROM THE GROUP CONSISTING OF POLYSTYRENE AND POLYMETHACRYLIC ACID METHYL ESTER, SAID RESIN CONTAINING A BLOWING AGENT CAPABLE OF EXPANDING SAID RESIN PARTICLES WHEN SOFTENED, WITH (B) 90 TO 10 PARTS BY WEIGHT OF A BINDING AGENT SELECTED FROM THE GROUP CONSISTING OF BITUMEN AND PARAFFIN WAXES HAVING A MELTING POINT BELOW THE SOFTENING POINT OF SAID RESIN PARTICLES; HEATING THE RESULTANT MIXTURE TO MELT SAID BINDING AGENT, SAID RESIN BEING INSOLUBLE IN SAID MOLTEN BINDING AGENT, WHEREBY SAID EXPANDABLE RESIN PARTICLES ARE UNIFORMLY COATED WITH SAID BINDING AGENT; FURTHER HEATING THE RESULTANT MIXTURE TO SOFTEN AND EXPAND SAID INDIVIDUAL COATED RESIN PARTICLES; AND PLACING SAID EXPANDED PARTICLES IN ADHERING CONTACT WITH EACH OTHER.
Claim 2
Dependent Claim
144 words
AN IMPROVED PROCESS FOR THE PRODUCTION OF A LIGHTWEIGHT EXPANDED MATERIAL WHICH COMPRISES: MIXING (A) 10 TO 90 PARTS BY WEIGHT OF EXPANDABLE INDIVIDUAL PARTICLES OF A THERMOPLASTIC RESIN SELECTED FROM THE GROUP CONSISTING OF POLYSTYRENE AND POLYMETHACRYLIC ACID METHYL ESTER, SAID RESIN CONTAINING A BLOWING AGENT CAPABLE OF EXPANDING SAID RESIN PARTICLES WHEN SOFTENED, WITH (B) 90 TO 10 PARTS BY WEIGHT OF A BINDING AGENT SELECTED FROM THE GROUP CONSISTING OF BITUMEN AND PARAFFIN WAXES HAVING A MELTING POINT BELOW THE SOFTENING POINT OF SAID RESIN PARTICLES; HEATING THE RESULTANT MIXTURE TO MELT SAID BINDING AGENT, SAID RESIN BEING INSOLUBLE IN SAID MOLTEN BINDING AGENT, WHEREBY SAID EXPANDABLE RESIN PARTICLES ARE UNIFORMLY COATED WITH SAID BINDING AGENT; FURTHER HEATING THE RESULTANT MIXTURE TO SOFTEN AND EXPAND SAID INDIVIDUAL COATED RESIN PARTICLES; AND PLACING SAID EXPANDED PARTICLES IN ADHERING CONTACT WITH EACH OTHER.
References Cited (Backward Citations)
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1961-11-17 | 1962-05-19 | 1962-11-18 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1965-11-17 | 1966-05-19 | 1966-11-18 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1969-11-17 | 1970-05-19 | 1970-11-18 | $7700.00 | Window Closed / Lapsed |