Process for descaling titanium
Assignee: Rohr Inc
•
Filing: 1955-09-06
•
Granted: 1957-08-27
•
Expires: 1975-09-06
Abstract
No abstract record available.
Inventors
- 👤 Wilfred J Wallace
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-23 07:50
CPC Classifications
C; C23; C23G; C23G1/00; C23G1/14; C23G1/20; C23G1/205; C23C; C23C22/00; C23C22/73; C23C22/74
Claims Analysis
Total Claims: 1
Claim 1
Independent Claim
96 words
THE METHOD OF FORMING A THIN SHEET OF TITANIUM TO THE SHAPE OF A CURVED DIE FACE WHICH COMPRISES THE STEPS OF WETTING THE ENTIRE SHEET WITH AN AQUEOUS SOLUTION CONSISTING ESSENTIALLY OF SODIUM NITRATE ABOUT 40 PERCENT, SODIUM CARBONATE ABOUT 2 TO 3 PERCENT, BALANCE WATER, DRYING THE WETTED SHEET TO PROVIDE DA THIN DRY SURFACE FILM THEREON; HEATING THE TREATED SHEET TO A TEMPERATURE WITHIN THE RANGE OF 400* TO 1200*F. TO PROVIDE A THIN SURFACE COATING OF THE LOWER OXIDES OF TITANIUM THEREON; AND PRESSING THE HOT COATED SHEET AGAINST SAID DIE FACE.
References Cited (Backward Citations)
DE734859C
Cited
US2309745A
Cited
US2289443A
Cited
US2499764A
Cited
US2598889A
Cited
US2554042A
Cited
US2704883A
Cited
US2724667A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1960-08-26 | 1961-02-25 | 1961-08-27 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1964-08-26 | 1965-02-25 | 1965-08-27 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1968-08-26 | 1969-02-25 | 1969-08-27 | $7700.00 | Window Closed / Lapsed |